STRUCTURE EVOLUTION OF AZ31 Mg ALLOY SHEET DURING BIDIRECTIONAL CYCLIC BENDING AT LOW TEMPERATURE AND SUBSEQUENT ANNEALING

  • ZHANG Lei ,
  • YANG Xu-Ti ,
  • TIAN Fang ,
  • ZHANG Yu-Jing ,
  • ZHOU Xiao-Jie ,
  • CHEN Jia
Expand
  • 1. School of Materials Science and Engineering, Central South University, Changsha 410083
    2. Key Laboratory of Nonferrous Metal Materials Science and Engineering, Ministry of Education, Central South University, Changsha 410083

Received date: 2011-01-17

  Revised date: 2011-04-13

  Online published: 2011-08-11

Supported by

Supported by National Natural Science Foundation of China (No.51071182)

Abstract

In this work, microstructure and texture evolution in the sheets of Mg alloy AZ31 was studied by means of bidirectional cyclic in–plane bending at 423 K followed by annealing at 523 K. The deformed and subsequent annealed microstructures were investigated by OM and SEM/EBSD examinations. The results showed that twinning is the dominant deformation mechanism. With the increase of deformation pass, more and more twins were produced in the grains near the surfaces of the sheets and finally these grains were serially divided up by twinning intersections. But only a few twins were formed in the grains of the middle of the sheets due to relatively lower strain. Finally, a gradient structure with high–density twins in the regions near the surfaces and, in contrast, lower density ones in the center of the sheets were induced. After 6 pass bending at 423 K followed by a subsequent annealing at 523 K, the average grain size near the surfaces was reduced to about 10 μm from the original size of 46 μm due to operation of static recrystallization at twin intersections and compression twins. Particularly, the relative intensity of the strong texture developed in the sheets was severely weakened by repeated bending, and this led to an increase of fracture elongation from 19.01% to about 24% with little change of tensile strength.

Cite this article

ZHANG Lei , YANG Xu-Ti , TIAN Fang , ZHANG Yu-Jing , ZHOU Xiao-Jie , CHEN Jia . STRUCTURE EVOLUTION OF AZ31 Mg ALLOY SHEET DURING BIDIRECTIONAL CYCLIC BENDING AT LOW TEMPERATURE AND SUBSEQUENT ANNEALING[J]. Acta Metall Sin, 2011 , 47(8) : 990 -996 . DOI: 10.3724/SP.J.1037.2011.00041

References

[1] Mordike B L, Ebert T. Mater Sci Eng, 2001; A302: 37

[2] Mackenzie L W F, Pekguleryuz M O. Scr Mater, 2008; 59: 665

[3] Jeong H T, Ha T K. J Mater Process Technol, 2007; 187–188: 559

[4] Barnett M R, Nave M D, Bettles C J. Mater Sci Eng, 2004; A386: 205

[5] Takamura H, Miyashita T, Kamegawa A, Okada M. J Alloys Compd, 2003; 356–357: 804

[6] P´erez–Prado M T, Del Valle J A, Ruano O A. Scr Mater, 2004; 50: 667

[7] Yang X Y, Zhang L, Jiang Y P, Zhu Y K. Chin J Nonferrous Met, 2011; 21: 269

(杨续跃, 张雷, 姜育培, 朱亚坤. 中国有色金属学报, 2011; 21: 269)

[8] Yang Q, Ghosh A K. Acta Mater, 2006; 54: 5147

[9] Huang G S, Song B, Xu W, Zhang L. Trans Nonferrous Met Soc China, 2010; 20: 1815

[10] Huang G S, Xu W, Huang G J, Li H C, Song B. J Mater Sci Technol, 2009; 25: 365

[11] Wang L N, Yang P, Xia W J, Chen Z H, Chen D, Li X, Meng L. Acta Metall Sin, 2009; 45: 58

(王丽娜, 杨平, 夏伟军, 陈振华, 陈鼎, 李萧, 孟利. 金属学报, 2009; 45: 58)

[12] Li X, Yang P, Meng L, Cui F E. Acta Metall Sin, 2010; 46: 147

(李萧, 杨平, 孟利, 崔凤娥. 金属学报, 2010; 46: 147)

[13] Li X, Yang P, Wang L N, Meng L, Cui F E. Mater Sci Eng, 2009; A517: 160

[14] Yang X Y, Sun Z Y, Zhang L. Acta Metall Sin, 2010, 46: 607

(杨续跃, 孙争艳, 张雷. 金属学报, 2010; 46: 607)

[15] Wang Y N, Huang J C. Acta Mater, 2007; 55: 897

[16] Liu Q. Acta Metall Sin, 2010; 46: 1458

(刘庆. 金属学报, 2010; 46: 1458)

[17] Yang X Y, Zhang L. Acta Metall Sin, 2009; 45: 1303

(杨续跃, 张雷. 金属学报, 2009; 45: 1303)

[18] Koike J, Sato Y, Ando D. Mater Trans, 2008; 49: 2792
Outlines

/