PARTITION OF Hf AMONG THE PHASES AND ITS EFFECTS ON PRECIPITATES IN PM Ni–BASED SUPERALLOY FGH97

  • ZHANG Xi-Wen ,
  • YU Fu-Meng ,
  • HU Ben-Fu
Expand
  • 1. School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083
    2. High Temperature Material Institute, Central Iron and Steel Research Institute, Beijing 100081
    3. School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083

Received date: 2011-09-02

  Revised date: 2011-12-03

  Online published: 2012-02-11

Supported by

Supported by National Basic Research Program of China (No.2010CB631204)

Abstract

The partition behavior of hafnium among different phases in FGH97 PM (powder metallurgy) superalloy and its effects on the precipitation behaviors of MC carbide and γ' phase were studied by means of 3DAP, SEM, TEM and physiochemical phase analysis. The results showed that element Hf mainly exists in γ' phase and MC carbide, which makes γ' composition transform to (Ni, Co)3(Al, Ti, Nb, Hf), also makes MC transform to (Nb, Ti, Hf)C. With Hf addition increasing, the proportion of Hf in γ' maintains constant, but in MC carbide increases and in γ decreases, which means that partition ratio (R1) between γ' phase and MC carbide is decreased, while partition ratio (R2) between γ' phase and γ matrix is increased, the average partition ratio between γ' phase and MC carbide is about 1 :0.1, and the average partition ratio between γ' phase and γ matrix is about 1:0.05. Hf is helpful to the precipitations of γ' phase and MC carbide, the morphology and size of γ' phase are influenced more by Hf than these of MC carbide.

Cite this article

ZHANG Xi-Wen , YU Fu-Meng , HU Ben-Fu . PARTITION OF Hf AMONG THE PHASES AND ITS EFFECTS ON PRECIPITATES IN PM Ni–BASED SUPERALLOY FGH97[J]. Acta Metall Sin, 2012 , 48(2) : 187 -193 . DOI: 10.3724/SP.J.1037.2011.00558

References

[1] Duhl D N, Sulivan C P. JOM, 1971; 23: 38

[2] Kotval P S, Venables J D, Calder R W. Metall Trans, 1972; 3: 453

[3] Wang L B, Chen R Z, Wang Y P. Aero Mater, 1982; 2: 1

(王罗宝, 陈荣章, 王玉屏. 航空材料, 1982; 2: 1)

[4] Zheng Y R, Cai Y L Ruan Z C, Ma S W. J Aero Mater, 2006; 26: 25

(郑运荣, 蔡玉林, 阮中慈, 马书伟. 航空材料学报, 2006; 26: 25)

[5] Belov A F, Anoshkin N F, Fatkullin O S. Heat Resistant Steel and Nickel Base High Temperature Alloy. Moscow: Science Press, 1984: 31

[6] Radavich J, Carneiro T, Furrer D. In: Reed R C, Green K A, Caron P eds., Superalloys 2008. Pennsylvania: TMS, 2008: 63

[7] Hardy M C, Zirbel B, Shen G. In: Green K A, Pollock T M, Haradra H eds., Superalloys 2004. Pennsylvania: TMS, 2004: 83

[8] Zhen B L, Zhang S J. Central Iron Steel Res Inst Technol Bull, 1981; 1(1): 65

(甄宝林, 张绍津. 钢铁研究总院学报, 1981; 1(1): 65)

[9] Maslekov S B, Burova N N, Makulov O V. Met Sci Heat Treat, 1980; 22(4): 283

[10] Zimina L N, Burova N N, Makushok O V. Met Sci Heat Treat, 1986; 28(2): 130

[11] Amouyal Y, Seidman D N. Acta Mater, 2011; 59: 3321

[12] Miner R V. Metall Trans, 1977; 8A: 259

[13] Flageolet B, Villechaise P, Jouiad M. In: Green K A, Pollock T M, Haradra H eds., Superalloys 2004. Pennsylvania: TMS, 2004: 371

[14] Starink M J, Reed P A. Mater Sci Eng, 2008; A491: 279

[15] Department of chemical analysis, Central Iron and Steel Research Institute. New Metall Mater, 1977; (5): 60

(钢铁研究总院化学分析室. 新金属材料, 1977; (5): 60)

[16] Markiv V Y, Burnashova V V. IZV Akad Nauk SSSR Met, 1969; (6): 113

[17] Samsonov G V, Vinickji I M. Refractory Compound. 2nd Ed., Moscow: Metallurgy Industry Press, 1976: 150

[18] Doi M, Miyazaki T, Wakatsuki T. Mater Sci Eng, 1984; 67: 247

[19] Ardell A J. Acta Metall, 1968; 16: 511

[20] Xia P C, Yu J J, Sun X F, Guan H R, Hu Z Q. J Shandong Univ Sci Technol (Nat Sci), 2009; 28: 51

(夏鹏成, 于金江, 孙晓峰, 管恒荣, 胡壮麒. 山东科技大学学报(自然科学版), 2009; 28: 51)
Outlines

/

〈 〉