论文

NUMERICAL SIMULATION ON TEMPERATURE FIELD IN HIGH SPEED STEEL COMPOSITE ROLL DURING CONTINUOUS POURING PROCESS FOR CLADDING
II. Copper Mould Method

  • FENG Meng-Jie ,
  • YU En-Gang ,
  • YU Jun-Gang ,
  • SHI Ji-Cheng
Expand
  • Key Laboratory of National Education Ministry for Electromagnetic Processing of Materials, Northeastern University, Shenyang 110819

Received date: 2011-04-02

  Revised date: 2011-05-21

  Online published: 2011-12-11

Supported by

Supported by National High Technology Research and Development Programme of China (No.2003AA331050) and National Natural Science Foundation of China (No.200809123)

Abstract

The effects of pouring temperature and casting speed on temperature field in high speed steel composite roll billet under copper mold and the selection of optimistic continuous casting technique parameters were studied by use of numerical simulation method based on Fluent 6.3 software. At the same time, the pouring billets experiment was also executed based on the simulation results. The results indicate that the casting speed and pouring temperature are the most important parameters to determine that a high speed steel composite roll billet can be well poured or not and the quality of interface of bimetal composite is better or not. Increases in pouring temperature and casting speed are conducive to metallurgical bond between the two metals, but their moreincreasing will make the depth of melting zone increase, the thickness of solidifying shell decrease and the feasibility of breakout increase. The simulated appropriate pulling temperature and casting speed are about 1873—1923 K and 0.3—0.5 m/min, respectively, which are proved by experiment results.

Cite this article

FENG Meng-Jie , YU En-Gang , YU Jun-Gang , SHI Ji-Cheng . NUMERICAL SIMULATION ON TEMPERATURE FIELD IN HIGH SPEED STEEL COMPOSITE ROLL DURING CONTINUOUS POURING PROCESS FOR CLADDING
II. Copper Mould Method[J]. Acta Metall Sin, 2011
, 47(12) : 1503 -1512 . DOI: 10.3724/SP.J.1037.2011.00194

References

[1] Walmag G, Skoczynski R J, Breyer J P. La Revue Metall–CIT, 2001; 98: 295

[2] Kunio G, yukio A. ISIJ Int, 1992; 32: 1131

[3] Sano Y, Thattori T, Haga M. ISIJ Int, 1992; 32: 1194

[4] Ichino K, Kataoka Y, Koseki T. Kawasaki Steel Technol Rep, 1997; 37(8): 13

[5] Feng M J, Wang E G, Wang J G, He J C. China Metall, 2006; 16(10): 14

(冯明杰, 王恩刚, 王俊刚, 赫冀成. 中国冶金, 2006; 16(10): 14)

[6] Feng M J, Wang E G, He J C. Acta Metall Sin, 2011; 47: 1495

(冯明杰, 王恩刚, 赫冀成. 金属学报, 2011; 47: 1495)

[7] Gan Y, Qiu S T, Xiao Z Q. Maths and Physics Simulation on Continuous Casting Steel. Beijing: Metallurgy Industry Press, 2001: 1

(干勇, 仇圣桃, 萧泽强. 连续铸钢过程数学物理模拟. 北京: 冶金工业出版社,2001: 1)

[8] Fu H G, Xing J D. Steel Res Int, 2007; 78: 266

[9] Lino G D, Rodolfo D M. Steel Res, 2001; 72: 346

[10] Yu H Q, Zhu M Y. Acta Metall Sin, 2008; 44: 1465

(于海岐, 朱苗勇. 金属学报, 2008; 44: 1465)

[11] Lei J M, Song W P, Cui X C. Chin J Mech Eng, 2001; 37(7): 74

(雷建民, 宋卫平, 崔小朝. 机械工程学报, 2001; 37(7): 74)

[12] Jin B G, Wang Q, Liu Y. Chin J Nonferrous Met, 2006; 16: 1931

(金百刚, 王强, 刘燕. 中国有色金属学报, 2006; 16: 1931)

[13] Meng X N, Zhun M Y, Liu X D. Acta Matell Sin, 2007; 43: 205

(孟祥宁, 朱苗勇, 刘旭东. 金属学报, 2007; 43: 205)

[14] Yu H Q, Zhu M Y. Acta Metall Sin, 2008; 44: 619

(于海岐, 朱苗勇. 金属学报, 2008; 44: 619)

[15] Ren B Z, Zhu M Y, Wang H D. Acta Metall Sin, 2008; 44: 507

(任兵芝, 朱苗勇, 王宏丹. 金属学报, 2008; 44: 507)

[16] Xia X J, Wang H M, Dai Q X, Li G R, Zhao Y T. Chin J Nonferrous Met, 2008; 18: 529

(夏小江, 王宏明, 戴起勋, 李桂荣, 赵玉涛. 中国有色金属学报, 2008; 18: 529)

[17] Feng M J, Wang E G, Deng A Y, He J C. J Northeast Univ (Nat Sci), 2006; 27: 665

(冯明杰, 王恩刚, 邓安元, 赫冀成. 东北大学学报(自然科学版), 2006; 27: 665)
Outlines

/