论文

EVOLUTION OF DISLOCATION MICROSTRUCTURES IN Ta–7.5%W ALLOY FOILS DURING COLD–ROLLING

  • CHEN Chang ,
  • WANG Meng-Piao ,
  • YU Shan ,
  • GU Yan-Lin ,
  • ZUO Bei ,
  • YAN Fu-Zhong
Expand
  • School of Material Science and Engineering, Central South University, Changsha 410083

Received date: 2011-04-12

  Revised date: 2011-05-19

  Online published: 2011-08-11

Supported by

Supported by High Technology Research and Development Program of China (No.2006AA03Z517)

Abstract

The most common texture formed in rolled bcc metals is 45? rotated cubic {001}<110>, the detailed deformation structure and microhardness of these grains in cold-rolled Ta–7.5%W alloy foils were carefully investigated. It was found that when cold reduction was 10%, the typical cold deformation microstructures were found in the grains, including dislocation dipoles, a"scissors" type dislocation reaction and dislocation debris. As the reduction increased, high dense dislocation walls were formed firstly and microbands formed subsequently in one kind of grains while typical dislocation cells were formed in another kind of grains. Based on energy analysis, dislocation mesh structures would relax into dislocation cells because the elastic energy of the dislocation cells is always lower than that of the dislocation mesh. It is probable that the microbands are derived from the high dense dislocation walls rather than dislocation cells while the dislocation density in the grains must reach a critical value which is about 1014/m2 in Ta–7.5%W alloy. The microhardness test showed that the work hardening rates were different in these grains. Compared with grains with cell structures, the work hardening rate was higher in grains with microbands.

Cite this article

CHEN Chang , WANG Meng-Piao , YU Shan , GU Yan-Lin , ZUO Bei , YAN Fu-Zhong . EVOLUTION OF DISLOCATION MICROSTRUCTURES IN Ta–7.5%W ALLOY FOILS DURING COLD–ROLLING[J]. Acta Metall Sin, 2011 , 47(8) : 984 -989 . DOI: 10.3724/SP.J.1037.2011.00230

References

[1] Shen K, Duggan B J. Acta Mater, 2007; 55: 1137

[2] Chen Q Z, Quadira M Z, Duggana B J. Philos Mag, 2006;86: 3633

[3] Li Z J, Winther G, Hansen N. Acta Mater, 2006; 54: 401

[4] Park Y B, Lee D N, Gottstein G. Acta Mater, 1998; 46: 3371

[5] Jonas J J. J Mater Process Technol, 2001; 117: 293

[6] Hansen N. Mater Sci Technol, 1990; 6: 1039

[7] Hutchinson B. Mater Sci Forum, 2007; 558–559: 13

[8] Li B L, Godfrey A, Meng Q C, Liu Q, Hansen N. Acta Mater, 2004; 52: 1069

[9] Kuhlmann–Wilsdorf D. Acta Mater, 1999; 47: 1697

[10] Nasser S N, Kapoo R. Int J Plasticity, 2001; 17: 1351

[11] Nemat–Nasser S, Isaacs J B. Acta Mater, 1997; 45: 907

[12] Tse Y Y, Duggan B J. Metall Mater Trans, 2006; 37A: 1055

[13] Duesbery M S. Acta Metall, 1983, 31: 1747

[14] Duesbery M S, Vitek V. Acta Mater, 1998; 46: 1481

[15] Hansen N, Huang X, Winther G. Mater Sci Eng, 2008; A494: 61

[16] Chang J P, Cai W, Bulatov V V. Comput Mater Sci, 2002; 23: 111

[17] Hirth J P, Lothe J. Theory of Dislocations, 2nd Ed. New York: John Wiley & Sons Inc., 1960: 63

[18] Kuhlmann–Wilsdorf D. Prog Mater Sci, 2009; 54: 707

[19] Chen Q Z, Duggan B J. Metall Mater Trans, 2004; 35A: 3423

[20] Quadir M Z, Duggan B J. Acta Mater, 2006; 54: 4337

[21] Hull D, Bacon D J. Introduction to Dislocations, 4th Ed.Oxford: A division of Reed Educational and Professional Publishing Ltd., 2001: 14
Outlines

/

〈 〉