论文

MOLECULAR DYNAMICS SIMULATION OF STRUCTURAL CHANGES IN Ti FILMS COVERING OVER THE TiAl ALLOY SUBSTRATE DURING HEATING

  • LIN -zhang ,
  • LI Wei ,
  • LIU Yong-Li ,
  • XUN Ben-Zhe ,
  • YU Jia-Qiang
Expand
  • Institute of Materials Physics and Chemistry, College of Science, Northeastern University , Shenyang 110819

Received date: 2010-12-01

  Revised date: 2011-02-10

  Online published: 2011-08-11

Supported by

Supported by National Basic Research Program of China (No.2011CB606403) and the Fundamental Research Funds for the Central University (No.N90405001)

Abstract

Structural changes in Ti films covering over Ti or Al atomic layer on the TiAl substrate during heating were investigated by molecular dynamics simulations within the framework of embedded atom method (EAM). On the basis of analyses of bond–pair types, mean square displacements, atomic density functions, and atom packing in different shells, it is shown that the structural changes in the Ti film could involve several stages owing to atomic position interchanging. In addition, the Ti or Al layers play an important role in the structural changes in Ti films.

Cite this article

LIN -zhang , LI Wei , LIU Yong-Li , XUN Ben-Zhe , YU Jia-Qiang . MOLECULAR DYNAMICS SIMULATION OF STRUCTURAL CHANGES IN Ti FILMS COVERING OVER THE TiAl ALLOY SUBSTRATE DURING HEATING[J]. Acta Metall Sin, 2011 , 47(8) : 1080 -1085 . DOI: 10.3724/SP.J.1037.2010.00644

References

[1] Peng C Q, Huang B Y, He Y H. Powder Metall Technol, 2001; 19: 297

(彭超群, 黄伯云, 贺跃辉. 粉末冶金技术, 2001; 19: 297)

[2] Liu W S, Huang B Y, Zhou K C, Gu S Q. Mater Rev, 2000; 14: 19

(刘文胜, 黄伯云, 周科朝, 顾松青. 材料导报, 2000; 14: 19)

[3] Ma L, Sun Y, He X D. J Aero Mater, 2008; 28: 5

(马李, 孙跃, 赫晓东. 航空材料学报, 2008; 28: 5)

[4] Duarte L I, Ramos A S, Vieira M F, Viana, F, Vieira M T, Kocak M. Intermetallics, 2006; 14: 1151

[5] Xu Q, Chaturvedi MC, Richards N L. Metall Mater Trans, 1999; 30A: 1717

[6] Arenas M F, Acoff V L. Weld J, 2003; 82: 110S

[7] Xu S N, Zhang L, Qi Y, Zhang C B. Physica, 2010; 405B: 632

[8] Zhang L, Xu S N, Zhang C B, Qi Y. Comp Mater Sci, 2009; 47: 162

[9] Zhang L, Zhang C B, Qi Y. Physica, 2009; 404B: 205

[10] Zhang L, Zhang C B, Qi Y. Phys Lett, 2008; 372A: 2874

[11] Zhang L, Sun H X. Solid State Comm, 2009; 149: 1722

[12] Zhang L, Sun H X. Chin J Chem Phys, 2009; 22: 69

[13] Farkas D, Roqueta D, Vilette A, Ternes K. Modell Simul Mater Sci Eng, 1996; 4: 359

[14] Ruda M, Farkas D, Abriata J. Phys Rev, 1996; 54B: 9765

[15] Zhang L, Wang S Q, Ye H Q. Chin Phys, 2006; 15: 610

[16] Honeycutt J D, Andersen H C. J Phys Chem, 1987; 91: 4950

[17] Clarke A S, Jonsson H. Phys Rev, 1993; 47E: 3975
Outlines

/

〈 〉