Ar gas was injected to the nozzle during continuous casting to prevent from nozzle clogging caused by solid inclusions, however, some gas bubbles were captured by the initial solidified billet shell, and subsequently billet defects were formed in final product. In present work, a physical model applying mold simulator was designed and used to investigate the bubble behavior in the solid/liquid interface. Different mold simulator angels and bubble diameters were considered, three typical behaviors were observed, some bubbles were captured by the solidified shell, several bubbles coalescence in the solid/liquid interface, and other bubbles stayed in the interface for a moment, and then left. The possible mechaism of gas bubble entrapped in solidified hell was anayzed. Besides, industial billets were studied, many dendites wee found around the hole, it was consdered to be a key factor for gas bubble engulfed in the solidification billets in the meniscus area. Further morethe effective technologes, such as electrical brake near the submerged entry nozzle and electrical stirring in the mold narrow face, can improve billet quality and reduce gas bubbles in solidified shewere imposed
JIN Xiao-Li
,
LEI Zuo-Qing
,
YU Tan
,
ZHANG Gao-Bin
,
DENG Kang
,
REN Zhong-Ming
. PHYSICAL SIMULATION OF Ar BUBBLE BEHAVIOR IN THE SOLID/LIQUID INTERFACE OF CONTINUOUS CASTING BILLET[J]. Acta Metall Sin, 2011
, 47(6)
: 763
-768
.
DOI: 10.3724/SP.J.1037.2010.00690
[1] Zhang L, Aoki J, Thomas B G. Metall Mater Trans, 2006; 37B: 361
[2] Pfeiler C, Wu M, Ludwig A. Mater Sci Eng, 2005; A413–414: 115
[3] Thomas B G, Huang X, Sussman R C. Metall Mater Trans, 1994; 25B: 527
[4] Singh V, Dash S K, Sunitha J S, Ajmani S K, Das A K. ISIJ Int, 2006; 46: 210
[5] Yu H Q, Zhu M Y. Acta Metall Sin, 2008; 44: 619
(于海岐, 朱苗勇. 金属学报, 2008; 44: 619)
[6] Yu H Q, Zhu M Y. Acta Metall Sin, 2008; 44: 1141
(于海岐, 朱苗勇. 金属学报, 2008; 44: 1141)
[7] Yu H X, Zhu G S, Wang X H, Zhang J M, Wang W J. J Univ Sci Technol Beijing, 2003; 25: 215
(于会香, 朱国森, 王新华, 张炯明, 王万军. 北京科技大学学报, 2003, 25: 215)
[8] Zhang S J, Zhu M Y, Zhang Y L, Zheng G S, Cheng N L, Song J X. Acta Metall Sin, 2006; 42: 1087
(张胜军, 朱苗勇, 张永亮, 郑淑国, 程乃良, 宋景欣. 金属学报, 2006; 42: 1087)
[9] Cao N, Zhu M Y. Acta Metall Sin, 2008; 44: 79
(曹 娜, 朱苗勇. 金属学报, 2008; 44: 79)
[10] Cao N, Zhu M Y. Acta Metall Sin, 2008; 44: 626
(曹娜, 朱苗勇. 金属学报, 2008; 44: 626)
[11] Feng W, Zhu C Y, Yu T J, Zhang H L, Liu C J, Jiang M F. Contin cast, 2007; (4): 4
(冯巍, 朱传运, 余挺进, 张红令, 刘承军, 姜茂发. 连铸, 2007; (4): 4)
[12] Lei H, Zhu M Y, He J C. Int J Cast Met Res, 2007; 20: 98
[13] Esaka H, Kuroda Y, Shinozuka K, Tamura M. ISIJ Int, 2004; 44: 682
[14] Chen Z H, Wang E G, Zhang X W, He J C. Acta Metall Sin, 2007; 43: 422
(陈芝会, 王恩刚, 张兴武, 赫冀成. 金属学报, 2007; 43: 422)
[15] Lei Z S, Zhang H B, Ren Z M, Deng K. J Iron Steel Res Int, 2008; 15(Suppl. 1): 538
[16] Yu Z, Zhang Z Q, Ren Z M, Lei Z S, Deng K. Acta Metall Sin, 2010; 46: 1275
(于湛, 张振强, 任忠鸣, 雷作胜, 邓康. 金属学报, 2010; 46: 1275)