The quenching–partitioning–tempering (Q–P–T) process was developed from quenching & partitioning (Q&P) process and their difference are first described in this paper. The development of Q–P–T steels from ultrahigh strength to high strength–ductility is summarized. Novel Q–P–T process and conventional quenching–tempering (Q–T) process and their different effects on mechanical properties are compared. The micro–mechanism of the ductility enhancement from retained austenite in unltrahigh strength steels during deformation is emphasized in discussion, which is as a theoretical direction of microstructural design and control on the further development of advanced high strength steels.
RONG Yong-Hua
. ADVANCED Q–P–T STEELS WITH ULTRAHIGH STRENGTH–HIGH DUCTILITY[J]. Acta Metall Sin, 2011
, 47(12)
: 1483
-1489
.
DOI: 10.3724/SP.J.1037.2011.00514
[1] Sakuma Y. In: Baker M A ed., Proc Int Conf on Advanced High Strength Sheet Steels for Automotive Applications. Warrendale: Association for Iron–Steel Technology, 2004: 11
[2] Sugimoto K, Kobayshi M, Hashimoto S. Metall Trans, 1992; 23: 3085
[3] Speer J G, Matlock D K, Cooman B C, Schroch J G. Acta Mater, 2003; 51: 2661
[4] Matlock D K, Brautigam V E, Speer J G. Mater Sci Forum, 2003; 426–432: 1089
[5] Wang X D, Zhong N, Rong Y H, Xu Z Y. J Mater Res, 2009; 24: 261
[6] Matlock D K, Speer J G. In: Lee H C ed., The 3rd Int Conf on Advanced Structural Steels. Korea: The Korean Institute of Metals and Materials, 2006: 774
[7] Hillert M, Agren J. Scr Mater, 2004; 50: 697
[8] Hillert M, Agren J. Scr Mater, 2005; 52: 87
[9] Speer J G, Matlock D K, DeCooman B C, Schroth J G. Scr Mater, 2005; 52: 83
[10] Speer J G, Edmonds D V, Rizzo F C, Matlock D K. Corruent Opinon Solid State Mater Sci, 2004; 8: 219
[11] Zhong N, Wang X D, Rong Y H, Wang L. J Mater Sci Technol, 2006; 22: 751
[12] Speer J G, Hackenberg R E, Decooman B C, Matlock D K. Philos Mag Lett, 2007; 87: 379
[13] Koistinen D P, Marburger R E. Acta Metall, 1959; 7: 59
[14] Zhong N. PhD Thesis, Shanghai Jiao Tong University, 2009
(钟宁. 上海交通大学博士学位论文, 2009)
[15] Xu Z Y. Mater Sci Forum, 2007; 2283: 561
[16] Zhong N, Wang X D, Rong Y H, Wang L. Mater Sci Eng, 2009; 506: 111
[17] Bhadeshia H K D H. Mater Sci Technol, 2005; 21: 1293
[18] Krauss G. Metall Trans, 2001; 32B: 205
[19] Lu L, Sui M L, Lu K. Science, 2000; 287: 1463
[20] Rong Y H. Requisition of National Natural Science Foundation of China (No.51031001)
(戎咏华. 国家自然科学基金重点项目申请书(批准号: 51031001))
[21] Zhang K, Xu W Z, Guo Z H, Rong Y H, Wang M Q, Dong H. Acta Metall Sin, 2011; 47: 489
(张柯, 许为宗, 郭正洪, 戎咏华, 王毛球, 董瀚. 金属学报, 2011; 47: 489)
[22] Zhang K, Zhang M H, Guo Z H, Chen N L, Rong Y H. Mater Sci Eng, 2011; 528: 8486
[23] Zackay V F, Parker E R, Fahr D, Busch R. Trans ASM, 1967; 60: 252
[24] Morris Jr J W, Lee C S, Guo Z. ISIJ Int, 2003; 43: 410