论文

SIMULATION OF MICROSTRUCTURE AND PROPERTIES EVOLUTION OF MICRO ALLOYED STEEL DURING HOT DEFORMATION BY CELLULAR AUTOMATON

  • ZHI Ying ,
  • LIU Xiang-Hua ,
  • YU Hai-Liang ,
  • YU Zhen-Fan
Expand
  • 1) State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819
    2) School of Mechanical, Materials and Mechatronic Engineering, University of Wollongong, Wollongong, NSW 2522, Australia

Received date: 2011-05-09

  Revised date: 2011-09-15

  Online published: 2011-11-11

Supported by

Supported by National Natural Science Foundation of China (Nos.51174249, 50974039 and 51034009),  National Basic Research Program of China (No.2011CB606306-2) and Specialized Research  Fund for the Doctoral Program of Higher Education (No.20090042120005)

Abstract

A model for prediction of the dynamic recrystallization microstructure and properties evolution of hot deformed austenite for micro alloyed steel by cellular automaton (CA) was developed. The theoretical modeling of dynamic recrystallization was on the basis of dislocation density, and the nucleation and grain growth of dynamic recrystallization were considered. The microstructure evolution of austenite dynamic recrystallization, such as the grain shape, grain size and volume fraction, was predicted quantitatively and visually described. Moreover the distribution and variation of the dislocation density and flow tress were obtained. Meanwhile, the microstructure and variation of the flow tress of micro alloyed< steel during hot deformation were measured by experiments. The measured results were in good agreement with the CA calculation results.

Cite this article

ZHI Ying , LIU Xiang-Hua , YU Hai-Liang , YU Zhen-Fan . SIMULATION OF MICROSTRUCTURE AND PROPERTIES EVOLUTION OF MICRO ALLOYED STEEL DURING HOT DEFORMATION BY CELLULAR AUTOMATON[J]. Acta Metall Sin, 2011 , 47(11) : 1396 -1402 . DOI: 10.3724/SP.J.1037.2011.00293

References

[1] Wang Y M, Li M Y, Wei G. Control Rolling and Control Cooling of Steel Plates. Beijing: Metallurgical Industry Press, 2007: 20

(王有铭, 李曼云, 韦光. 钢材的控制轧制和控制冷却. 北京: 冶金工业出版社, 2007: 20)

[2] Zhu L J, Wu D, Zhao X M. J Northeastern Univ, 2006; 27): 987

(朱丽娟, 吴迪, 赵宪明. 东北大学学报, 2006; 27: 987)

[3] Ghosh S, Gabane P, Bose A, Chakraborti N. Comp Mater Sci, 2009; 45: 96

[4] Yang B J, Hattiangadi A, Li W Z, Zhou G F, McGreevy T E. Mater Sci Eng, 2010; A527: 2978

[5] Zheng C W, Xiao N M, Hao L H, Li D Z, Li Y Y. Acta Mater, 2009; 57: 2956

[6] Hesselbarth H W, Gobe1 I R. Acta Metall, 1991; 39: 2135

[7] Davies C H J. Scr Mater, 1995; 33: 1139

[8] Zhen C W, Lan Y J, Xiao N M, Li D Z, Li Y Y. Acta Metall Sin, 2006; 42: 474

(郑成武, 兰勇军, 肖纳敏, 李殿中, 李依依. 金属学报, 2006; 42: 474)

[9] Liu X H. Acta Metall Sin, 2010; 46: 1025

(刘相华. 金属学报, 2010; 46: 1025)

[10] Zhan X H, Wei Y H, Dong Z B. J Mater Process Technol, 2008; 208: 1

[11] Yazdipour N, Davies C H J, Hodgson P D. Comput Mater Sci, 2008; 44: 566

[12] Chen F, Cui Z S, Liu J, Chen W, Chen S J. Mater Sci Eng, 2010; A527: 5539

[13] Bos C, Mecozzi M G, Sietsma J. Comput Mater Sci, 2010; 48: 692

[14] Li D Z, Xiao N M, Lan Y J, Zheng C W, Li Y Y. Acta Mater, 2007; 55: 6234

[15] Mao W M, Zhao X B. Recrystallization and Grain Growth of Metal. Beijing: Metallurgical Industry Press, 1994: 213

(毛卫民, 赵新兵. 金属的再结晶与晶粒长大. 北京: 冶金工业出版社, 1994: 213)

[16] Serajzadeh S, Taheri A K. Mater Des, 2002; 23: 271

[17] Cabrera J M, Omar A A, Jonas J J, Prado J M. Metall Mater Trans, 1997; 28A: 2233

[18] Serajzadeh S, Taheri A K. Mech Res Comum, 2003; 30: 87

[19] Zhu L J, Wu D, Zhao X M. J Iron Steel Res Int, 2007; 14(2): 61

[20] Zheng C W, Xiao N M, Li D Z, Li Y Y. Comput Mater Sci, 2008; 44: 507

[21] Mandal S, Sivaprasad P V, Venugopal S, Murthy K P N. Modell Simul Mater Sci Eng, 2006; 14: 1053

[22] Lu Y, Zhang L W, Deng X H, Pei J B, Wang S, Zhang G L. Acta Metall Sin, 2008; 44: 292

(卢瑜, 张立文, 邓小虎, 裴继斌, 王赛, 张国梁. 金属学报, 2008; 44: 292)

[23] Hallberg H, Wallin M, Ristinmaa M. Comput Mater Sci, 2010; 49: 25

[24] Guo H M, Liu X B, Yang X J. J Mater Eng, 2003; 8: 23

(郭洪民, 刘旭波, 杨湘杰. 材料工程, 2003; 8: 23)

[25] Li Z H. Master Dissertation. Shenyang: Northeastern University, 2004

(李治华. 东北大学硕士学位论文, 沈阳, 2004)

[26] Jin W Z, Wang L, Liu X H, Wang Z F. Mech Eng Mater, 2005; 29(10): 10

(金文忠, 王 磊, 刘相华, 王振范. 机械工程材料, 2005; 29(10): 10)
Outlines

/

〈 〉