论文

LARGE EDDY SIMULATION FOR UNSTEADY TURBULENT FLOW IN THIN SLAB CONTINUOUS CASTING MOLD

  • LI Bao-Kuan ,
  • LIU Zhong-Qiu ,
  • ZI Feng-Sheng ,
  • YU Fang ,
  • XU Guo-Dong
Expand
  • 1) Department of Materials and Metallurgy, Northeastern University, Shenyang 110819
    2) Baoshan Iron and Steel Limited Company, Shanghai 201900

Received date: 2011-07-19

  Revised date: 2011-12-09

  Online published: 2012-01-11

Supported by

Supported by National Natural Science Foundation of China (No.50934008)

Abstract

Unsteady turbulent flow in the thin slab continuous casting mold has been computed using the large eddy simulations (LES). The cassette filter function is used to deal with unsteady Navier-Stokes equation, and the Smagorinsky-Lilly sub-grid scale model is used to calculate the dissipative effort of the unresolved small eddies. And this LES model has been validated with the measurements of the particle image velocimetry (PIV) and the ultrasonic flaw detection. The computational domain includes the entire submerged entry nozzle (SEN) starting from the tundish exit and the extended mold region. The results show the characteristics of the unsteady turbulent flow in the thin slab continuous casting processes, such as the vortices distribution and the formation, development, shedding and fracture process of the large eddy coherent structures. The simulation also shows that the turbulent flow is asymmetric even if the nozzle and mold is perfect symmetric in geometry. The flow deviation of the molten steel in the mold is inevitable existence. And the interactions of flows in two sides of nozzle also can cause intensity velocity fluctuation near the meniscus. With the development of the unsteady turbulent flow, the flow deviation of the molten steel in the thin continuous casting strand presented periodic change, and the period is about 40 s.

Cite this article

LI Bao-Kuan , LIU Zhong-Qiu , ZI Feng-Sheng , YU Fang , XU Guo-Dong . LARGE EDDY SIMULATION FOR UNSTEADY TURBULENT FLOW IN THIN SLAB CONTINUOUS CASTING MOLD[J]. Acta Metall Sin, 2012 , 48(1) : 23 -32 . DOI: 10.3724/SP.J.1037.2011.00464

References

[1] Ho Y, Chen C, Wang WH. ISIJ Int, 1994; 24: 255

[2] Bai H, Thomas B G. Metall Mater Trans, 2001; 32B: 253

[3] Miki Y J, Thomas B G. Metall Mater Trans, 1999; 30B: 639

[4] Hershey D E, Thomas B G, Najjar F M. Int J Numer Methods Fluids, 1993; 17: 23

[5] Bai H, Thomas B G. Metall Mater Trans, 2001; 32B: 269

[6] Aboutalebi M R, Hasan M, Guthrie R I L. Metall Mater Trans, 1995; 26B: 731

[7] Lan X K, Khodadadi J M, Shen F. Metall Mater Trans, 1997; 28B: 321

[8] Bastiaansa Rob J M, Rindta C C M, Nieuwstadtb F T M, Steenhovena A A. Int J Heat Mass Transfer, 2000; 43: 375

[9] Moser R D, Kim J, Mansour N N. Phys Fluids, 1999; 4: 943

[10] Lesieur M, Metais O. Annu Rev Fluid Mech, 1996; 28: 45

[11] Thomas B G, Yuan Q, Sivaramakrishnan S, Shi T, Vanka S P, Assar M B. ISIJ Int, 2001; 41: 1262

[12] Thomas B G, Huang X, Sussman R C. Metall Mater Trans, 1994; 25B: 527

[13] Yuan Q, Sivaramakrishnan S, Vanka S P, Thomas B G. Metall Mater Trans, 2004; 35B: 967

[14] Yuan Q, Thomas B G, Vanka S P. Metall Mater Trans, 2004; 35B: 685

[15] Li B K, Li D H. Acta Metall Sin, 2002; 38: 315

(李宝宽, 李东辉. 金属学报, 2002; 38: 315)

[16] Li B K, Tsukihashi F. ISIJ Int, 2001; 41: 844

[17] Li B K, Okane T, Umeda T. Metall Mater Trans, 2000; 31B: 1491

[18] Li B K, Okane T, Umeda T. Metall Mater Trans, 2001; 32B: 1053

[19] Qian Z D, Wu Y L. Acta Metall Sin, 2004; 40: 88

(钱忠东, 吴玉林. 金属学报, 2004; 40: 88)

[20] Tang X L, Qian Z D, Wu Y L. J Tsinghua Univ (Sci Technol), 2003; 6: 802

(唐学林, 钱忠东, 吴玉林. 清华大学学报(自然科学版), 2003; 6: 802)

[21] Real C, Miranda R, Vilchis C, Barron M, Hoyos L, Gonzalez J. ISIJ Int, 2006; 46: 1183

[22] Herring J R. Front Fluid Mech, 1984; 14: 68

[23] Germano M. J Fluid Mech, 1992; 238: 325

[24] Smagorinsky J. Mon Weather Rev, 1963; 91: 99

[25] Lilly D K. Mon Weather Rev, 1965; 93: 11

[26] Van Driest E R. J Spacecr Rockets, 2003; 40: 1012

[27] Li X S, Xu J Z, Gu C W. Sci China Ser G, 2009; 1: 83

(李雪松, 徐建中, 顾春伟. 中国科学G辑, 2009; 1: 83)

[28] Zhang L, Thomas B G. ISIJ Int, 2003; 43: 271

[29] Yuan Q, Thomas B G, Vanka S P. Metall Mater Trans, 2004; 35B: 703

[30] Shi X G. Turbulence. Tianjin: Tianjin University Press, 1994: 190

(是勋刚. 湍流. 天津: 天津大学出版社, 1994: 190)
Outlines

/

〈 〉