论文

EFFECT OF THE CROSS-INTERACTION ON THE FORMATION AND EVOLUTION OF INTERMETALLIC COMPOUNDS IN Cu(Ni)/Sn-Ag-Cu/Cu(Ni) BGA STRUCTURE SOLDER JOINTS

  • LI Xun-Beng ,
  • ZHOU Min-Bei ,
  • YAN Jian-Min ,
  • MA Xiao ,
  • ZHANG Xin-Beng
Expand
  • School of Materials Science and Engineering, South China University of Technology, Guangzhou 510640

Received date: 2011-01-27

  Revised date: 2011-02-10

  Online published: 2011-05-11

Supported by

Supported by Program of New Century Excellent Talents in University (No.NCET-04-0824) and Science and Technology Major Project of Guangdong Province (No.2009A080204005)

Abstract

The formation and evolution of interfacial intermetallic compounds (IMCs) in Cu(Ni)/Sn-3.0Ag-0.5Cu/Cu(Ni) BGA (Ball Grid Array) structure solder joints both in the as-reflowed state and undergoing isothermal aging at 125℃ were investigated. The results show that there exists a significant cross-interaction effect of the solder pad/under bump metal (UBM) on the composition, morphology and growth kinetics of interfacial IMCs in solder joints. The reactions of solder/Ni UBM strongly depends on the Cu content of the solder, for a high Cu content, a continuous (Cu, Ni)6Sn5 layer forms at the interface, while for a low Cu content, a continuous (Ni, Cu)3Sn4 layer appears at the interface. The cross-interaction of Cu and Ni in Cu/Sn-3.0Ag-0.5Cu(SAC)/Ni solder joints has obvious influence on the composition and morphology of the interfacial IMC; and the IMC spalling phenomenon occurs at the interface of Ni side. During isothermal aging at 125℃, the growth rate constant of the interfacial IMC layer in SAC/Cu and Cu/SAC/Cu joints increases with the Cu concentration, and the cross-interaction of Cu and Cu decreases the interfacial IMC growth rate constant at once-reflowed Cu side. However, both of the cross-interactions of Cu-Ni and Ni-Ni increase the growth rate constant of the interfacial IMC at once-reflowed Ni side and Ni has a greater influence than Cu. The cross-interaction of Cu and Ni is beneficial for suppression of growth of Cu3Sn and reduction the growth rate of IMC at Cu side, while having no significant influence on the porosity of Kirkendall voids in Cu3Sn layer at Cu side of the joint.

Cite this article

LI Xun-Beng , ZHOU Min-Bei , YAN Jian-Min , MA Xiao , ZHANG Xin-Beng . EFFECT OF THE CROSS-INTERACTION ON THE FORMATION AND EVOLUTION OF INTERMETALLIC COMPOUNDS IN Cu(Ni)/Sn-Ag-Cu/Cu(Ni) BGA STRUCTURE SOLDER JOINTS[J]. Acta Metall Sin, 2011 , 47(5) : 611 -619 . DOI: 10.3724/SP.J.1037.2011.00063

References

[1] Alam M O, Chan Y C. Chem Mater, 2003; 15: 4340

[2] Tsai C M, Luo W C, Chang C W, Shieh Y C, Kao C R. J Electro Mater, 2004; 33: 12

[3] Yoon J W, Jung S B. J Alloys Compd, 2008; 448: 177

[4] Wang Y W, Chang C C, Kao C R. J Alloys Compd, 2009; 478:L1

[5] Ho C E, Lin Y L, Kao C R. Chem Mater, 2002; 14: 949

[6] Lee J H, Shin D H, Kim Y S. Met Mater Int, 2003; 9: 577

[7] Hong K K, Ryu J B, Park C Y, Huh J Y. J Electro Mater, 2008; 37: 61

[8] Zhou M B, Li X P, Ma X, Zhang X P. Acta Metall Sin, 2010; 46: 569

(周敏波, 李勋平, 马骁, 张新平. 金属学报. 2010; 46: 569)

[9] Jang G Y, Duh J G. J Electro Mater, 2006; 35:2061

[10] Ahat S, Sheng M, Luo L. J Electro Mater, 2001; 30:1317

[11] Tsai J Y, Hu YC, Tsai C M, Kao C R. J Electro Mater, 2003; 32: 1203

[12] Jeon Y D, Nieland S, Ostmann A, Reichl H, Paik K W. J Electro Mater, 2003; 32: 548

[13] He M, Lau W H, Qi G J, Chen Z. Thin Solid Films, 2004; 462–463: 376

[14] Vuorinen V, Yu H, Laurila T, Kivilahti J K. J Electro Mater, 2008; 37: 792

[15] Chen H T, Wang C Q, Li M Y, Tian D W. Mater Lett, 2006; 60: 1669

[16] Vuorinen V, Laurila T, Mattila T, Heikinheimo E, Kivilahti J K. J Electro Mater, 2007; 36: 1355

[17] Gagkuano R A, Fine E M. J Electron Mater, 2003; 32: 1441

[18] Takenaka T, Kano S, Kajihara M, Kurokawa N, Sakamoto K. Mater Sci Eng, 2005; A396: 115

[19] Wang S J, Liu C Y. J Electro Mater, 2006; 35: 1955

[20] Yoon JW, Kim B K, Shur C C, Jung S B. J Alloys Compd, 2009; 486: 142

[21] Gao F, Takemoto T, Nishikawa H. Mater Sci Eng, 2006; A420: 39

[22] Zeng K J, Stierman R, Chiu TC, Edwards D. J Appl Phys, 2005: 024508

[23] Blair H D, Pan T Y, Nicholson J M. 48th Electronic Components Technology Conference, USA: IEEE, 1998: 259

[24] Gong J C, Liu C Q, Conway P P, Silberschmidt V V. Acta Mater, 2008; 56: 4291

[25] Gao F, Choi S, Subramanian K N, Bieler T R, Lucas J P, Achari A, Paruchuri M. Mater Sci Eng, 2003; A351: 190
Outlines

/

〈 〉