MICROSTRUCTURE CONTROL AND PREDICTION OF GH738 SUPERALLOY DURING HOT DEFORMATION
I. Construction of Microstructure Evolution Model

  • YAO Zhi-Gao ,
  • DONG Jian-Xin ,
  • ZHANG Mai-Cang
Expand
  • School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083

Received date: 2011-08-11

  Revised date: 2011-11-04

  Online published: 2011-12-11

Supported by

Supported by National Natural Science Foundation of China (No.51071017)

Abstract

The hot deformation behavior of GH738 superalloy with different initial grain sizes was studied using hot compression experiments via Gleeble–1500. Correlations between flow stress, process parameters and microstructure evolution were characterized in the temperature range of 1000—1160 ℃, strain rate range of 0.01—10 s−1 and engineering strain range of 15%—70%. Besides, metadynamic recrystallization and static recrystallization were studied in the temperature range of 1040—1120 ℃, strain rate range of 0.1—10 s−1 and engineering strain range of 15%—50% with soaking time for 0—45 s; grain growth behavior was researched in the temperature range 980—1140  with soaking time for 0—4 h. The results show that recrystallization behavior of GH738 superalloy was significantly affected by initial grain size, deformation temperature, strain and strain rate. Thermomechanical behavior and microstructural evolution models were systematically constructed based on the investigation of dynamic recrystallization, meta–dynamic recrystallization, static recrystallization and grain growth. The analyses indicate that these models shows a high correlation with actual results of GH738 superalloy.

Cite this article

YAO Zhi-Gao , DONG Jian-Xin , ZHANG Mai-Cang . MICROSTRUCTURE CONTROL AND PREDICTION OF GH738 SUPERALLOY DURING HOT DEFORMATION
I. Construction of Microstructure Evolution Model[J]. Acta Metall Sin, 2011
, 47(12) : 1581 -1590 . DOI: 10.3724/SP.J.1037.2011.00522

References

[1] Yao Z H, Dong J X, Zhang M C, Zheng L. Rare Met Mater Eng, 2010; 39: 1565

(姚志浩, 董建新, 张麦仓, 郑磊. 稀有金属材料与工程, 2010; 39: 1565)

[2] Chang K M, Liu X B. Mater Sci Eng, 2001; A308: 1

[3] Semiatin S L, Fagin P N, Glavicic M G. Scr Mater, 2004; 50: 625

[4] Liu X B, Kang B, Chang K M. Mater Sci Eng, 2003; A340: 8

[5] Yao Z H, Dong J X, Zhang M C, Yu Q Y, Zheng L. Trans Mater Heat Treat, 2011; 32: 44

(姚志浩, 董建新, 张麦仓, 于秋颖, 郑磊. 材料热处理学报, 2011; 32: 44)

[6] Donachie M J, Pinkowish A A, Danesi W P, Radavich J F, Couts W H. Metall Trans, 1970; 1: 2623

[7] Guimaraes A A, Jonas J J. Metall Trans, 1981; A12: 1655

[8] Livesey D W, Sellars C M. Mater Sci Technol, 1985; 1: 136

[9] Li M Q, Yao X Y, Luo J, Lin Y Y, Su S B, Wang H R. Acta Metall Sin, 2007; 43: 937

(李淼泉, 姚晓燕, 罗皎, 林莺莺, 苏少博, 王海荣. 金属学报, 2007; 43: 937)

[10] Salehi A R, Serajzadeh S, Yazdipour N.Mater Chem Phys, 2007; 101: 153

[11] Gao H, Barber G C, Chen Q A, Lu Y Q. J Mater Process Technol, 2003; 142: 52

[12] Ganapathysubramanian S, Zabaras N. Int J Solid Struct, 2004; 41: 2011

[13] Wang B X, Liu X H, Wang G D. Mater Sci Eng, 2005; A393: 102

[14] Sui F L, Xu L X, Chen L Q, Liu X H. J Mater Process Technol, 2011; 211: 433

[15] Zhao M L, Sun W R, Yang S L, Qi F, Guo S R, Hu Z Q. Acta Metall Sin, 2009; 45: 79

(赵美兰, 孙文儒, 杨树林, 祁峰, 郭守仁, 胡壮麒. 金属学报, 2009; 45: 79)

[16] Sellars C M, McTegart W J. Acta Metall, 1966; 14: 1136

[17] McQueen H J, Ryan N D. Mater Sci Eng, 2002; A322: 43

[18] Sommitsch C, Mitter W. Acta Metall, 2006; 54: 357

[19] Gottstein G, Frommert M, Goerdeler M, Schafer N. Mater Sci Eng, 2004; A387–389: 604

[20] Solhjoo S. Mater Des, 2010; 31: 1360

[21] Poliak E I, Jonas J J. ISIJ Int, 2003; 43: 692

[22] Li G, Maccagno T M, Bai D Q. ISIJ Int, 1996; 36: 1479

[23] Bai D Q, Yue S, Jonas J J. ISIJ Int, 1996; 36: 1084

[24] Shen B Z, Fang N W, Shen H F, Liu B C. Mater Sci Technol, 2005; 13: 516

(沈丙振, 方能炜, 沈厚发, 柳百成. 材料科学与工艺, 2005; 13: 516)

[25] Li G, Maccagno T M, Bai D Q. ISIJ Int, 1996; 36: 1479

[26] Sellars C M, Whiteman J A. Met Sci, 1979; 13: 187

[27] Anelli E. ISIJ Int, 1992; 32: 440
Outlines

/