论文

CHARACTERIZATION OF TiAl PRE–ALLOYED POWDER AND ITS DENSIFICATION MICROSTRUCTURE

  • YU Gang ,
  • ZHENG Zhuo ,
  • CHANG Li-Shou ,
  • XU Lei ,
  • CUI Yu-You ,
  • YANG Rui
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2011-03-16

  Revised date: 2011-04-27

  Online published: 2011-10-11

Abstract

TiAl pre–alloyed powder (nominal composition Ti–47Al–2Cr–2Nb–0.2W–0.15B, atomic fraction, %) was produced by electrode induction melting gas atomization (EIGA) technique. The average diameter is 120.7 μm, and the distribution of the powder diameter follows Gaussian distribution. The phase constitution is a function of particle diameter. The amount of the γ phase increases with powder diameter increasing, the finest powder consists of predominantly α2 phase. The α2 phase in the powder was transformed into γ phase after annealing at temperatures higher than 500 ℃. Local coarsening was observed in the microstructure of TiAl compact duo to the microsegregation of elements in the powder. The XPS result indicated that the outer layer of the TiAl pre–alloyed particle consists of a thin layer of Al2O3 and TiO2.

Cite this article

YU Gang , ZHENG Zhuo , CHANG Li-Shou , XU Lei , CUI Yu-You , YANG Rui . CHARACTERIZATION OF TiAl PRE–ALLOYED POWDER AND ITS DENSIFICATION MICROSTRUCTURE[J]. Acta Metall Sin, 2011 , 47(10) : 1263 -1269 . DOI: 10.3724/SP.J.1037.2011.00136

References

[1] Dimiduk D M. Mater Sci Eng, 1999; A263: 281

[2] Thomas M, Berteaux O, Popoff F, Bacos M P, Morel A, Passilly B, Ji V. Intermetallics, 2006; 14: 1143

[3] Lu X, Zhao L M, Qu X H. Mater Rev, 2006; 20(8): 69

(路新, 赵丽明, 曲选辉. 材料导报, 2006; 20(8): 69)

[4] Gouma P I, Saunders N, Loretto M H. Mater Sci Technol, 1996; 12: 823

[5] Gerling R, Clemens H, Schimansky F P. Adv Eng Mater, 2004; 6: 23

[6] Unal R. J Mater Process Technol, 2006; 180: 291

[7] Wegmann G, Gerling R, Schimansky F P. Acta Mater, 2003; 51: 741

[8] Clemens H. Z Metallk, 1995; 86: 814

[9] Zhang Y W, Shangguang Y H. Powder Metall Ind, 2004; 14(6): 30

(张义文, 上官永恒. 粉末冶金工业, 2004; 14(6): 30)

[10] Miles T E, Rhodes J F. In: Mehrabian R, Kear  B H, Cohen M, eds., Rapid Solidification Processing: Principles and Technologies. Baton Rouge: Claitor’s Pub, 1978: 347

[11] Cahn R W. Mater Sci Eng, 2002; A324: 1

[12] Wang P, Viswanathan G B, Vasudevan V K. Metall Mater Trans, 1992; 23A: 690

[13] Fischer F D, Cha L, Dehm G, Clemens H. Intermetallics, 2010; 18: 972

[14] Adams A G, Rahaman M N, Dutton R E. Mater Sci Eng, 2008; A477: 137

[15] Rao G A, Srinivas M, Sarma D S. Mater Sci Eng, 2006; A435–436: 84
Outlines

/

〈 〉