论文

DESIGN AND INVESTIGATION ON THE HOT ROLLING TWIP STEEL WITH TRIP EFFECT

  • LIU Ren-Dong ,
  • SHI Wen ,
  • HE Yan-Lin ,
  • FU Ren-Yu ,
  • ZHANG Mei ,
  • LI Lin ,
  • ZHANG Xiao-Gang ,
  • YU Fu
Expand
  • 1) School of Materials and Metallurgy, Northeastern University, Shenyang 110819
    2) Technology Center, Anshan Iron and Steel Group Corporation, Anshan 114009
    3) School of Materials Science and Engineering, Shanghai University, Shanghai 200072

Received date: 2011-06-17

  Revised date: 2011-12-01

  Online published: 2012-01-11

Supported by

Supported by National Basic Research Program of China (No.{\footnotesize\it 2010CB630802}) and National Natural Science Foundation of China (Nos.50934011 and 50971137)

Abstract

There exists obvious deficiency in traditional twining induced plasticity (TWIP) steel which exhibits excessive ductility but rather low strength. In order to improve the property, new composition of a test steel, i.e., Fe-18Mn-0.528Si-0.6C (mass fraction, %) steel is designed through increasing C content and decreasing Mn content upon the estimation result of stack fault energy and phase diagram calculation. That the γ→ε transformation may happen during deformation at room temperature in the designed steel is predicted through calculation. The microstructure, before and after tensile test, of the hot rolling test steel is analyzed with OM, XRD and TEM. It is shown that there occurs simultaneously TWIP and transformation induced plasticity (TRIP) effect in the steel treated by a special hot rolling process (rolling starting temperature 1100 ℃, finishing rolling temperature 850 ℃\linebreak and air cooling) and superior mechanical property with strength higher than 1 GPa and elongation rate higher than 60\% are then obtained which fit very well with the requirement of the third generation automobile steel. It is also revealed the existence of ε martensite obtained through quenching or induced by stress would damage the mechanical property.

Cite this article

LIU Ren-Dong , SHI Wen , HE Yan-Lin , FU Ren-Yu , ZHANG Mei , LI Lin , ZHANG Xiao-Gang , YU Fu . DESIGN AND INVESTIGATION ON THE HOT ROLLING TWIP STEEL WITH TRIP EFFECT[J]. Acta Metall Sin, 2012 , 48(1) : 122 -128 . DOI: 10.3724/SP.J.1037.2011.00375

References

[1] Grassel O, Frommeyer G, Derder C, Hofmann H. J Phys IV, 1997; 7(C5): 383

[2] Vercammen S, Blanpain B, De Cooman B C, Wollants P. Acta Mater, 2004; 52: 2005

[3] Remy L, Pineau A. Mater Sci Eng, 1977; 28: 99

[4] Frommeyer G, Br¨ux U, Neumann P. ISIJ Int, 2003; 43: 438

[5] Sato K, Ichinose M, Hirotsu Y, Inoue Y. ISIJ Int, 1989; 29: 868

[6] Allain S, Chateau J P, Bouaziz O, Migot S, Guelton N. Mater Sci Eng, 2004; A387–389: 158

[7] Dumay A, Chateau J P, Allain S, Migot S, Bouaziz O. Mater Sci Eng, 2008; A483–484: 184

[8] Lee Y K, Choi C S. Metall Mater Trans, 2000; 31A: 355

[9] Kim J Y, Lee S J, De Cooman B C. 1st Int Conf on High Manganese Steels, Seoul, Korea, CD–ROM, 2011: A19

[10] Li L, Gao Y, Shi W, Liu R D, He Y L, Fu R Y, Zhang M. 1st Int Conf on High Manganese Steels, Seoul, Korea,CD–ROM, 2011: A40

[11] Edmonds D V, Speer J G. Mater Sci Technol, 2010; 26: 386

[12] Olson G B, Cohen M. Metall Trans, 1976; 7A: 1897

[13] Inden G. Z Metallk, 1977; 68: 529

[14] Hillert M, Jarl M. Calphad, 1978; 2: 227

[15] Dinsdale A T. Calphad, 1991; 15: 317

[16] Li L, Hsu T Y. Calphad, 1997; 21: 443

[17] Chou K C. Calphad, 1995; 19: 315

[18] Li L. Transformation Induced Plasticity Steel-Principles, Properties, Design and Application. Beijing: Science Press, 2009: 3

(李麟. 相变塑性钢---原理、性能、设计和应用. 北京: 科学出版社, 2009: 3)
Outlines

/

〈 〉