论文

STOCHASTIC PROCESS-BASED MODELING METHOD FOR PITTING CORRSION OF Ni-BASED ALLOY 690

  • ZHOU Bing-Hai ,
  • DI Zi-Jing
Expand
  • 1) School of Mechanical Engineering, Tongji University, Shanghai 201804
    2) School of Mechanical Engineering, Shanghai Jiaotong University, Shanghai 200240

Received date: 2011-01-17

  Revised date: 2011-03-12

  Online published: 2011-09-11

Supported by

Supported by National Natural Science Foundation of China (No.71071115) and High Technology Research and Development Program of China (Nos.2009AA043403 and 2009AA043000)

Abstract

Pitting corrosion is one of the most serious modes of localized corrosions that can cause deteriorations of Ni-based alloy 690 steam generator tubes. Because the initiation and propagation of pitting are subject to interactions of different factors, it is a stochastic process. It is almost impossible to draw any deterministic models for formations of the processes. To efficiently model the formation process of pitting, firstly, experimental schemes of pitting formations were designed. Based on stochastic theory, combined experimental data and analyzing results, a modeling method was presented with stochastic processes. Namely, non-homogeneous Poisson process (NHPP) was used to model the pitting initiation process and non-stationary Gamma model was used to set up pitting propagation model. A systemic method was built for pitting corrosion failure of the Ni-based alloy 690 tubes, including experimental method, modeling method and simulation method. Finally, the stochastic degradation failure of the Ni-based alloy 690 tubes was simulated. The probability distribution of the lifespan of the Ni-based alloy 690 tubes was obtained under different working environments. The results showed that the proposed modeling method is valid to analyze the initiation and propagation of pitting of the tubes according to different combinations of modeling parameters. It is important for the lifespan prediction and development of relevant maintenance plans of the tubes.

Cite this article

ZHOU Bing-Hai , DI Zi-Jing . STOCHASTIC PROCESS-BASED MODELING METHOD FOR PITTING CORRSION OF Ni-BASED ALLOY 690[J]. Acta Metall Sin, 2011 , 47(9) : 1159 -1166 . DOI: 10.3724/SP.J.1037.2011.00039

References

[1] Park I G. Corros Sci Technol, 2002; 31: 6

[2] Joseph R. Electrocorrosion and Protection of Metals. Amsterdam: Elsevier, 2008: 13

[3] Datla S V, Jyrkama M I. Nucl Eng Des, 2007; 238: 1771

[4] Zapp P E. Corrosion, 1996; 96: 24

[5] Frankel G S. J Electrochem Soc, 1998; 145: 2186

[6] Turnbull A L, McCartney N. Corros Sci, 1996; 48: 2084

[7] Shibata T. Corrosion, 1996; 52: 813

[8] Hong H P. Corrosion, 1999; 55: 10

[9] Aziz P M. Corrosion, 1956; 12: 495

[10] Provan J W, Rodriguez E S. Corrosion, 1989; 45: 178

[11] Valor A, Caleyo F. Corros Sci, 2007; 49: 559

[12] Zhang B H, Cong W B, Yang P. Metal Electrochemical Corrosion and Protection. Beijing: Chemical Industry Press, 2005: 75

(张宝宏, 丛文博, 杨萍. 金属电化学腐蚀与防护. 北京: 化学工业出版社, 2005: 75)

[13] Datla S V, Jyrkama M I, Panday M D. Nucl Eng Des, 2008; 238: 1771

[14] Li P. Chin J Appl Probab Statis, 2004; 20: 179

(李平. 应用概率统计, 2004; 20: 179)

[15] Blain C, Barros A. Risk Reliab Soc Safety, 2007; 3: 2395

[16] Castanier B, Yeung T. In: Revie M, Bedford T J, Walls L A eds., Proc 2008 Annual Reliability and Maintainability Symposium, Washington, IEEE Computer Society, 2008: 25

[17] Yuan X X, Mao D, Pandey M D. Nucl Eng Des, 2008; 38: 16

[18] Xiao G, Li T T. System Reliability Analysis of Monte Carlo Method. Beijing: Science Press, 2003: 38

(肖刚, 李天柁, 系统可靠性分析中的蒙特卡罗方法. 北京: 科学出版社, 2003: 38)

[19] Avramidis A N, L’Ecuyer P, Tremblay P A. In: Chick S, Sa’nzhes P J, Ferrin D, Morrice D J eds., Proc 2003 Winter Simulation Conference, Piscataway: IEEE, 2003: 319
Outlines

/

〈 〉