LASER CLADDING FeCoNiCrAl2Si HIGH–ENTROPY ALLOY COATING

  • ZHANG Hui ,
  • HE Yi-Zhu ,
  • PAN Ye
Expand
  • 1. School of Materials Science and Engineering, Jiangsu Key Lab of Advanced Metallic Materials, Southeast University, Nanjing 211189
    2. School of Materials Science and Engineering, Anhui Key Lab of Materials Science and Processing, Anhui University of Technology, Maanshan 243002

Received date: 2011-01-18

  Revised date: 2011-05-24

  Online published: 2011-08-11

Abstract

The influences of laser rapid solidification and annealing treatment at 600—1000 ℃ on the microstructure and properties of laser clad FeCoNiCrAl2Si high–entropy alloy coating were investigated. The experimental results indicate that the precipitation of intermetallic compounds in the coating could be effectively inhibited by laser cladding with rapid solidification. The coating had simple ordered bcc solid solution phases with high microhardness (900 HV0.5), good high temperature phase stability and softening resistance. The coating was mainly composed of dendrites, Fe, Cr and Si are enriched in interdendritic region, Ni, Co and Al are enriched in dendritic region. As the annealing temperature increase, the segregations of Al and Si increase, but segregations of Fe, Cr, Ni and Co changed little. Massive low angle grain boundaries were distributed at the interface between dendritic and interdendritic microstructures. After annealing at 600 ℃ for 5 hours, the microstructure was greatly refined, and the grain boundary misorientation converted from low to high angles.

Cite this article

ZHANG Hui , HE Yi-Zhu , PAN Ye . LASER CLADDING FeCoNiCrAl2Si HIGH–ENTROPY ALLOY COATING[J]. Acta Metall Sin, 2011 , 47(8) : 1075 -1079 . DOI: 10.3724/SP.J.1037.2011.00043

References

[1] Yeh J W, Chen S K, Lin S J, Gan J Y, Chin T S, Shun T T, Tsau C H, Chang S Y. Adv Eng Mater, 2004; 6: 299

[2] Zhang K B, Fu Z Y, Zhang J Y, Shi J, Wang W M, Wang H, Wang Y C, Zhang Q J. J Alloys Compd, 2010; 502: 295

[3] Chou H P, Chang Y S, Chen S K, Yeh J W. Mater Sci Eng, 2009; B163: 184

[4] Hsu C Y, Sheu T S, Yeh J W, Chen S K. Wear, 2010; 268: 653

[5] Wen L H, Kou H C, Li J S, Chang H, Xue X Y, Zhou L. Intermetallics, 2009; 17: 266

[6] Chang H W, Huang P K, Yeh J W, Davison A, Tsau C H, Yang C C. Surf Coat Technol, 2008; 202: 3360

[7] Yao C Z, Zhang P, Liu M, Li G R, Ye J Q, Liu P, Tong Y X. Electrochim Acta, 2008; 53: 8359

[8] Singh S, Wanderka N, Murty B S, Glatzel U, Banhart J. Acta Mater, 2011; 59: 182

[9] Zhang H, He Y Z, Yuan X M, Pan Y. Appl Surf Sci, 2010; 256: 5837

[10] Li M X, He Y Z, Sun G X. Appl Surf Sci, 2004; 230: 201

[11] Zhang S H, Li M X, Cho T Y, Jae H Y, Chan G L, He Y Z. Opt Laser Technol, 2008; 40: 716

[12] Yue T M, Su Y P, Yang H O. Mater Lett, 2007; 61: 209

[13] Shun T T, Hung C H, Lee C F. J Alloys Compd, 2010; 493: 105

[14] Zhang K B, Fu Z F, Zhang J Y, Shi J, Wang W M, Wang H, Wang Y C, Zhang Q C. J Alloys Compd, 2009; 485: L31

[15] Lin C M, Tsai H L, Bor H Y. Intermetallics, 2010; 18: 1244

[16] Tong C J, Chen M R, Yeh J W, Lin S J, Chen S K, Shun T T, Chang S Y. Metall Mater Trans, 2005; 36A: 1263

[17] Zhang H, Pan Y, He Y Z. Mater Des, 2011; 32: 1910

[18] Zhang K B, Fu Z Y, Zhang J Y, Wang W M, Lee S W, Niihara K. J Alloys Compd, 2010; 495: 33

[19] Zhu J M, Fu H M, Zhang H F, Wang A M, Li H, Hu Z Q. Mater Sci Eng, 2010; A527: 7210

[20] Zhu J M, Fu H M, Zhang H F, Wang A M, Li H, Hu Z Q. J Alloys Compd, 2011; 509: 3476
Outlines

/

〈 〉