论文

IN SITU OBSERVATION OF MnS INCLUSION BEHAVIOR IN RESULFURIZED FREE-CUTTING STEEL DURING HEATING

  • SHAO Xiao-Jing ,
  • YU Xin-Hua ,
  • YU Mo-Jun ,
  • JIANG Min ,
  • HUANG Fu-Xiang ,
  • JI Yun-Qing
Expand
  • School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083

Received date: 2011-03-31

  Revised date: 2011-06-22

  Online published: 2011-09-11

Abstract

MnS is a common type of non-metallic inclusions in steel, which is of good deformability during rolling. As elongated MnS inclusions in rolling direction often cause poor mechanical property of steel. However, MnS is indispensable in resulfurized free-cutting steel. In order to improve mechanical property, especially cutting property of free-cutting steel, the good control of shape and size of MnS is important. In this study, confocal scanning laser microscope was used firstly to observe the morphology evolution of large-sized slender MnS during heating. The effect of heating rate was also considered. The results indicated that for morphology evolution of MnS, the shrink occurred in longitudinal direction, whereas expansion and contraction happened in radial direction, which finally caused the split of slender MnS. When samples were heated at the rate between 0.5-2℃/s, the split degree of MnS decreased with the increase of heating rate. When the heating rate was in the range of 6-10℃/s, the splitting behavior of MnS could not occur.

Cite this article

SHAO Xiao-Jing , YU Xin-Hua , YU Mo-Jun , JIANG Min , HUANG Fu-Xiang , JI Yun-Qing . IN SITU OBSERVATION OF MnS INCLUSION BEHAVIOR IN RESULFURIZED FREE-CUTTING STEEL DURING HEATING[J]. Acta Metall Sin, 2011 , 47(9) : 1210 -1215 . DOI: 10.3724/SP.J.1037.2011.00183

References

[1] Chen H X, Zhou P, Chen A J, L¨u H L, Li C F. China Metall, 2001; 11: 32

(陈洪星, 周平, 陈爱洁, 吕洪亮, 李丰常. 中国冶金, 2001; 11: 32)

[2] Jiang G H. Master Dissertation, Kunming University of Science and Technology, 2006

(蒋光辉. 昆明理工大学硕士学位论文, 2006)

[3] Mao Z Q. Auto Technol Mater, 2000; 2: 1

(毛志强. 汽车工艺与材料, 2000; 2: 1)

[4] Li Y M, Zhu F X, Cui F P, Fang K. J Northeastern Univ (Nat Sci), 2007; 28: 1002

(李艳梅, 朱伏先, 崔凤平, 房 轲. 东北大学学报(自然科学版), 2007; 28: 1002)

[5] Chen M, Liu G, Zhang X H, Shen Z, Yang G J. Chin J Mechan Eng, 2007; 43: 161

(陈明, 刘钢, 张晓辉, 沈中, 杨贵军. 机械工程学报, 2007; 43: 161)

[6] Xu J, Xu D S, Li L C, Xiong L L, Wang J F. Auto Sci Technol, 2003; 1: 28

(许俊, 徐德生, 李良策, 熊龙亮, 王劲枫. 汽车科技, 2003; 1: 28)

[7] Li L S, Zhu R, Dong J. In: Li W X ed., CSM 2003 Annual Meeting Proceedings, Beijing: Metallurigical Industry Press, 2003: 335

(李联生, 朱 荣, 董杰. 见: 李文秀主编, 2003中国钢铁年会论文集, 北京: 冶金工业出版社, 2003: 335)

[8] Xia Y J,Wang F M,Wang J L, Zhao J. J Univ Sci Technol Beijing, 2010; 32B: 1271

(夏云进, 王福明, 王金龙, 赵晶. 北京科技大学学报, 2010; 32B: 1271)

[9] Chen L, Chen W Q, Xiao F H. Spec Steel, 2008; 29: 47

(陈列, 陈伟庆, 肖飞虎. 特殊钢, 2008; 29: 47)

[10] Li G Z, Wang F M, Hui R, Cao W K. Int J Miner Metall Mater, 2009; 16: 650

[11] Li L S, Zhu R, Yin H, Liu P, Zhang L P, Wei C Z, Zhou P, Dong J. Chin Rare Earths, 2005; 26(5): 48

(李联生, 朱 荣, 殷浩, 刘平, 张利平, 魏承志, 周平, 董杰. 稀土, 2005; 26(5): 48)

[12] Yun G A, Qin Z, Tian Z H, Sun Y H,Cai K K. J Univ Sci Technol Beijing, 2007; 29B: 685

(严国安, 秦哲, 田志红, 孙彦辉, 蔡开科. 北京科技大学学报, 2007; 29B: 685)

[13] Shao X J, Wang X H, Wang W J, Huang F X, Jiang M. J Univ Sci Technol Beijing, 2010; 32B: 570

(邵肖静, 王新华, 王万军, 黄福祥, 姜敏. 北京科技大学学报, 2010; 32B: 570)

[14] Nichols F A. J Mater Sci, 1976; 11: 1077

[15] Nichols F A, MullinsWW. Trans Metall Soc AIME, 1965; 233: 1840

[16] Liu W J, Jonas J J. Metall Trans, 1989; 20A: 1361
Outlines

/

〈 〉