Abstract

Zr-2.5Nb-xCu (x=0.2, 0.5, mass fraction, %) specimens were annealed at 580 ℃ for 50 h and 620 ℃ for 2 h after β-quenching and cold rolling, and then corroded in autoclave with 500 ℃/10.3 MPa superheated steam. SEM and TEM equipped with EDS were employed to investigate their corrosion behaviors through analyzing the microstructures of the fracture surface of the oxide layers or of the cross-section of oxide layers. It was found that the addition of copper can improve the corrosion resistance of Zr-2.5Nb alloy, which is closely related to the increases in the fraction and size of columnar grains in the oxide film.

Cite this article

LI Jiang , LIANG Xue , PENG Jian-Tiao , YU Kang , YAO Mei-Yi , ZHOU Bang-Xin . EFFECT OF Cu-ADDITION ON THE CORROSION BEHAVIOR OF Zr-2.5Nb ALLOYS IN 500 ℃/10.3 MPa SUPERHEATED STEAM[J]. Acta Metall Sin, 2011 , 47(7) : 877 -881 . DOI: 10.3724/SP.J.1037.2011.00275

References

[1] Garzarolli F, Seidel H, Tricot R, Gros J P. In: Eucken C M, Garde A M, eds., Zirconium in the Nuclear Industry: Ninth International Symposium, ASTM STP 1132, Philadelphia: American Society for Testing and Materials, 1991: 395

[2] Takeda K, Anada H. In: Sabol G P, Moan G D, eds., Zirconium in the Nuclear Industry: Twelfth International Symposium, ASTM STP 1354, West Conshohocken, PA: American Society for Testing and Materials, 2000: 592

[3] Bouvier P, Godlewski J, Lucazeau G. J Nucl Mater, 2002; 300: 118

[4] Jeong Y H, Kim H G, Kim T H. J Nucl Mater, 2003; 317: 1

[5] Sabol G P. J ASTM Int, 2005; 2: 3

[6] Bossis P, Pˆecheur D, Hanifi K, Thomazet J, Blat M. J ASTM Int, 2006; 3: 494

[7] Kim H G, Jeong Y H, Kim T H. J Nucl Mater, 2004; 326: 125

[8] Jeong Y H, Lee K O, Kim H G. J Nucl Mater, 2002; 302: 9

[9] Park J Y, Choi B K, Jeong Y H, Jung Y H. J Nucl Mater, 2005; 340: 237

[10] Park J Y, Choi B K, Jeong Y H, Kim K T, Jung Y H. Proc of 2005 Water Reactor Fuel Performance Meeting, Kyoto, Japan, 2005: 188

[11] Li Q. PhD Thesis, Shanghai University, 2008

(李强. 上海大学博士论文, 2008)

[12] Zhou B X, Li Q, Yao M Y, Liu WQ, Chu Y L. Nucl Power Eng, 2005; 26: 364

(周邦新, 李强, 姚美意, 刘文庆, 褚玉良. 核动力工程, 2005; 26: 364)

[13] Zhou B X, Li Q, Liu W Q , Yao M Y, Chu Y L. Rare Met Mater Eng, 2006; 35: 1009

(周邦新, 李 强, 刘文庆, 姚美意, 褚玉良. 稀有金属材料与工程, 2006; 35: 1009)

[14] Yao M Y. PhD Thesis, Shanghai University, 2007

(姚美意. 上海大学博士论文, 2007)
Outlines

/

〈 〉