论文

INVESTIGATION ON HEAT TREATMENT OF A DUPLEX STAINLESS STEEL FOR NUCLEAR POWER PLANT IMPELLER

  • LU Shan-Beng
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2011-03-23

  Revised date: 2011-04-12

  Online published: 2011-07-11

Supported by

Supported by Investigation on Fundamental Issues of Stainless Steels from SYNL, IMR, CAS

Abstract

Effects of heat treatment on microstructure and mechanical property of a cast duplex stainless steel used as making impeller of seawater circular pump in nuclear power plant were investigated. The results demonstrate that the impact energy and elongation
decrease sharply when heat-treated time was longer than 5 min at 800-850 ℃ or when the cooling rate was less than 7.5 ℃/min. The σ phases have been identified through SEM and XRD. The weakness of the mechanical properties is attributed to the precipitation of σ phase. With increasing aging time, the σ phase coarsened and the nucleation position moved from the γ/δ interfaces into the whole ferrite phase.

Cite this article

LU Shan-Beng . INVESTIGATION ON HEAT TREATMENT OF A DUPLEX STAINLESS STEEL FOR NUCLEAR POWER PLANT IMPELLER[J]. Acta Metall Sin, 2011 , 47(7) : 921 -926 . DOI: 10.3724/SP.J.1037.2011.00165

References

[1] Wu J. Duplex Stainless Steel. Beijing: Metallurgy Industry Press, 1999: 1

(吴玖. 双相不锈钢. 北京: 冶金工业出版社, 1999: 1)

[2] Guha P, Clark C A. In: Lula R A, ed., Duplex Stainless Steels Conference Proceedings, Ohio: American Society for Metals, 1983: 355

[3] Atkinson R F, King RW, In: Lula R A, ed., Duplex Stainless Steels Conference Proceedings, Ohio: American Society for Metals, 1983: 399

[4] Xiang H L, He F S, Liu D. Acta Metall Sin, 2009; 45: 1456

(向红亮, 何福善, 刘 东. 金属学报, 2009; 45: 1456)

[5] Wang X F, Chen W Q, Zheng H G. Iron Steel, 2009; 44: 64

(王晓峰, 陈伟庆, 郑宏光. 钢铁, 2009; 44: 64)

[6] Srivastava S K. In: Lula R A, ed., Duplex Stainless Steels Conference Proceedings, Ohio: American Society for Metals, 1983: 1

[7] Robert N Gunn. Duplex Stainless Steels: Microstructure, Properties and Applications. Cambridge England: Abington Publishing, 1997: 24

[8] Truman J E, Pirt K R. In: Lula R A, ed., Duplex Stainless Steels Conference Proceedings, Ohio: American Society for Metals, 1983: 113

[9] Johnson E, Kim Y J, Chumbley L S, Gleeson B. Scr Mater, 2004; 50: 1351

[10] Lo K H, Shek C H, Lai J K L. Mater Sci Eng, 2009; R65: 39

[11] Shek C H, Shen G J, Lai J K L, Duggan B J. Mater Sci Technol, 1994; 10: 306

[12] Nilsson J O, Wilson A. Mater Sci Technol, 1993; 9: 545

[13] Martins M, Casteletti L C. Mater Charact, 2009; 60: 792

[14] И Я CokoΠ, translated by Li P Z, Wang X Z. Duplex Stainless Steels. Beijing: Atomic Energy Press, 1979: 23

([苏]И Я CokoΠ著; 李丕钟, 王欣增译. 双相不锈钢. 北京: 原子能出版社, 1979: 23)

[15] Nisson J O. Mater Sci Technol, 1992; 8: 685

[16] Chance J, Coop W, Gradwell K J. In: Lula R A, ed., Duplex Stainless Steels Conference Proceedings, Ohio: American Society for Metals, 1983: 317

[17] Kuo K H. JISI, 1995; 181: 213

[18] Kuo K H. JISI, 1995; 181: 128

[19] Lee Y D, Kim K T, Kim B U, Lee Y H. Eur Pat, EP0777756, 1996
Outlines

/

〈 〉