Abstract

Ultra–purified ferrite stainless steels (UP–FSS) are widely used in the fields of automobile, household appliances etc. Much better performance than conventional ferrite stainless steels is obtained by minimizing the interstitial elements level in UP–FSS. However, some negative effects, such as degradation of the formability and ridging–resistance, are also brought by purifying the steels, which lead to abnormally growth of the columnar grains. Moreover, the grains in heat affected zone (HAZ) are apt to coarsen during welding process. One of the effective ways to resolve such problems is to increase the equiaxial grain ratio in as–cast microstructure and refine the grain size. Micro–alloying of steels with strong carbide and nitride former, such as Ti and Nb, is a way to do that. In this work, the effects of Ti and Nb micro–alloying on the as–cast, as–rolled, and HAZ microstructures of the ultrapurified 11%Cr ferrite stainless steels with different interstitial element levels were investigated by both experimental research and thermodynamic calculation. The results indicated that the effect of Ti and Nb micro–alloying was better when the content of C and N in the steel was 0.0163%, which showed the minimum grain size in as–cast, as–rolled, and HAZ microstructures, and the equiaxial grain ratio in as–cast microstructure was evidently improved as well. It was found by calculation that, with increasing of C and N content and addition of Ti and Nb to the steels, the solid–liquid two–phase region was broadened. This was beneficial to increase the undercooling in front of the liquid–solid interface and the probability of heterogeneous nucleation, and consequently, increase the equiaxial grain ratio and decrease te mean grain size in as–cast microstructure. On the other hand, with addition of Ti and increase of N conent, TiN type particles might precipitate in olid–liquid two–phase regio, which was helpful for promoting the heterogeneous nucleation of δ ferrite.

Cite this article

LIU Jing , LUO Xin-Hong , HU Xiao-Jiang , LIU Shi . EFFECT OF Ti AND Nb MICRO–ALLOYING ON THE MICROSTRUCTURE OF THE ULTRA–PURIFIED 11%Cr FERRITE STAINLESS STEELS[J]. Acta Metall Sin, 2011 , 47(6) : 688 -696 . DOI: 10.3724/SP.J.1037.2011.00059

References

[1] Meng F M, Fu J Y. Modern Niobium Containing Stainless Steels. Beijing: Metallurgical Industry Press, 2004: 99

(孟繁茂, 付俊岩. 现代含铌不锈钢. 北京:冶金工业出版社, 2004: 99)

[2] Yazawa Y, Kato Y, Kobayashi M. Kawasaki Steel Tech Rep, 1999; 40: 23

[3] Hamada J, Matsumoto, Fudanoki F, Maeda S. ISIJ Int, 2003; 3: 12

[4] Park S H, Kim K Y, Lee Y D, Park C G. ISIJ Int, 2002; 42: 100

[5] Tsuj N, Tsuzaki K, Make T. ISIJ Int, 1994; 34: 1008

[6] Shan Y T. Master Dissertation, Chinese Academy of Sciences, Shenyang, 2010

(单亚廷. 中国科学院硕士学位论文, 沈阳, 2010)

[7] Qi J J, Huang Y H, Zhang Y. Microalloyed Steels. Beijing: Metallurgical Industry Press, 2006: 2

(齐俊杰, 黄运华, 张 跃. 微合金化钢. 北京: 冶金工业出版社, 2006: 2)

[8] Shi X F, Cheng G G, Shi C X, Zhao P. In: The Chinese Society for Metals ed., CSM 2007 Annual Meeting Proceedings, Beijing: Metallurgical Industry Press, 2007: 15

(施晓芳, 成国光, 史彩霞, 赵沛. 见: 中国金属学会主编, 2007中国钢铁年会论文集, 北京: 冶金工业出版社, 2007: 15)

[9] DeArdo A J. In: Zhang H T,Wang R Z, Pang G Y eds., Nb Containing Steels and Nb Alloys—China & Brazil Symposium Proceedings, Beijing: Metallurgical Industry Press, 2000: 109

(DeArdo A J. 见: 章洪涛, 王瑞珍, 庞干云主编, 铌钢和铌合金-中国&巴西学术研讨会, 北京: 冶金工业出版社, 2000: 109)

[10] Sato K, Ishiguro Y. In: The Iron and Steel Institute of Japan ed., International Forum for Physical Metallurgy of IF Steels, Tokyo: ISIJ, 1994; 45

[11] Hua M, Garcia C I, DeArdo A J. Scr Mater, 1993; 28: 973

[12] Tither G, Garcia C I, Hua M, DeArdo A J. In: The Iron and Steel Institute of Japan ed., International Forum for Physical Metallurgy of IF Steels, Tokyo: ISIJ, 1994; 293

[13] Fujita N, Ohmura K, Kikuchi M. Scr Mater,1996; 35: 705

[14] Xu H, Xu L D, Zhang S J, Han Q. Scr Mater, 2006; 54: 2191

[15] Yong Q L. Secondary Phases in Steels. Beijing: Metallurgical Industry Press, 2006: 93

(雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 93)

[16] Wang J X, Huang J R, Lin J S. Fundamentals and Control of Metal Solidification. Beijing: China Machine Press, 1983: 180

(王家昕, 黄积荣, 林建生. 金属的凝固及其控制. 北京: 机械工业出版社, 1983: 180)

[17] Hunt J D. Mater Sci Eng, 1984; 65: 75

[18] Lippold J C, Kotecki D J, translated by Chen J H.Welding Metallurgy and Weldability of Stainless Steels. Beijing: China Machine Press, 2008: 81

(Lippold J C, Kotecki D J著, 陈剑虹译. 不锈钢焊接冶金学及焊接性. 北京: 机械工业出版社, 2008: 81)
Outlines

/

〈 〉