Abstract

Use Cu–31Si alloy (31mol% Si) prepared by inductive melting metallurgical grade silicon as anode and molybdenum as cathode and reference electrode, the cathodic behavior of molten salt 81CaCl2–8.0 NaCl–8.5CaO–2.5Si (Mole fraction, %) at 1173 K was studied by means of cyclic voltammetry and chronopotentiometry, and the reduction steps of silicon from the molten salt were discussed. The electro–refining of silicon was performed in the two electrode system under the voltage of −0.2 V. SEM, EDS and inductively coupled plasma atomic emission spectrometry (ICPAES) technologies were used to analyze and characterize the morphology and composition of the deposited silicon. Polycrystalline silicon was obtained after the electro–refining. Main impurity in the metallurgical grade silicon are greatly decreased. Especially boron and phosphorous which are very harmful to solar cell grade silicon were greatly removed. The contents of boron and phosphorous are decreased from 42×10−6 and 25×10−6 to 4.5×10−6 and 8.2×10−6, respectively. The current efficiency of the electro–refining process is 84.4%.

Cite this article

YU Shu-Lan , CHEN Xiao-Yun . STUDY ON THE ELECTRO–REFINING SILICON IN MOLTEN SALT CaCl2–NaCl–CaO[J]. Acta Metall Sin, 2012 , 48(2) : 183 -186 . DOI: 10.3724/SP.J.1037.2011.00547

References

[1] O’Mara W C, Herring R B, Hunt I P. Handbook of Semiconductor Silicon Technology. New Jersey: Noyes Publications, 1990: 795

[2] Ciszek T F, Schwuttke G H, Yang H K. IBM J Res Dev, 1978; 23: 270

[3] Martorano M A, Ferreira Neto J B, Oliveira T S, Tsubak T O. Mater Sci Eng, 2011; B176: 217

[4] Ciftja A, Engh T A, Tangstad M, Anne K, Johannes O E. J Miner Met Mater Soc, 2010; 51: 56

[5] Pires J C S, Otubo J, Braga A F B, Mei P R. J Mater Process Technol, 2005; 169: 21

[6] Rousseau S, Benmansour M, Morvan D, Amouroux J. Solar Energy Mater Solar Cells, 2007; 91: 1906

[7] Hunt L P, Dosaj V D, McCormick J R, Crossman L D. Proc International Symposium on Solar Energy, Washington DC, Moly 5–17, 1976: 200

[8] Chu T L, Chu S S. J Electrochem Soc, 1983; 130: 455

[9] Dietl J. Sol Cells, 1983; 10: 145

[10] Ma X D, Zhang J, Wang T M, Li T J. Rare Met, 2009; 28: 221

[11] Santos I C, Goncalves A P, Santos C S, Almeida M, Afonso M H, Cruz M J. Hydrometallurgy, 1990; 23: 237

[12] Yu Z L, Ma W H, Dai Y N, Yang B, Liu D C, Dai W P, Wang J X. Trans Nonferrous Met Soc China, 2007; 17: 1030

[13] Aulish H A, Eisenrith K H, Urbach H P. J Mater Sci, 1984; 19: 1710

[14] Aratani F, Sakaguchi Y, Yuge N. Bull Jpn Inst Met, 1991; 30: 433

[15] Schulze F W, Fenzl H J, Geim K, Hecht H D, Aulich H A. in Ralph E L ed.. Proc 17th IEEE Photovoltaic Specialists Conf, New York: IEEE, 1984: 584

[16] Nohira T, Yasuda K, Ito Y. Nat Mater, 2003; 2: 397

[17] Deng Y, Wang D, Xiao W, Jin X, Hu X, Chen G Z. J Phys Chem, 2005; 109B: 14043

[18] Pistorius P C, Fray D J. J South Afr Inst Min Metall, 2006; 106: 31

[19] Yasuda K, Nohira T, Hagiwara R, Ogata Y H. Electrochim Acta, 2007; 53: 106

[20] Li J, Yan J F, Lai Y Q, Tian A L, Jia M, Yi J G. Acta Energy Solar Sin, 2010; 31: 1068

(李劬, 闫剑锋, 赖延清, 田忠良, 贾明, 伊继光. 太阳能学报, 2010; 31: 1068)

[21] Cai Z Y, Li Y G, He X F, Liang J L. Metall Mater Trans, 2010; 41B: 1033

[22] SGTE. http://www.sgte.org/fact/documentation/FTsalt/ CaCl2–NaCl.jpg

[23] Wang S L, Zhang F S, Liu X, Zhang L J. Thermo Acta, 2008; 470: 105

[24] Katsutoshi O, Ryosuke O S. JOM, 2002; 54: 59

[25] Schwandt C, Fray D J. Electrochim Acta, 2005; 51: 66

[26] Wang S L, Wang W, Li S C, Cao S H. IJMMM, 2010; 17: 791

[27] Luo Y R. Handbook of Chemical Bonding Energy. Beijing: Science press, 2005: 48

(罗渝然. 化学键能数据手册. 北京: 科学出版社, 2005: 48)

[28] Liang Y J, Che Y C. Handbook of Thermodynamic Data of of Inorganic Substances. Shenyang: Northeastern University press, 1993: 1

(梁英教, 车阴昌. 无机物热力学数据手册. 沈阳: 东北大学出版社, 1993: 1)

[29] SGTE. http://www.crct.polymtl.ca/fact/phase diagram.php? file=Cu–Si.jpg&dir=SGTE

[30] Zhang Z X, Wang R K. Principle and Method of Electrochemistry. Beijing: Science Press, 2000: 55

(张祖训, 汪尔康. 电化学原理与方法. 北京: 科学出版社, 2000: 55)
Outlines

/