A UNIFIED ANALYTICAL MODEL FOR THE PRIMARY SOLIDIFICATION PATH IN TERNARY ALLOYS

  • DIAO Guang-Wei ,
  • XU Ta-Ming ,
  • FU Heng-Zhi ,
  • DU Yong ,
  • HE Ti-Hui
Expand
  • 1) School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001
    2) State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083

Received date: 2011-04-02

  Revised date: 2011-06-25

  Online published: 2011-09-11

Supported by

Supported by  National Natural Science Foundation of China (Nos.50771041 and 50801019), National Basic Research Program of China
(No.2011CB610406) and Open Project of State Key Laboratory of Powder Metallurgy of Central South University (No.2008112042)

Abstract

Accurate prediction for the solidification path of a multicomponent alloy and the amounts of the secondary phases presented under a given solidification condition is critical in understanding and controlling the performances of the solidified alloy materials/parts. The degree of freedom of a single-phase solidification in multicomponent alloys is at least more than one, whilch brings some difficulty in accurate predicting of the solidification path. A new analytical model for predicting a single-phase solidification paths in ternary alloys was developed based on a previously proposed unified microsegregation model for dendrite solidification of binary alloys. The present unified analytical model can not only include the three limiting solidification conditions of equilibrium, nonequilibrium and paraequilibrium solidification, but also take into account of any solid diffusion coefficient, dendrite geometrical morphologies and solidification rates, etc. The algorithms for calculating the solidification paths of ternary alloys was closely coupled with a commercial software package/database of Thermo-Calc via its TQ6-interface in order to directly access to the thermodynamic data. The availability of the proposed analytical model for predicting the primary solidification paths of ternary alloys were demonstrated by the sample computations on Al-1.0Cu-6.3Mg, Al-1.49Si-0.64Mg and Al-1.49Si-2.90Mg alloys under different solidification conditions of solid back diffusion. It was found that the solidification conditions affect the solidification paths significantly. For an alloy, especially with a nominal composition far away from the ternary eutectic point, different solid back diffusion conditions and solidification rate can result in different amounts and even different kinds of secondary phase.

Cite this article

DIAO Guang-Wei , XU Ta-Ming , FU Heng-Zhi , DU Yong , HE Ti-Hui . A UNIFIED ANALYTICAL MODEL FOR THE PRIMARY SOLIDIFICATION PATH IN TERNARY ALLOYS[J]. Acta Metall Sin, 2011 , 47(9) : 1135 -1140 . DOI: 10.3724/SP.J.1037.2011.00195

References

[1] Lu X S. Phase Diagram and Phase Transformation. Hefei: Press of University of Science and Technology of China, 1990: 3

(陆学善. 相图与相变. 合肥: 中国科学技术大学出版社, 1990: 3)

[2] Wang C L. Phase Diagrams and Its Application. Beijing: Higher Education Press, 2008: 17

(王崇琳. 相图理论及其应用. 北京: 高等教育出版社, 2008: 17)

[3] Mehrabian R, Flemings M C. Metall Trans, 1970; 1: 455

[4] Shawn C A, Krane J M. Mater Sci Eng, 2003; A359: 91

[5] Lacaze J, Lesoult G, Relave O, Ansara I, Riquet J P. Z Metallkd, 1987; 78: 141

[6] Boettinger W J, Kattner U R, Banerjee D K. In: Thomas B G, Beckermann C eds., Modeling of Casting, Welding and Advanced Solidification Processes VIII, Warrendale: TMS, 1998: 159

[7] Chen S L, Yang Y, Chen S W, Lu X G, Chang Y A. J Phase Equilibria Diffusion, 2009; 30: 429

[8] Dupont J N. Metall Mater Trans, 2006; 37A: 1937

[9] Xie F Y, Kraft T, Zuo Y, Moon C H, Chang Y A. Acta Mater, 1999; 47: 489

[10] Ro´osz A, Exner H E. Acta Matall Mater, 1990; 38: 375

[11] Won Y M, Thomas B G. Metall Mater Trans, 2001; 32A: 1755

[12] Matsumiya T. Mater Trans, 1992, 33: 783

[13] Xu D M, Guo J J, Fu H Z. In: Howard J ed., Proceedings of the 5th Decennial International Conference on Solidification Processing. Sheffield: The University of Sheiffield, 2007: 94

[14] Xu D M. Metall Mater Trans, 2001; 32B: 1129

[15] Zhao G W, Xu D M, Song M H, Fu H Z, Du Y, He Y H. Acta Metall Sin, 2009; 45: 956

(赵光伟, 徐达鸣, 宋梦华, 傅恒志, 杜勇, 贺跃辉. 金属学报, 2009; 45: 956)
Outlines

/

〈 〉