EFFECTS OF NITROGEN CONTENT ON MICROSTRUCTURE AND MECHANICAL PROPERTY OF ALLOY 690

  • LIU Kui
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2011-03-23

  Revised date: 2011-04-18

  Online published: 2011-07-11

Supported by

Supported by National Natural Science Foundation of China (No.50901076)

Abstract

The microstructure and mechanical property at room temperature of Ni-30Cr-10Fe-xN (x=0.001, 0.011, 0.018, 0.030, mass fraction, %) base alloy 690 were investigated. The OM observation shows that the amounts of precipitated nitrides and the annealing twins in the matrix increase with more nitrogen added in the alloy. The carbide precipitation along boundary and the chromium depletion near the grain boundary are modified by nitrogen addition, carbide becomes less and chromium depletion is mitigated. The tensile test result shows that both of the yield and tensile strengths are increased by about 50 MPa when nitrogen content increased from 0.001% to 0.030%, while the ductility lowers a little. The fractographs exhibit typical ductile dimple pattern and the sizes of the dimples reduce with increasing nitrogen content in the alloy.

Cite this article

LIU Kui . EFFECTS OF NITROGEN CONTENT ON MICROSTRUCTURE AND MECHANICAL PROPERTY OF ALLOY 690[J]. Acta Metall Sin, 2011 , 47(7) : 816 -822 . DOI: 10.3724/SP.J.1037.2011.00158

References

[1] Kai J J, Liu M N. Scr Metall, 1989; 23: 17

[2] Sarver J M, Crum J R, MankinsWL. Corros NACE, 1988; 44: 288

[3] Fuchs G E, Haydon S Z. Scr Metall Mater, 1991; 25: 1483

[4] Kai J J, Tsai C H, Huang T A, Liu M N. Metall Trans, 1989; 20A: 1077

[5] Dutta R S, Tewari R, De P K. Corros Sci, 2007; 49: 303

[6] Zhu H, Dong J X, Zhang M C, Hu Y H, Xie X S. J Univ Sci Technol Beijing, 2002; 24: 511

(朱红, 董建新, 张麦仓, 胡尧和, 谢锡善. 北京科技大学学报, 2002; 24: 511)

[7] Lu Y, Qin X B. Boiler Manufactur, 1994; 154: 54

(鲁 悦, 秦绪斌. 锅炉制造, 1994; 154: 54)

[8] Mudali U K, Baldev R, Translated by Li J, Huang Y H. High Nitrogen Steels and Stainless Steels-Manufacturing, Properties and Applications. Beijing: Chemical Industry Press, 2006: 48

(Mudali U K, Baldev R著; 李晶, 黄运华  译. 高氮钢和不锈钢---生产, 性能与应用. 北京: 化学工业出版社, 2006: 48)

[9] Simmons J W. Mater Sci Eng, 1996; A207: 159

[10] Reed R P. JOM, 1989; 3: 16

[11] Rhodes G O, Conway J J. JOM, 1996; 4: 28

[12] Levey P R, van Bennekom A. Corrosion, 1995; 51: 911

[13] Thuvander M, Stiller K, Olsson E. Mater Sci Technol, 1999; 15: 237

[14] Liu K, Hao X C, Gao M, Li S, Li Y Y, Wan B F. Proc 17th Int Conf Nuclear Engineering, Three Park Avenue, New York, 2010 (CD–ROM)

[15] Dutta R S, Lobo A, Purandare R, Kulkarni S K, Dey G K. Metall Mater Trans, 2002; 33A: 1437

[16] Meng F J, Wang J Q, Han E H, Ke W. Corros Sci, 2010; 52: 927

[17] Abdulranhan R F, Hendry A. Metall Mater Trans, 2001; 32B: 1103

[18] Mitchell A. Acta Metall Sin (Engl Lett), 2005; 18: 575

[19] Simmons J W, Covino B S, Hawk J A. ISIJ Int, 1996; 36: 846

[20] Degallaix S, Foct J, Hendry A. Mater Sci Technol, 1986; 2: 946

[21] Pande C S, Rath B B, Imam M A. Mater Sci Eng, 2004; A367: 171

[22] Pande C S, Imam M A. Mater Sci Eng, 2009; A512: 82
Outlines

/

〈 〉