PHASES AND ELEMENTAL DISTRIBUTIONS IN SiCp/Al–Cu–Mg COMPOSITE FABRICATED BY POWDER METALLURGY

  • ZHANG Qi ,
  • YU Quan-Zhao ,
  • XIAO Ba-Lv ,
  • MA Zong-Xi
Expand
  • 1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    2. School of Chemistry and Materials Science, University of Science and Technology of China, Hefei 230026

Received date: 2011-07-22

  Revised date: 2011-11-09

  Online published: 2012-02-11

Supported by

Supported by National Basic Research Program of China (No.2012CB619600)

Abstract

SiCp/2009Al composites were fabricated through powder metallurgy and subsequent extrusion. The phases and elemental distributions in the hot pressed and extruded composites were studied. The slight macro–segregation was found in the hot pressed composite billet. The concentrations of Cu and Mg in the bottom of the billet are somewhat higher than those in the top of the billet. The hot pressed composite contains Al, SiC, Al2Cu, Mg2Si and a small quantity of Al7Cu2Fe and oxide of Mg. After solid solution treatment, Al2Cu and Mg2Si dissolved into the matrix and Cu was distributed uniformly in the matrix. However, Mg was still preferentially distributed near the boundaries of the Al particles and in the clusters of SiC. No change of the phases types in the composites was found, however, the extrusion resulted in uniformly distribution of the SiC particles and broke up the oxide shell of the initial Al particles, thus Cu and Mg were distributed homogeneously in the extruded composites after solid solution treatment.

Cite this article

ZHANG Qi , YU Quan-Zhao , XIAO Ba-Lv , MA Zong-Xi . PHASES AND ELEMENTAL DISTRIBUTIONS IN SiCp/Al–Cu–Mg COMPOSITE FABRICATED BY POWDER METALLURGY[J]. Acta Metall Sin, 2012 , 48(2) : 135 -141 . DOI: 10.3724/SP.J.1037.2011.00472

References

[1] Lloyd D J. Int Mater Rev, 1994; 39: 1

[2] Geiger A L, Walker J A. JOM, 1991; 43: 8

[3] Hong S H, Chung K H. Mater Sci Eng, 1995; A194: 165

[4] Song M, He Y H. Mater Des, 2010; 31: 985

[5] Jin P, Xiao B L, Wang Q Z, Ma Z Y, Liu Y, Li S. Acta Metall Sin, 2011; 47: 298

(金鹏, 肖伯律, 王全兆, 马宗义, 刘越, 李曙. 金属学报, 2011; 47: 298)

[6] Jin P, Xiao B L, Wang Q Z, Ma Z Y, Liu Y, Li S. Mater Sci Eng, 2011; A528: 1504

[7] Ogel B, Gurbuz R. Mater Sci Eng, 2001; A301: 213

[8] Zhou J, Duszczyk J. J Mater Sci, 1999; 34: 545

[9] Liu Z Y, Wang Q Z, Xiao B L, Ma Z Y, Liu Y. Mater Sci Eng, 2010; A527: 5582

[10] Mondolfo L F. Aluminum Alloys: Structure and Properties, London: Butterworths, 1976: 1

[11] Kiourtsidis G E, Skoliano S M, Litsardakis G A. Mater Sci Eng, 2004; A382: 351

[12] Urena A, Martinez E E, Rodrigo P, Gil L. Compos Sci Technol, 2004; 64: 1843

[13] Li Y, Li P, Zhao G, Liu X T, Cui J Z. Mater Sci Eng, 2005; A397: 204

[14] Rodrigo P, Poza P, Utrilla V, Urena A. J Alloys Compd, 2009; 479: 451

[15] Mcleod A D, Gabryel C M. Metall Trans, 1992; A23: 1279

[16] Strangwood M, Hippsley C A, Lewandowski J J. Scr Metall Mater, 1990; 24: 1483

[17] Nutt S R, Carpenter R W. Mate Sci Eng, 1985; 75: 169

[18] Kimura A, Shibata M, Kondoh K, Takeda Y, Katayama M, Kanie T, Takada H. Appl Phys Lett, 1997; 70: 3615

[19] Ma Z Y, Lu Y X, Luo M, Bi J. J Mater Sci Technol, 1995; 11: 291

[20] Liu Z Y, Wang Q Z, Xiao B L, Ma Z Y, Liu Y. Acta Metall Sin, 2010; 46: 1121

(刘振宇, 王全兆, 肖伯律, 马宗义, 刘越. 金属学报, 2010; 46: 1121)

[21] Gutin S S, Panov A A, Khlopin M I. Powder Metall Met Ceram, 1972; 11: 280
Outlines

/

〈 〉