论文

DENDRITE ARM SPACINGS AND MICROSEGREGATIONS IN <001>  AND <011> ORIENTATED SINGLE CRYSTAL SUPERALLOYS DD407

  • YANG Chu-Bin ,
  • LIU Lin ,
  • DIAO Xin-Bao ,
  • LIU Gang ,
  • ZHANG Jun ,
  • FU Heng-Zhi
Expand
  • State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi’an 710072

Received date: 2011-03-18

  Revised date: 2011-04-16

  Online published: 2011-10-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50931004 and 50827102), National Basic Research Program of China (Nos.2010CB631202 and 2011CB610406), Research Fund of the State Key Laboratory of Solidification Processing (NWPU) of China (Nos.09–BZ–2010 and 57–TZ–2011)

Abstract

Single crystal superalloys DD407 with <001> and <011> orientations were produced with seeding technique by using the liquid metal cooling Bridgman furnace. The dendrite arm spacings (DAS) and microsegregations in the single crystal superalloys with <001> and <011> orientations were investigated. The results indicated that increasing the deviation angle from <001> orientation or decreasing the deviation angle from <011> would increase the dendrite arm spacing. In addition, DAS of single crystal grown along <011> orientation is obviously greater than that of <001> orientation for side–branching. EMPA results showed that the positive segregation elements Al, Ti and Ta enriched in the interdendritic region, and the negative segregation element W enriched in the dendrite core. The microsegregation in the single crystal with <011> orientation paralleled to the sample axis is the lightest. It is found that not only the DAS but the mechanism of dendrite evolution and arrayed pattern of dendrite affect the degree of microsegregation.

Cite this article

YANG Chu-Bin , LIU Lin , DIAO Xin-Bao , LIU Gang , ZHANG Jun , FU Heng-Zhi . DENDRITE ARM SPACINGS AND MICROSEGREGATIONS IN <001>  AND <011> ORIENTATED SINGLE CRYSTAL SUPERALLOYS DD407[J]. Acta Metall Sin, 2011 , 47(10) : 1246 -1250 . DOI: 10.3724/SP.J.1037.2011.00142

References

[1] Huang Q Y, Li H K. Superalloys. Beijing: Metallurgical Industry Press, 2004: 2

(黄乾尧, 李汉康. 高温合金. 北京: 冶金工业出版社, 2004: 2)

[2] Hu ZQ, Liu L R, Jin T, Sun X F. Aeroengine, 2005; 31(3): 1

(胡壮麒, 刘丽荣, 金 涛, 孙晓峰. 航空发动机, 2005; 31(3): 1)

[3] Han G M, Yu J J, Sun Y L, Sun X F, Hu Z Q. Mater Sci Eng, 2010; A527: 5383

[4] Zhang S H, Zhang J, Lou L H. J Mater Sci Technol, 2011; 27: 107

[5] Ding G L, Tewari S N. J Cryst Growth, 2002; 236: 420

[6] Zhao X B, Liu L, Yu Z H, Zhang W G, Fu H Z. Mater Charact, 2010; 61: 7

[7] He G, Li J G, Mao X M, Fu H Z. Acta Metall Sin, 1995; 31: 469

(何国, 李建国, 毛协民, 傅恒志. 金属学报, 1995; 31: 469)

[8] Gandin C A, Eshelman M, Trivedi R. Metall Mater Trans, 1996; 27A: 2727

[9] Grugel R N, Zhou Y. Metall Trans, 1989; 20A: 969

[10] Huang T W, Liu L, Zhang W G, Zhang J, Fu H Z. Acta Metall Sin, 2009; 45: 1225

(黄太文, 刘林, 张卫国, 张军, 傅恒志. 金属学报, 2009; 45: 1225)

[11] Polock T M, Murphy W H, Goldman E H, Uram D L, Tu J S. In: Antolovich S D, Stusrud R W, Mackay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1992, Warrendale: TMS, 1992: 125

[12] Ma D X, Grafe U. Mater Sci Eng, 1999; A270: 339

[13] Kearsey R M, Beddoes J C, Jaansalu K M, Thompson W T, Au P. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Warrendale: TMS, 2004: 801

[14] Karunaratne M S A, Cox D C, Carter P, Reed R C. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S L, Schirra J J eds., Superalloys 2000, Warrendale: TMS, 2000: 263

[15] Seo S M, Lee J H, Yoo Y S, Jo C Y, Miyahara H, Ogi K. In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S R eds., Superalloys 2008, Warrendale: TMS, 2008: 277

[16] Zhao X B, Liu L, Zhang W G, Liu G, Zhang J, Fu H Z. Mater Lett, 2009; 63: 2635

[17] Hunt J D. Solidification and Casting of Metals. London: The Metals Society, 1979: 3

[18] Kurz W, Fisher D J. Acta Metall, 1981; 29: 11

[19] Trivedi R. Metall Trans, 1984; 15A: 977

[20] Han S H, Trivedi R. Acta Metall Mater, 1994; 1: 25

[21] An G Y, Liu L X. J Cryst Growth, 1987; 80: 383

[22] Zhao X B. PhD Thesis, Northwestern Polytechnical University, Xi’an, 2010

(赵新宝. 西北工业大学博士学位论文, 西安, 2010)

[23] Till W A, Jackson K A, Rutter J W, Chalmers B. Acta Metall, 1953; 1: 428

[24] Schneider M C, Gu J P, Beckermann C, Boettinger W J, Kattner U R. Metall Mater Trans, 1997; 28A: 1517

[25] Ma D, Sahm P R. Giesserei–Forschung, 1990; 82: 869

[26] Basaran M. Metall Trans, 1981; 12A: 1235

[27] Gu L Y, Liu Z Y, Shi Z X. Trans Nonferrous Met Soc China, 1996; 6: 110

(顾林喻, 刘忠元, 史正兴. 中国有色金属学报, 1996; 6: 110)

[28] Karunaratne M S A, Carter P, Reed R C. Mater Sci Eng, 2000; 281A: 229

[29] Zhao N R, Wang Z H, Li J G, Jin T, Sun X F, Yang H C, Hu Z Q. J Mater Eng, 2008; 2: 58

(赵乃仁, 王志辉, 李金国, 金涛, 孙晓峰, 杨洪才, 胡壮麒. 材料工程, 2008; 2: 58)
Outlines

/