论文

EFFECT OF MULTIPASS HOT ROLLING ON THE PROPERTY AND BONDING INTERFACE OF CLAD BAR

  • XIE Hong-Biao ,
  • GAO Ya-Nan ,
  • YU Shou ,
  • XIAO Hong
Expand
  • Mechanical Engineering College, Yanshan University, Qinhuangdao 066004

Received date: 2011-06-10

  Revised date: 2011-10-03

  Online published: 2011-12-11

Supported by

Supported by National Natural Science Foundation of China (No.51075353) and Natural Science Foundation of Hebei Province (No.E2010001208)

Abstract

Because of climate and human factors, the corrosion of reinforced steel bar has become one of the important reasons of premature deterioration of concrete buildings and infrastructure. Stainless steel bar cannot be widely used due to its high price. Therefore, stainless steel clad carbon steel bar comes into being. It is a new material used in construction, which is made up of corrosion resistant stainless steel outer layer and carbon steel core. In the present study, an experimental study was conducted to investigate the mechanical property and bonding state of stainless steel clad carbon steel bar. The tensile strength of clad bar and bonding strength of two metals were measured using tension test and shearing test. Then, microscopic morphology, element diffusion and microhardness near the interface were analyzed using OM, SEM, EDS and microhardness tester. The results show that the two metals of the bar extend proportionally in the rolling process. The tensile strength is 550 MPa and the percentage of elongation is 45%. The neck phenomenon in the tensile experiment is obvious and the two metals are undivided in the fracture. With the increment of rolling pass, the bonding between the metals becomes denser and this increases the shearing strength. The max shearing strength is 333 MPa and the typical plastic dimples and shearing slip were observed on the shearing fracture surface.  Element diffusion occurs at the interface where the Cr, Mn, Ni of stainless steel diffuse into carbon steel and the Fe of carbon steel diffuses into stainless steel, and the total width of diffusion distance is about 30 μm. It makes the microhardness of the carbon steel near the interface increased significantly and the value is 399.4 HV which is higher than carbon steel after sixth pass rolling. Therefore, the metallurgical diffusion bonding is formed in the interface of clad bar.

Cite this article

XIE Hong-Biao , GAO Ya-Nan , YU Shou , XIAO Hong . EFFECT OF MULTIPASS HOT ROLLING ON THE PROPERTY AND BONDING INTERFACE OF CLAD BAR[J]. Acta Metall Sin, 2011 , 47(12) : 1513 -1519 . DOI: 10.3724/SP.J.1037.2011.00364

References

[1] Hwang Y M, Hsu H H, Hwang Y L. Int J Mech Sci, 2000; 42: 2417

[2] Kang H, Kim J, Huh M, Engler O. Mater Sci Eng, 2007; A452–453: 347

[3] Lee J, Bae D, Chung W, Kim K, Cho Y. J Mater Process Technol, 2007; 187–188: 546

[4] Soltanalinezhad M, Haerianardakani A. Mater Des, 2009; 30: 1103

[5] Zhang L, Meng L, Zhou S P, Yang F T. Mater Sci Eng, 2004; A371: 65

[6] Bulent K. J Mater Process Technol, 2007; 190: 138

[7] Motarjemi A K, Korcak M, Ventzke V. Int J Pres Ves Pip, 2002; 79: 181

[8] Li S X, Xuan F Z, Tu S T. J Nucl Mater, 2007; 366(1/2): 1

[9] Madaah–Hosseini H R, Kokabi A H. Mater Sci Eng, 2002; A335: 186

[10] Kundu S, Chatterjee S. Mater Sci Eng, 2006; A425(1/2): 107

[11] He P, Yue X, Zhang J. Mater Sci Eng, 2008; A486: 171

[12] Elrefaey A, Tillmann W. J Mater Process Technol, 2009; 209: 2746

[13] Wu C J, Wu Y, Xue Z Y, Liang H, Liu Q. Acta Metall Sin (Engl Lett), 2010; 23: 206

[14] Lesik L, Dyja H, Pilarczyk J W, Wiewiorowska S. Wire J Int, 2001; 34(2): 94

[15] Dyja H, Lesik L, Milenin A, Mroz S. J Mater Process Technol, 2002; 125–126: 731

[16] Berski S, Dyja H, Maranda A, Nowaczewski J, Banaszek G. J Mater Process Technol, 2006; 177: 582

[17] Manesh H, Taheri A. J Mater Process Technol, 2005; 166: 163

[18] Yuan J W, Pang Y H, Li T. J Wuhan Univ Technol, 2011; 26: 111

[19] Dyja H, Mroz S, Milenin A, Lesik L. In: International Rolling Conference ed., 44th MWSP Conference Proceeding, Orlando: Association for Iron & Steel, 2002: 40: 653

[20] Dyja H, Mroz S, Stradomski Z. Metalurgija, 2003; 42(3): 185

[21] Dyja H, Mroz S, Milenin A. J Mater Process Technol, 2004; 153–154: 100

[22] Szota P, Dyja H. J AMME, 2007; 25(1): 55

[23] Mroz S, Szota P, Dyja H, Kawalek A. Metalurgija, 2011; 50(2): 85

[24] Ricardo R. Master Dissertation, Massachusetts Institute of Technology, Cambridge, 2001

[25] Purk Y. Master Dissertation, North Carolina State University, Raleigh, 2003

[26] Gregory W. PhD Thesis, Virginia Polytechnic Institute and State University, Blacksburg, 2007
Outlines

/