论文

THREE-DIMENSIONAL MICROSTRUCTURE RECONSTRUCTION AND THE EUTECTIC SPACING ADJUSTMENT DURING DIRECTIONAL SOLIDIFICATION OF Al-40%Cu HYPEREUTECTIC ALLOY

  • LI Shuang-Meng ,
  • DIAO Peng ,
  • FU Heng-Zhi
Expand
  • State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072

Received date: 2011-07-15

  Revised date: 2011-12-12

  Online published: 2012-01-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50971101 and 51074127) and Basic Research Foundation of NWPU (No.JC201029)

Abstract

Three-dimensional (3D) microstructures can clearly reveal the size, shape and distribution of the phases, providing a novel way to deeply understand the formation mechanism of the solidified phases. In this paper, by using the serial sectioning technique, the 3D microstructure of the primary Al2Cu phase was reconstructed and the eutectic spacing adjustment was investigated during directional solidification of Al-40%Cu hypereutectic alloy. The results show that the primary Al2Cu phase pattern was observed faceting due to the growing faceted angle and plane parallel to the solidification direction at the pulling rate of 5 μm/s. Further, there existed some hopper-like cavities in the 3D microstructure of the primary Al2Cu phase that caused by remelting owing to a large amount of the latent heat difficult to be extracted from the solidification interface. For the 3D eutectic microstructures of the Al-40%Cu alloy, the growth direction of the Al and Al2Cu phases in the coupled eutectics had a deviation angle of 5.1o with the heat flux direction and the phase volume fractions of the  Al and Al2Cu phases were measured directly to be 56.8% and 43.2%, respectively. In addition, at the abrupt change in pulling rate from 2 μm/s to 500 μm/s, the lamellar-to-rod eutectic transition was observed and the continuously splitting and branching occurred in different planes responsible for the eutectic spacing adjustment in the 3D microstructure of the Al-40%Cu alloy. Meanwhile the renuleation mechanism in the 2D microstructure for the adjustment of the eutectic spacing did not work in the 3D eutectic microstructure of the Al-40%Cu alloy.

Cite this article

LI Shuang-Meng , DIAO Peng , FU Heng-Zhi . THREE-DIMENSIONAL MICROSTRUCTURE RECONSTRUCTION AND THE EUTECTIC SPACING ADJUSTMENT DURING DIRECTIONAL SOLIDIFICATION OF Al-40%Cu HYPEREUTECTIC ALLOY[J]. Acta Metall Sin, 2012 , 48(1) : 33 -40 . DOI: 10.3724/SP.J.1037.2011.00450

References

[1] Spanos G. Scr Mater, 2006; 55: 3

[2] Isheim D, Kolli R P, Fine M E, Seidman D N. Scr Mater, 2006; 55: 35

[3] Liu H H, Schmidt S, Poulsen H F, Godfrey A, Liu Z Q, Sharon J A, Huang X. Science, 2011; 332: 833

[4] Khor K H, Buffiere J Y, Ludwig W, Sinclair I. Scr Mater, 2006; 55: 47

[5] Spowart J E. Scr Mater, 2006; 55: 5

[6] Mendoza R, Savin I, Thornton K, Voorhees P W. Nat Mater, 2004; 3: 385

[7] Wu D T. Nat Mater, 2004; 3: 353

[8] Kammer D, Voorhees P W. Acta Mater, 2006; 54: 1549

[9] Kammer D, Mendoza R, Voorhees P W. Scr Mater, 2006; 55: 17

[10] Luo L S, Wang X, Su Y Q, Li X Z, Guo J J, Fu H Z. Mater Rev, 2010; 24: 1

(骆良顺, 王新, 苏彦庆, 李新中, 郭景杰, 傅恒志. 材料导报, 2010; 24: 1)

[11] Lee J H, Liu S, Trivedi R. Metall Mater Trans, 2005; 36A: 3111

[12] Norris S A, Davis S H, Watson S J, Voorhees P W. J Cryst Growth, 2008; 310: 414

[13] Dantzig J A, Rappaz M. Solidification. Swiss: EPFL Press, 2009: 362

[14] Walkers H, Liu S, Lee J H, Trivedi R. Metall Mater Trans, 2007; 38A: 1417

[15] Quan Q R, Li S M, Fu H Z. Acta Metall Sin, 2010; 46: 500

(全琼蕊, 李双明, 傅恒志. 金属学报, 2010; 46: 500)

[16] Contieri R J, Rios C T, Zanotello M, Caram R. Mater Charact, 2008; 59: 693

[17] Singh H, Gokhale A M, Tewari A, Zhang S, Mao Y. Scr Mater, 2009; 61: 441

[18] Lee S G, Gokhale A M, Sreeranganathan A. Mater Sci Eng, 2006; 427: 92

[19] Liu S, Lee J H, Enlow D, Trivedi R. In: Rappaz M, Beckermann C, Trivedi R eds., Solidification Processes and Microstructures. Charlotte: TMS, 2004: 257

[20] Hunt J D, Liu S Z. Handbook of Crystal Growth, Vol.2, North–Holland: Elsevier, 1994: 1113

[21] Stefanescu D M. Science and Engineering of Casting Solidification. 2nd Ed., Berlin: Springer, 2009: 215

[22] Kurz W, Fisher D J. Fundamentals of solidification. 4th Ed., Switzerland: Trans Tech Pub, 2005: 109

[23] Tang L, Li S M, Fu H Z. Rare Met Mater Eng, 2007; 36: 617

(唐玲, 李双明, 傅恒志. 稀有金属材料与工程, 2007; 36: 617)

[24] Sunagawa I. Morphology and Perfection. Cambridge: Cambridge University Press, 2005: 370

[25] Colfen H, Antonietti M. Mesocrystals and Nonclassical Crystallization. Mississauga: John Wiley & Sons Ltd, 2008: 25

[26] Singh H, Gokhale A M, Mao Y, Tewari A, Sachdev A K. J Cryst Growth, 2009; 311: 4454

[27] Cantor B, Chadwick G A. J Cryst Growth, 1974; 23: 12

[28] Seetharamn V, Trivedi R. In: Stefanescu D M, Abbashian G J eds., Solidification Processing of Eutectic Alloys. Cincinnati: TMS, 1988: 65

[29] Hu H Q. Theory of Metal Solidification. 2nd Ed., Beijing: China Machine Press, 2000: 175

(胡汉起. 金属凝固原理. 第2版, 北京: 机械工业出版社, 2000: 175)
Outlines

/

〈 〉