SOLIDIFICATION MECHANISM OF TERNARY QUASIPERITECTIC ALLOY OF Al-11.8Cu-24.22Mg

  • YAN Er-Hu ,
  • LI Xin-Zhong ,
  • XU Ta-Ming ,
  • DIAO Guang-Wei ,
  • GUO Jing-Jie ,
  • FU Heng-Zhi
Expand
  • 1) School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001
    2) State Key Lab of Mold & Die Technology, Huazhong University of Science and Technology, Wuhan 430074

Received date: 2011-06-02

  Revised date: 2011-07-19

  Online published: 2011-11-11

Supported by

Supported by National Natural Science Foundation of China (Nos.51071062 and 50801019), Open Project of State Key Lab of Mold $\&$ Die Technology of Huazhong University of Science and Technology (No.2011-P03) and National Basic Research Program of China (No.2011CB610406)

Abstract

In the field of condensed matter physics and materials science, it is of great importance to investigate the microstructures, properties and solidification regularities of liquid metals. In the last few decades, the theories of solidification of binary alloys, such as dendritic growth and eutectic growths have been built. Great progress has also been made on the study of monetectic and peritectic alloys. But a solidification theory on ternary quasiperitectic alloys has not been established up to now. The study of the solidification process of quasiperitectic alloys will provide a basic work for solidification theories of ternary alloys.
The master alloy of Al-11.8Cu-24.22Mg was prepared from pure Al (99.99%), pure Mg (99.99%) and Al-54.2Cu in a resistance furnace under CO2 and SF6 (volume proportion is 40∶1) atmosphere. The melted alloy (840-850℃) was pouring into different quenching graphite crucibles at the same time, and the cooling curves were recorded by a sixteen channels temperature recorder. The graphite crucible was quenched into cold--water immediately for rapid cooling at the preplanned quenching temperature. After the experiment, the microstructures of the sample were analyzed by SEM, with EDS analysis.
The experiment result indicates that the primary phase is identified as S (Al2CuMg) and the quasiperitectic phases are α-Al and T (Al6CuMg4). The solidification microstructure is composed of remnant primary phase, quasiperitectic phases, binary eutectic and ternary eutectic. Although the quasiperitectic phases and binary eutectic are composed of the same phases (α-Al+T(Al6CuMg4)), their structures are different. The former structure presents strip form and the later present dendritic form. The ternary eutectic reaction is suppressed and the remnant primary S phase is reserved in the matrix with non-equilibrating crystallization.

Cite this article

YAN Er-Hu , LI Xin-Zhong , XU Ta-Ming , DIAO Guang-Wei , GUO Jing-Jie , FU Heng-Zhi . SOLIDIFICATION MECHANISM OF TERNARY QUASIPERITECTIC ALLOY OF Al-11.8Cu-24.22Mg[J]. Acta Metall Sin, 2011 , 47(11) : 1464 -1469 . DOI: 10.3724/SP.J.1037.2011.00346

References

[1] Li L, Lu X Y, Dai F P. Foundry Technol, 2008; 29: 601

(李丽, 鲁晓宇, 代富平. 铸造技术, 2008; 29: 601)

[2] Lipton J, Kurz W, Trivedi R. Acta Metall, 1987; 35: 957

[3] Trivedi R, Lipton J, Kurz W. Acta Metall, 1987; 35: 965

[4] Jackson K, Hunt J. Trans AIME, 1966; 236: 1129

[5] Kurz W, Fisher D J. Acta Metall, 1980; 28: 777

[6] Trivedi R, Magnin P, Kurz W. Acta Metall, 1987; 35: 971

[7] Hillig W B, Mccarroll B. J Chem Phys, 1966; 45: 3887

[8] Wang N, Wei B. Mater Sci Eng, 2003; A345: 145

[9] Kerr H W, Kurz W. Int Mater Rev, 1996; 41: 129

[10] Boettinger W J, Coriell S R, Greer A L, Karma A, Kurz W, Rappaz M, Trivedi R. Acta Mater, 2000; 48: 43

[11] Asta M, Beckermann C, Karma A, Kurz W, Napolitano R, Plapp M, Purdy G, Rappaz M, Trivedi R. Acta Mater, 2009; 57(4): 941

[12] Sha G, Reilly K A Q O, Cantor B, Tichmarsh J M, Hamerton R G. Acta Mater, 2003; 51: 1883

[13] Raghavan V. JPEDAV, 2007; 28: 174

[14] Chen Z M. J Shandong Inst Technol, 2001; 15(3): 25

(陈宗明. 山东工程学院学报, 2001; 15(3): 25)

[15] Li L, Lu X Y, Cao C D, Dai F P. Chin Sci Bull, 2009; 54: 2108

(李丽, 鲁晓宇, 曹崇德, 代富平. 科学通报, 2009; 54: 2108)

[16] Fan L, Lu X Y, Dai F P. Foundry, 2010; 59: 775

(范龙, 鲁晓宇, 代富平. 铸造, 2010; 59: 775)

[17] Lewis D J. PhD Thesis, Bethlehem: Lehigh University, 2000: 1

[18] Snugovsky L, Snugovsky P, Perovic D D. Mater Sci Technol, 2008; 24: 245

[19] Ruan Y, Wei B. Sci China, 2007; 50G: 563

[20] Li J G, Mao X M, Fu H Z, Shi Z X. Mater Sci Prog, 1991; 5: 461

(李建国, 毛协民, 傅恒志, 史正兴. 材料科学进展, 1991; 5: 461)

[21] Zhou G, Wang W H, Li Y Y. Acta Metall Sin, 2000; 36: 478

(周刚, 王文皓, 李依依. 金属学报, 2000; 36: 478)

[22] Xu H S. Aerospace Mater Technol, 1997; 6: 41

(徐禾水. 宇航材料工艺, 1997; 6: 41)

[23] Yan X Y. PhD Thesis, Madison: University of Wisconsin–Madison, 2001
Outlines

/

〈 〉