Abstract

A mercury model was developed to investigate the control of the jet–pattern magnetic field on the flow in medium and heavy slab continuous casting mold. The velocities in mold with and without magnetic field was measured by ultrasonic Doppler velocimeter. The influences of the magnetic field on the flow discharged from the nozzle, the flow in the mold, the flow at the meniscus and washing intensity to wall were analyzed and studied. The results showed that the flow discharged from the nozzle is suppressed, and dissipated before impinging against wall, the flow in the upper eddy is strengthened, the flow in the lower eddy is weakened, and the flow at the meniscus is improved by jet–pattern magnetic field. Compared with electromagnetic braking (EMBr) ruler, the brake effect of the the jet–pattern magnetic field on the flow discharged from the nozzle and the flow at the meniscus are the better.

Cite this article

YU Yin , ZHANG Zhen-Jiang , YU Tan , GU Hui , DENG Kang , LEI Zuo-Qing , REN Zhong-Ming . EXPERIMENTAL STUDY ON FLOWIN SLAB MOLD CONTROLLED BY JET–PATTERN MAGNETIC FIELD[J]. Acta Metall Sin, 2011 , 47(10) : 1285 -1291 . DOI: 10.3724/SP.J.1037.2011.00215

References

[1] Kim D S, Kim W S, Cho K H. ISIJ Int, 2000; 40: 670

[2] Harada H, Toh T, Ishii T. ISIJ Int, 2001; 41: 1236

[3] Zeze M, Tanaka H, Takeuchi E, Mizoguchi S. 79th Conference of the Steelmaking. Pittsburgh: Iron and Steel Society, 1996: 225

[4] Mao B. Contin Cast, 1999; 6: 37

(毛斌. 连铸, 1999; 6: 37)

[5] Ha M Y, Lee H G, Seong S H. J Mater Process Technol, 2003; 133: 322

[6] Takatani K, Nakai K, Kasai N, Watanabe T, Nakajima H. ISIJ Int, 1989; 29: 1063

[7] Yu H Q, Wang B F, Li H Q, Li J C. J Mater Process Technol, 2008; 202: 179

[8] Cukierski K, Thomas B G. Metall Mater Trans, 2008; 39B: 94

[9] Zeze M, Harada H, Takeuchi E, Ishii T. 76th Steelmaking Conference Proceedings. Dallas: Iron and Steel Society, 1993: 267

[10] Yu Z, Zhang Z Q, Ren Z M, Lei Z S, Deng K. Acta Metall Sin, 2010; 46: 1275

(于湛, 张振强, 任忠鸣, 雷作胜, 邓康. 金属学报, 2010; 46: 1275)

[11] Li B K, Okane T, Umeda T. Metall Mater Trans, 2000; 31B: 1491

[12] Han G R, Xu H W. Contin Cast, 2004; 1: 4

(韩国瑞, 许宏伟. 连铸, 2004; 1: 4)

[13] Brito D, Nataf H C, Cardin P, Aubert J, Masson J P. Exp Fluids, 2001; 31: 653

[14] Yu Z, Lei Z S, Jia H H, Jin X L, Ren Z M, Deng K, Zhong Y B. Shanghai Met, 2007; 29(2): 54

(于湛, 雷作胜, 贾洪海, 金小礼, 任忠鸣, 邓康, 钟云波. 上海金属, 2007; 29: 54)
Outlines

/

〈 〉