HOT COMPRESSION DEFORMATION BEHAVIOR OF Mg–Zn–Al–(Y) ALLOYS REINFORCED WITH QUASICRYSTAL

  • ZHONG Jian ,
  • HUANG Hua ,
  • YUAN An-Yin ,
  • DING Wen-Jiang
Expand
  • 1. Light Alloy Net Forming National Engineering Research Center, School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240
    2. The State Key Laboratory of Metal Matrix Composite, School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240

Received date: 2011-06-17

  Revised date: 2011-10-14

  Online published: 2011-12-11

Supported by

Supported by National Natural Science Foundation of China (No.51174136), Specialized Research Fund for the Doctoral Program of Higher Education of China (No.20100073110004) and Science and Technology Commission of Shanghai Municipality (No.10JC1407400)

Abstract

Quasicrystal phase offers a good combination of strength and ductility due to the strong interface between the quasicrystal phase and the Mg–matrix. Hot compression tests of Mg–Zn–Al–(Y) based alloys reinforced with quasicrystal were performed on Gleeble–1500 thermal simulation machine at a constant deformation temperature of 230℃ and strain rates ranged from 0.0015 s−1 to 1.5 s−1. Microstructure evolution of hot–compressed Mg–Zn–Al–(Y) alloys and the relationship between flow stress and strain rate were studied. XRD and SAED results show that the microstructures of as–cast Mg–8Zn–4Al (ZA84) andMg–8Zn–4Al–0.5Y (ZAY8405) are composed of icosahedral quasicrystal phase and α-Mg matrix. The quasicrystals in ZA84 and ZAY8405 alloys have a stoichiometric composition of Mg38Zn43Al19 and Mg51Zn30Al19 respectively. Dynamic recrystalization (DRX) take place during hot compression and the flow stress increases with increase of strain rate at constant compression temperature, which can be represented by the Power Exponential Equation. Deformation twinning and dynamic recrystalization are easier to take place in ZAY8405 alloys due to the refined and dispersed quasicrystal phase with Y addition.

Cite this article

ZHONG Jian , HUANG Hua , YUAN An-Yin , DING Wen-Jiang . HOT COMPRESSION DEFORMATION BEHAVIOR OF Mg–Zn–Al–(Y) ALLOYS REINFORCED WITH QUASICRYSTAL[J]. Acta Metall Sin, 2011 , 47(12) : 1520 -1526 . DOI: 10.3724/SP.J.1037.2011.00372

References

[1] Decker R F. Adv Mater Processes, 1998; 154(3): 31

[2] Liu Q. Acta Metall Sin, 2010; 46: 1458

(刘庆. 金属学报, 2010; 46: 1458)

[3] Lu Y Z, Wang Q D, Ding W J. Mater Lett, 2000; 44: 265

[4] Mukai T, Yamanoi M,Watanabe H, Higashi K. Scr Mater,2001; 45: 89

[5] Kim W J, Hong S I, Kim Y S. Acta Mater, 2003; 51: 3293

[6] Yang X Y, Zhang L. Acta Metall Sin, 2009; 45: 1303

(杨续跃, 张 雷. 金属学报, 2009; 45: 1303)

[7] Jin Q L, Shim S Y, Lim S G. Scr Mater, 2006; 55: 843

[8] Shechtman D, Blech I, Gratias D, Cahn J W. Phys Rev Lett, 1984; 53: 1951

[9] Yuan G Y, Liu Y, DingWJ. Mater Sci Eng, 2008; A474: 348

[10] Liu Y, Yuan G Y, Lu C. J Mater Sci, 2008; 43: 5527

[11] Somekawa H, Singh A, Mukai T. Adv Eng Mater, 2009; 11: 782

[12] Yuan G Y, Amiya K, Kato H, Inoue A. J Mater Res, 2008; 19: 1531

[13] Elser V. Phys Rev, 1985; 32B: 4892

[14] Bourgeois L, Mendis C L, Muddle B C. Philos Mag Lett, 2001; 81: 709

[15] Vogel M, Kraft O, Behm G. Scr Mater, 2001; 45: 517

[16] Galiyev A, Kaibyshev R, Gottstein G. Acta Mater, 2001; 49: 1199

[17] Agnew S R, Yoo M H, Tome C N. Acta Mater, 2001; 49: 4277

[18] Li Z J, Jin Q L, Jiang Y H, Zhou R. Acta Metall Sin, 2009; 45: 924

(李再久, 金青林, 蒋业华, 周荣. 金属学报, 2009; 45: 924)

[19] Bae D H, Kim S H, Kim D H, Kim W T. Acta Mater, 2002; 50: 2343

[20] Singh A, Watanabe M, Kato A, Tsai A P. Sci Technol Adv Mater, 2005; 6: 895

[21] Lee J Y, Lim H K, Kim D H, Kim W T, Kim D H. Mater Sci Eng, 2008; A491: 349

[22] Hu G X, Cai X. Fundamental of Material Science. Shanghai: Shanghai Jiao Tong University Press, 2004: 193

(胡赓祥, 蔡旬.材料科学基础. 上海: 上海交通大学出版社, 2004: 193)

[23] Yu K, Shi T, Wang R C, Li W X, Wang X Y, Cai Z Y. J Cent South Univ (Sci Technol), 2008; 39: 216

(余琨, 史提, 王日初, 黎文献, 王晓艳, 蔡志勇.中南大学学报(自然科学版), 2008; 39: 216)

[24] Poirier J P, translated by Guan D L. The Plastic Deformation of Crystals at High Temperature. Dalian: Dalian University of Science and Technology Press, 1989: 25

(Poirier J P著, 关德林译. 晶体的高温塑性变形. 大连: 大连理工大学出版社,1989: 25)

[25] Takuda H, Fujimoto H, Hatta N. J Mater Process Technol,1998; 80–81: 513
Outlines

/

〈 〉