论文

PREPARATION AND MICROSTRUCTURE OF HARD BAINITE IN SURFACE LAYER OF CARBURIZED 20CrMnMoAl STEEL

  • ZHANG Peng ,
  • ZHANG Fu-Cheng ,
  • YU Tian-Sheng
Expand
  • State Key Laboratory of Metastable Materials Science & Technology, Yanshan University, Qinhuangdao 066004

Received date: 2011-02-25

  Revised date: 2011-04-24

  Online published: 2011-08-11

Supported by

Supported by National Science Foundation for Distinguished Young Scholars of China (No.50925522), National Natural Science Foundation of China (Nos.50871094 and 50821001) and Excellent Youth Foundation of Hebei Province Scientific Committee of China (No.E2009001632)

Abstract

A new technology was developed based on carburization and succedent low–temperature austempering to produce hard bainitic microstructure in the surface layer of low–carbon steel 20CrMnMoAl. The microstructure and property of the hard bainite were investigated. The samples were carburized in a gas carburizing furnace at 930 ℃ for 8 h. The carbon content in the surface layer increased to 0.81%(mass fraction) after carburization. The carbonized samples were heated at 930℃ for austenitization and then isothermally quenched at different temperatures in salt bath. The microstructures were investigated by OM, TEM and XRD, and the hardness was tested by HV–sclerometer. The results show that for the samples which were isothermally quenched at 220 and 250℃, ultrafine hard bainite was obtained in the surface layer with a hardness of 630 HV. The plate of ultrafine bainitic ferrite was as thin as 70 nm and film of retained austenite had a thickness of several nanometers. Low carbon lath martensite was obtained in the center and mixstructures of the ultrafine bainite and low carbon martensite in the transition layer.

Cite this article

ZHANG Peng , ZHANG Fu-Cheng , YU Tian-Sheng . PREPARATION AND MICROSTRUCTURE OF HARD BAINITE IN SURFACE LAYER OF CARBURIZED 20CrMnMoAl STEEL[J]. Acta Metall Sin, 2011 , 47(8) : 1038 -1045 . DOI: 10.3724/SP.J.1037.2011.00093

References

[1] Garcia M C, Caballero F G, Bhadeshia H K D H. ISIJ Int, 2003; 43: 1238

[2] Caballero F G, Bhadeshia H K D H. Curr Opin Solid State Mater Sci, 2004; 8: 251

[3] Caballero F G, Bhadeshia H K D H, Mawella K J A, Jones D G, Brown P. Mater Sci Technol, 2002; 18: 279

[4] Kim H K, Choi M I, Chung C S, Shin D H. Mater Sci Eng, 2003; A340: 243

[5] Chapetti M D, Miyata H, Tagawa T, Miyata T, Fujioka M. Int J Fatigue, 2005; 27: 235

[6] Qian Y P, He Q F, Yan G C. Locomotive Roll Stock Technol, 2001; (4): 1

(钱云鹏, 何庆复, 阎国臣. 机车车辆工艺, 2001; (4): 1)

[7] Ritchie R, Cedeno M H C, Zackay V F, Parker E R. Metall Mater Trans, 1978; 9A: 35

[8] Wang T S, Yang J, Shang C J, Li X Y, L¨u B, Zhang M, Zhang F C. Surf Coat Technol, 2008; 202: 4036

[9] Garcia M C, Caballero F G, Bhadeshia H K D H. ISIJ Int, 2003; 43: 1821

[10] Andrews K W. J Iron Steel Inst, 1965; 203: 721

[11] Bhadeshia H K D H, Honeycombe S R. Steels, 3rd Ed. Oxford: Elsevier Ltd, 2006: 129

[12] Bhadeshia H K D H. Mater Sci Technol, 2005; 21: 1293

[13] Fang H S, Wang J J, Yang Z G, Li C M, Bo X Z, Zheng Y K. Bainite Transformation. Beijing: Science Press, 1999: 149

(方鸿生, 王家军, 杨志刚, 李春明, 薄祥正, 郑燕康. 贝氏体相变, 北京: 科学出版社, 1999: 149)

[14] De A K, Murdock D C, Mataya M C, Speer J G, Matlock D K. Scr Mater, 2004; 50: 1445

[15] Bhadeshia H K D H. Bainite in Steels, 2nd Ed. London: The Institute of Materials, 2001: 373

[16] Caballero F G, Miller M K, Babu S S, Garcia M C. Acta Mater, 2007; 55: 381

[17] Bhadeshia H K D H. Materials Algorithms Project, http://www.msm.cam.ac.uk/map/steel/programs/mucg83.html

[18] Jr Caskey G R. Mater Sci Eng, 1972; 10: 357
Outlines

/

〈 〉