论文

OXIDATION BEHAVIOR OF THE β-Nb PHASE PRECIPITATED IN Zr-2.5Nb ALLOY

  • LI Jiang ,
  • LIANG Xue ,
  • PENG Jian-Tiao ,
  • LIU Ren-Zhi ,
  • YU Kang ,
  • ZHOU Bang-Xin
Expand
  • Laboratory for Microstructures, Shanghai University, Shanghai 200444

Received date: 2011-04-29

  Online published: 2011-07-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50871064 and 50971084), National High Technology Research and Development Program of China (No.2008AA031701),  Natural Science Foundation of Shanghai (No.09ZR1411700) and Shanghai Leading Academic Discipline Project (No.S30107)

Abstract

The corrosion behavior for Zr--2.5Nb specimens heat--treated at 580 ℃ for 50 h after $\beta$--quenching
and cold rolling has been investigated in 500 ℃/10.3 MPa superheated steam by autoclave tests. HRTEM
equipped with EDS was employed to investigate the matrix microstructure and the oxidation behavior of the
$\beta$--Nb second phase particles (SPPs). It was found that many $\beta$--Nb SPPs with small sizes ($<$100 nm)
randomly precipitated after heat treating at 580 ℃ for 50 h. It was noted that the $\beta$--Nb SPPs were more
slowly oxidized than the zirconium matrix. The $\beta$--Nb SPPs of bcc structure were oxidized to form the mixed
structure of amorphous oxide and crystalline NbO$_{2}$ at the initial oxidation stage, and then the amorphous phase was changed to the
main structure at the middle oxidation stage, finally the niobium oxides were dissolved into the corrosion medium.

Cite this article

LI Jiang , LIANG Xue , PENG Jian-Tiao , LIU Ren-Zhi , YU Kang , ZHOU Bang-Xin . OXIDATION BEHAVIOR OF THE β-Nb PHASE PRECIPITATED IN Zr-2.5Nb ALLOY[J]. Acta Metall Sin, 2011 , 47(7) : 893 -898 . DOI: 10.3724/SP.J.1037.2011.00276

References

[1] Ells C E, Evans W. Can Min Metall Bull, 1981; 74: 105

[2] Yang W D. Reactor Materials Science. Beijing: Atomic Energy Press, 2006: 19

(杨文斗. 反应堆材料学. 北京: 原子能出版社, 2006: 19)

[3] Comstock R J, Schoenberger G, Sable G P. In: Bradley E R, Sabol G P, eds., Zirconium in the Nuclear Industry. Philadelphia: American Society for Testing and Materials, 1996: 710

[4] Ramasubramanian N, Balakrishnan P V. In: Garde A M, Bradley E R, eds., Zirconium in the Nuclear Industry: Tenth International Symposium, ASTM STP 1245, Philadelphia: American Society for Testing and Materials, 1994: 378

[5] Anada H, Takeda K. In: Bradley E R, Sabol G P, eds., Zirconium in the Nuclear Industry: Eleventh International Symposium, ASTM STP 1295, Philadelphia: American Society for Testing and Materials, 1996: 35

[6] Perkins R A, Busch R A. In: Eucken C M, Garde A M, eds., Zirconium in the Nuclear Industry: Ninth International Symposium, ASTM STP 1132, Philadelphia: American Society for Testing and Materials, 1991: 595

[7] Shebaldov P V, Peregud M M, Nikulina A V, Bibilashvili Y K, Lositski A F, Kuz’menko N V, Belov V I, Novoselov A E. In: Sabol G P, Moan G D, eds., Zirconium in the Nuclear

Industry: Twelfth International Symposium, ASTM STP 1354, West Conshohocken, PA: American Society for Testing and Materials, 2000: 545

[8] Kim H G, Jeong Y H, Kim T H. J Nucl Mater, 2004; 326: 125

[9] Jeong Y H, Lee K O, Kim H G. J Nucl Mater, 2002; 302: 9

[10] Koutsky J, Kocik J. Radiation Damage of Structural Materials. Amsterdam: Materials Science Monographys, 1994: 315

[11] Jeong Y H, Kim H G, Kim T H. J Nucl Mater, 2003; 317: 1

[12] Nikulina A V, Markelov V A, Peregud M M, Bibilashvili Y K, Kotrekhov V A, Lositsky A F, Kuzmenko N V, Shevnin Y P, Shamardin V K, Kobylyansky G P, Novoselov A E. In: Bradley E R, Sabol G P, eds., Zirconium in the Nuclear Industry: Eleventh International Symposium, ASTM STP 1295, Philadelphia: American Society for Testing and Materials, 1996: 785

[13] Kim H G, Choi B K, Park J Y, Cho H D, Jeong Y H. J Alloys Compd, 2009; 481: 867

[14] Liu W Q, Zhou B X, Li Q. Nucl Power Eng, 2002; 23: 69

(刘文庆, 周邦新, 李强. 核动力工程, 2002; 23: 69)

[15] Li Q. PhD Thesis, Shanghai University, 2008

(李强. 上海大学博士论文, 2008)

[16] Li Q, Liu W Q, Zhou B X. Rare Met Mater Eng, 2002; 31: 389

(李强, 刘文庆, 周邦新. 稀有金属材料与工程, 2002; 31: 389)
Outlines

/