LOW TEMPERATURE DEFORMATION BEHAVIOR OF HIGH–NITROGEN NICKEL–FREE AUSTENITIC STAINLESS STEELS

  • XU Meng-Zhou ,
  • YU Jian-Jun ,
  • LIU Chun-Meng
Expand
  • Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819

Received date: 2011-03-17

  Revised date: 2011-05-06

  Online published: 2011-10-11

Supported by

Supported by National Science and Technology Major Project of China (No.2009ZX04008–021) and Project of Department of Science and Technology of Liaoning Province (No.2007221007)

Abstract

The low–temperature deformation behaviors of two high–nitrogen nickel–free austenitic stainless steels (HNSs) with different N content were investigated by impact test, tensile test, XRD and TEM. The results indicate that HNS shows apparent ductile–to–brittle transformation (DBT) and work–hardening at low temperature. In the range of the experimental steels’ Mn content, the increase of Mn content improved the plasticity and the toughness at low temperature, and decreased the DBT temperature of HNS. Deformation–induced martensite transformation occurs in steel 18Cr–12Mn–0.55N during tensile deformation at low temperature, but the content of martensite is low and the decrease of temperature has no obvious effect on its formation. Deformation–induced martensite enhances the work–hardening ability but decreases the plasticity and toughness of HNS at low temperature. The decreases of work–hardening ability and stacking fault energy with temperature decreasing are the main reasons for brittle fracture of Fe–Cr–Mn HNS at low temperature.

Cite this article

XU Meng-Zhou , YU Jian-Jun , LIU Chun-Meng . LOW TEMPERATURE DEFORMATION BEHAVIOR OF HIGH–NITROGEN NICKEL–FREE AUSTENITIC STAINLESS STEELS[J]. Acta Metall Sin, 2011 , 47(10) : 1335 -1341 . DOI: 10.3724/SP.J.1037.2011.00141

References

[1] Cheng X N, Dai Q X. The Design and Control of Austenitic Stainless Steel. Beijing: National Defense IndustryPress, 2005: 3

(程晓农, 戴起勋. 奥氏体钢设计与控制. 北京: 国防工业出版社, 2005: 3)

[2] Mudali U K, Raj B, translated by Li J, Huang Y H. High Nitrogen Steels and Stainless Steels, Manufacturing, Properties and Applications. Beijing: Chemical Industry Press, 2006: 5

(Mudali U K, Raj B著, 李晶, 黄运华  译. 高氮钢和不锈钢--生产、性能与应用. 北京: 化学工业出版社, 2006: 5)

[3] Ilola R J, Hänninen H E, Ullakko K M. ISIJ Int, 1996; 36: 873

[4] Tomota Y, Endo S. ISIJ Int, 1990; 30: 656

[5] Gavriljuk V G, Sozinova A L, Foct J, Petrov J N, Polushkin Y A. Acta Mater, 1998; 46: 1157

[6] Milititsky M, Matlock D K, Regully A, Dewispelaere N, Penning J, Hanninen H. Mater Sci Eng, 2008; A496: 189

[7] Tomoto Y, Xia Y, Inoue K. Acta Mater, 1998; 46: 1577

[8] Ishizaka J, Orita K, Terao K. Tetsu Hagan´e, 1992; 78: 1846

[9] Tobler R L, Leyn D. Metall Mater Trans, 1988; 19A: 1626

[10] Ojima M, Adachi Y, Tomota Y, Ikeda K, Katada Y. J Jpn Inst Met, 2009; 73: 283

[11] Milititsky M, Matlock D K, Regully A. Mater Sci Eng, 2008; A496: 189

[12] Saller G, Hahn K S, Scheu C, Clemens H. Mater Sci Eng, 2006; A427: 246

[13] Liu S X, Liu X M, Liu R, Wang C X, Xing F. J Iron Steel Res, 2005; 17: 40

(刘树勋, 刘宪民, 刘蕤, 王春旭, 邢峰. 钢铁研究学报, 2005; 17: 40)

[14] Simmons J W. Acta Mater, 1997; 45: 2467

[15] Breedis J, Robertson W. Acta Metall, 1962; 10: 1077

[16] Lee T H, Oh C S, Kim S J. Scr Mater, 2008; 58: 110

[17] Liu S Y, Liu D Y, Liu S C. J Mater Sci, 2007; 42: 7514

[18] Cheng X N, Dai Q X. The Design and Control of Austenitic Stainless Steel. Beijing: National Defense Industry Press, 2005: 28

(程晓农, 戴起勋. 奥氏体钢设计与控制. 北京: 国防工业出版社, 2005: 28)

[19] Gavriljuk V G, Berns H. High Nitrogen Steels. Berlin: Springer, 1999: 192

[20] Kibey S, Liu J B, Curtis M J, Johnson D D, Sehitoglu H. Acta Mater, 2006; 54: 2991

[21] Hu B F, Jia C C. Acta Metall Sin, 2001; 37: 703

(胡本芙, 贾成厂. 金属学报, 2001; 37: 703)

[22] Hübner W, Pyzalla A, Assmus K, Wild E, Wroblewski T. Wear, 2003; 255: 476

[23] Gulyaev A P, Lebedev D V, Gadzhibalaev G A. Met Sci Heat Treat, 1973; 15: 1051

[24] Wang S T. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2008

(王松涛. 中国科学院金属研究所博士学位论文, 沈阳, 2008)

[25] Byun T S, Hashimoto N, Farrell K. Acta Mater, 2004; 52:3889

[26] Wang W, Yan W, Yang K, Shan Y Y. J Mater Eng Perform,2010; 19: 1214
Outlines

/