INFLUENCES OF TiN INCLUSION ON CORROSION AND STRESS CORROSION BEHAVIORS OF ALLOY 690 TUBE IN HIGH TEMPERATURE AND HIGH PRESSURE WATER

  • YU Jian-Qiu ,
  • ZHI Xiao-Hui
Expand
  • State Key laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2011-04-06

  Revised date: 2011-04-15

  Online published: 2011-07-11

Supported by

Supported by National Basic Research Program of China (No.2011CB610502) and National Science and Technology Major Project (No.2011ZX06004-009})

Abstract

TEM and SEM were used for studying the existing forms and distribution states of TiN inclusions in alloy 690. The corrosion and stress corrosion behaviors of alloy 690 were investigated through high temperature high pressure electrochemical measurement and immersion tests. TiN particles are the main inclusion in alloy 690 and randomly distribute in austenitic matrix. Corrosion experiments showed that pitting corrosion occurs preferentially at the inclusions containing Ti with high potential in simulated primary water of pressurized water reactor (PWR). In high temperature high pressure alkali solution containing lead, the region near TiN inclusion and close to the side of matrix is the preferred position for corrosion, and TiN inclusions at grain boundary can subsequently cause local stress concentration on grain boundary, both of which lead to intergranular stress corrosion cracking in alloy 690.

Cite this article

YU Jian-Qiu , ZHI Xiao-Hui . INFLUENCES OF TiN INCLUSION ON CORROSION AND STRESS CORROSION BEHAVIORS OF ALLOY 690 TUBE IN HIGH TEMPERATURE AND HIGH PRESSURE WATER[J]. Acta Metall Sin, 2011 , 47(7) : 847 -852 . DOI: 10.3724/SP.J.1037.2011.00205

References

[1] Crum J R. Corrosion, 1986; 42: 368

[2] Dutta R S, Tewari R, De P K. Corros Sci, 2007; 49: 303

[3] Dutta R S, Tewari R. Br Corros J, 1999; 34: 201

[4] Cheung C, Erb U, Palumbo G. Mater Sci Eng, 1994; A185: 39

[5] Ahn S, Rao V S, Kwon H, Kim U. Corros Sci, 2006; 48: 1137

[6] Fairchild D P, Howden D G, Clark W A T. Metall Mater Trans, 2000; 31A: 641

[7] Yan W, Shan Y Y, Yang K. Metall Mater Trans, 2006; 37A: 2147

[8] Lim Y S, Kim J S, Kwon H S. J Nucl Mater, 2005; 336: 65

[9] Meng F, Wang J, Han E H, Ke W. Corros Sci, 2009; 52: 927

[10] Macdonald D D, Scot A C, Wentrcek P. J Electrochem Soc, 1979; 126: 908

[11] Dutta R S, Lobo A, Purandare R, Kulkarni S K, Dey G K. Metall Mater Trans, 2002; 33A: 1437

[12] Kuo T Y, Lee H T. Mater Sci Eng, 2002; A338: 202

[13] Dutta R S, Purandare R, Lobo A, Kulkarni S K, Dey G K. Corros Sci, 2004; 46: 2937

[14] Was G S, Kruger R M. Acta Metall, 1985; 33: 841

[15] Kai J, Yu G, Tsai C, Liu M, Yao S. Metall Mater Trans, 1989; 20A: 2057

[16] In C B, Kim Y I, KimW W, Kim J S, Chun S S, LeeW J. J Nucl Mater, 1995; 224: 71

[17] Feron D, Lambert I. In: Proc 12th Int Conf Properties of Water and Steam, IAPWS, Orlando, FL, USA, 1994: 783

[18] Yamanaka K. In: Proc 5th Int Symp Enviromental Degradation of Materials in Nuclear Power Systems–Water Reactors, California: American Nuclear Society, TMS, NACE, 1991: 773

[19] Was G, Tischner H, Latanision R. Metall Mater Trans, 1981; 12A: 1397

[20] Yu G P, Yao H C. Corrosion, 1990; 46: 391
Outlines

/

〈 〉