论文

THREE DIMENSIONAL DYNAMICAL MEASUREMENT OF DISTORTION OF HEAVY STEEL CASTINGS DURING HEAT TREATMENT PROCESS

  • KANG Jin-Wu ,
  • ZHE Gang ,
  • YU Hai-Liang ,
  • MANG Hai-Min ,
  • HAO Xiao-Kun ,
  • HUANG Tian-You ,
  • HU Yong-Yi
Expand
  • 1) Department of Mechanical Engineering, Key Laboratory for Advanced Materials Processing Technology, Tsinghua University, Beijing 100084
    2) State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110004

Received date: 2010-11-16

  Revised date: 2011-01-14

  Online published: 2011-05-11

Abstract

At the forced air cooling stage in normalizing process of heavy steel castings, the nonuniform cooling might result in thermal and phase transformation stresses, which might cause the distortion, especially for the heavy yet thin blade castings. Dynamical measurement of the distortion of castings during heat treatment process will be significant for understanding the mechanism of distortion and then taking the control measures in productions. In this paper, a novel measuring method, fixed direction method, was proposed, which could three-dimensionally and dynamically measure the distortion of castings without index points at high temperature, and the corresponding analysis method was established. The method was employed to measure the distortion of a hydro blade casting at the forced cooling stage in normalizing process, and the dynamical distortion behavior in three dimensions of the blade casting was obtained. And the measurement error of blade casting was analyzed. The results show that under the conditions of no index points and high temperature, the three-dimensional distortion of castings could be dynamically measured through the fixed direction method.

Cite this article

KANG Jin-Wu , ZHE Gang , YU Hai-Liang , MANG Hai-Min , HAO Xiao-Kun , HUANG Tian-You , HU Yong-Yi . THREE DIMENSIONAL DYNAMICAL MEASUREMENT OF DISTORTION OF HEAVY STEEL CASTINGS DURING HEAT TREATMENT PROCESS[J]. Acta Metall Sin, 2011 , 47(5) : 535 -539 . DOI: 10.3724/SP.J.1037.2010.00617

References

[1] Yu H L, Kang J W, Huang T Y. Front Mater Sci, 2010; 4: 332

[2] Huang T Y, Liu X G, Kang J W, Shen H F, Liu B C. Foundry, 2007; 56: 899

(黄天佑, 刘小刚, 康进武, 沈厚发, 柳百成. 铸造, 2007; 56: 899)

[3] Liu B C, Kang J W, Xiong S M. Sci Technol Adv Mater, 2001; 2: 157

[4] Bruschi S, Ghiotti A. Int J Machine Tools Manuf, 2008; 48: 761

[5] Yu H L, Kang J W, Huang S X, Huang T Y. Adv Mater Res, 2011; 148–149: 103

[6] Wang P, Xiao N, Li D, Li Y. Mater Sci Forum, 2010; 654– 656: 1565

[7] Wang Z K, Hu Z H. Dongfang Electric Rev, 2004; 18(3): 137

(王贞凯, 胡章洪. 东方电气评论, 2004; 18(3): 137)

[8] Wang Y X, Zhang P C, Li B C, Zeng W D. China Foundry Mach Technol, 2007; 1: 24

(王云霞, 张鹏程, 李宝治, 曾卫东. 中国铸造装备与技术, 2007; 1: 24)

[9] Yu H L, Kang J W, Huang T Y. Sci China, 2011; 54E: 81

[10] Jiang R S, Zhang D H, Wang W H, Bu K, Cheng Y Y. Spec Cast Nonferrous Alloys, 2009; 29(1): 13

(蒋睿嵩, 张定华, 汪文虎, 卜 昆, 程云勇. 特种铸造及有色合金, 2009; 29(1): 13)

[11] Han W, Yu W S, Kong S G, Wu J T, Li J T, Ma Z L, Zhao M H. Foundry, 2009; 58: 1108

(韩伟, 于望生, 孙胜国, 吴剑涛, 李俊涛, 马章林, 赵明汉. 铸造, 2009; 58: 1108)

[12] Yu H L, Kang J W, Nie G, Long H M, Hao X K, Huang T Y. China Foundry, 2011; in press

[13] Coret M, Combescure A. Int J Mech Sci, 2002; 44: 1947

[14] Sun C Y, Fang G, Lei L P, Zeng P. Trans Mater Heat Treat, 2008; 29: 162

(孙朝阳, 方刚, 雷丽萍, 曾 攀. 材料热处理学报, 2008; 29: 162)