A creative and simple horizontal electrorefining method had been developed for high pure aluminum production in fluoride molten salt. Impure primary aluminum was purified due to the different electronegativity between Al and impurities during electrorefining. Pre–electrolysis was effective in the purification of electrolyte, concentration of impurities such as Cu, Si and P were reduced to 3.2×10−6, 14×10−6 and 1.5×10−6, respectively. Aluminum electrorefining could run steady with current density as high as 800 mA/cm2, hich indicated that the uneven current density istribution had no bad effect on the electrochemical process. The anode nd cathode were both covered by Na3AlF6–LiF electrolyte, hich argely reduced the oxidation of aluminum at hih temperature and yieded a igh curent efficiency of 98.6%. The analysis of the anode feed and refined aluminum showed a remarkabe reduction of the mass fraction of Cu, from 14.5×10−6 to 0.9×10−6. Besides, particular mention should be made of efficient removaof impuritis likF, Si and Zn, the purity of electrorefined aluminum was above 99.99%.
GU Meng
,
TIAN Zhong-Liang
,
LAI Yan-Qing
,
LIU Fang-Xiang
,
LI Jie
,
LIU Ye-Xiang
. HORIZONTAL ELECTROREFINING OF Al IN Na3AlF6–LiF MOLTEN SALT[J]. Acta Metall Sin, 2011
, 47(6)
: 727
-734
.
DOI: 10.3724/SP.J.1037.2011.00028
[1] Liu Y X, Li JModern Aluminum Electrolysis. Beijing:Metallurgicl Indusry Press, 2008: 520
(刘业翔, 李劼.现代铝电解. 北京: 冶金工业出版社, 2008: 520)
[2] James W E. JOM, 2007; 59: 30
[3] De Nora V. Aluminium, 2000; 76: 998
[4] Qiu Z X. Smelting Aluminum in Pre–baked Cell. 3nd Ed., Beijing: Metallurgical Industry Press, 2005: 413
(邱竹贤. 预焙槽炼铝. 第三版. 北京: 冶金工业出版社, 2005: 413)
[5] Solheim A, Rolseth S. Metall Mater Trans, 1996; 10B: 739
[6] Craig W B. In: Peterson R D ed., Light Metals Proceedings. Nashville: Miner Metals & Mater Soc, 2000: 391
[7] Mariola S, Katowice J B. Aluminum, 2005; 3: 81
[8] Johansen K, Sadoway D R, Myhre B, Engvoll M, Engvoll K. US Pat, 20070215483, 2007
[9] Slater S A, Raraz A G, Willit J L. Sep Purif Technol, 1999; 15: 197
[10] Kononov A, Kuznetsov S, Polyakov E. J Alloys Compd, 1995; 218: 173
[11] Ueda M, Ohmura T, Konda S, Sasaki T, Ohtsuka T, Ishikawa T. J Appl Electrochem, 2001; 31: 871
[12] Schwarz V, Wendt H. J Appl Electrochem, 1995; 25: 34
[13] Kanda M, Sato K, Kimura E. In: Lin R Y, Chang Y A, Reddy R G, Liu C T eds., Light Metals Proceedings. Anaheim: Miner Metals & Mater Soc, 1996: 1087
[14] Olson J M, Carleton K L. J Electrochem Soc, 1981; 128: 2698
[15] Jia M, Tian Z L, Lai Y Q, Li J, Yi J G, Yan J F, Liu Y X. Acta Phys Sin, 2010, 59: 1938
(贾 明, 田忠良, 赖延清, 李劼,伊继光, 闫剑锋, 刘业翔. 物理学报. 2010; 59: 1938)
[16] Zhang Z X, Wang E K. Electrochemistry Principle and Method. Beijing: Science Press, 2000: 55
(张祖训, 汪尔康. 电化学原理和方法. 北京: 科学出版社, 2000: 55)
[17] Wicks C E, Block F E. Thermodynamic Properties of 65 Elements–Their Oxides, Halides, Carbides, and Nitrides. Washington: United States Government Printing, 1963: 1
[18] Liu D R, Yang Z H, LiWX, Qiu S L, Luo Y T. Electrochim Acta, 2001; 31: 871
[19] Boen R, Bouteillon J. J Appl Electrochem, 1983; 13: 277
[20] Cohen U, Huggins R A. J Electrochem Soc, 1976; 123: 381