The WC-Ni cemented carbide, as a promising seal component material in nuclear power plant, was treated by high-intensity pulsed ion beam (HIPIB) with ion energy of 300 keV, ion current density of 300 A/cm2, i.e., at a power density of 108 W/cm2 and at a pulse duration of 70 ns up to 10 shots. The phase composition, surface morphology and element distribution in the surface of WC-Ni cemented carbide before and after HIPIB irradiation were investigated by using XRD, SEM and EPMA, and its properties were characterized by microhardness measurement and block-on-ring wear testing. It is found that the phase transformation from hexagonal WC to cubic β-WC1-x underwent in the irradiated surface layer, and the amount of β-WC1-x phase increased with increasing shot number. The surface remelting and selective ablation of the nickel binder phase resulted in the formation of hilly topography with numerous protrusions on the irradiated surfaces, and the dimension of protrusions expanded under repetitive irradiation. As increasing the irradiation up to 10 shots, a network of hill-valleys was finally produced on the irradiated surfaces but the surface is smoothed and densified in a micro scale. A hardened depth of 160 μm was obtained, which is attributable to the strong stress wave induced during the irradiation. As a result, the wear resistance of WC-Ni cemented carbides is considerably improved by a factor of 3 along with a 38% reduction in the friction coefficient after 10-shot irradiation.
LEI Meng-Kai
. SURFACE MODIFICATION OF WC-Ni CEMENTED CARBIDE FOR SEALS BY HIGH-INTENSITY PULSED ION BEAM IRRADIATION[J]. Acta Metall Sin, 2011
, 47(7)
: 958
-964
.
DOI: 10.3724/SP.J.1037.2011.00228
[1] Cappelli E, Orlando S, Pinzari F, Napoli A, Kaciulis S. Appl Surf Sci, 1999; 138–139: 376
[2] Karatas C, Yilbas B S, Aleem A, Ahsan M, Kaciulis S. J Mater Process Technol, 2007; 183: 234
[3] Li T J, Lou Q H, Dong J X, Wei Y R, Liu J R. Appl Surf Sci, 2001; 172: 51
[4] Gnyusov S, Tarasov S, Ivanov Yu, Rothstein V. Wear, 2004; 257: 97
[5] Kano S, Inoue T. Surf Coat Technol, 2004; 257: 97
[6] Gnyusov S, Tarasov S, Ivanov Yu, Rothstein V. Wear, 2004; 257: 97
[7] Davis H A, Remnev G E, Stinnett R W, Yatsui K. MRS Bull, 1996; 21: 58
[8] Yilbas B S, Shuja S Z, Arif A, Gondal M A. J Mater Process Technol, 2003; 135: 6
[9] Lei M K, Zhu X P, Liu C, Xin J P, Han X G, Li P, Dong Z H, Wang X, Miao S M. J Manuf Sci Eng, 2009; 131: 031013
[10] Zhu X P, Lei M K, Dong Z H, Ma T C. Rev Sci Instrum, 2003; 74 : 47
[11] Zhang H T, Wang T M, Wang C, Wang W J, Han B X, Yan S, Zhao W J, Han Y F. Rare Met Mater Eng, 2003; 32: 216
(张洪涛, 王天民, 王聪, 王文军, 韩宝玺, 颜莎, 赵渭江, 韩雅芳. 稀有金属材料工程, 2003; 32: 216)
[12] Wang X, Zhang J S, Lei M K. Acta Metall Sin, 2007; 43: 393
(王旭, 张俊善, 雷明凯. 金属学报, 2007; 43: 393)
[13] Uglov V V, Anishchik V M, Astashynski V M, Cherenda N N, Gimro I G, Kovyazo A V. Surf Coat Technol, 2005; 200: 245
[14] Gromilov S A, Kinelovskii S A, Kireenko I B. Combust, Explos Shock Waves, 2003; 39: 601
[15] Zhu X P, Lei M K, Dong Z H, Miao S M, Ma T C. Surf Coat Technol, 2003; 173: 105
[16] Jia K, Fischer T E. Wear, 1996; 200: 206
[17] Satio H, Iwabuchi A, Shimizu T. Wear, 2004; 261: 126