论文

STUDY ON THE BEHAVIOR OF HYDROGEN IN STEEL HEAT TREATMENT PROCESS WITH PROTON CONDUCTOR SENSOR

  • LI Yang ,
  • DING Yu-Shi ,
  • HU Jing-Shou ,
  • YU Chang-Zhen
Expand
  • College of Materials and Metallurgy, Northeastern University, Shenyang 110819

Received date: 2010-11-16

  Revised date: 2011-01-13

  Online published: 2011-05-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50774018 and 51074038)

Abstract

The dehydrogenation behavior in two steels during heat treatment process was investigated by using CaZr0.9In0.1O3-α proton conductor hydrogen sensor and electrochemical impedance spectroscopes of these steels have been measured and analyzed. Based on the changes of hydrogen partial pressure in these steels with temperature and with time at constant temperatures of 600℃ and 800℃, it is found that the dehydrogenation begins only when heat treatment temperature is higher than 600℃. Although this temperature exceeds higher than 727℃, the dehydrogenation behavior is not significantly improved. This means that the reasonable heat treatment temperature is in the range of 600-730℃. The experimental results show that the CaZr0.9In0.1O3-α proton conductor hydrogen sensor could be used to monitor in situ changes of partial hydrogen pressure during dehydrogenation of solid state steels as a suitable sensor.

Cite this article

LI Yang , DING Yu-Shi , HU Jing-Shou , YU Chang-Zhen . STUDY ON THE BEHAVIOR OF HYDROGEN IN STEEL HEAT TREATMENT PROCESS WITH PROTON CONDUCTOR SENSOR[J]. Acta Metall Sin, 2011 , 47(5) : 553 -558 . DOI: 10.3724/SP.J.1037.2010.00615

References

[1] Nagumo M, Yagi T, Saitoh H. Acta Mater, 2000; 48: 943

[2] Ohmisawa T, Uchiyama S, Nagumo M. J Alloys Compd, 2003; 356–357: 290

[3] Nagumo M, Matsuda H. Philos Mag, 2002; 82A: 3415

[4] Zhu J C, Li D C. Foundry Technol, 2003; 24(2): 83

(朱家琛, 李德臣. 铸造技术, 2003; 24(2): 83)

[5] Kanezaki T, Narazaki C, Mine Y, Matsuoka S, Murakami Y. Int J Hydrogen Energy, 2008; 10: 2604

[6] Singh S, Altstetter C. Metall Trans, 1982; 10A: 1799

[7] Zheng C L, Zhang F C, L¨u B, Wang T S, Zheng Y Z. Trans Mater Heat Treat, 2008; 29(2): 71

(郑春雷, 张福成, 吕 博, 王天生, 郑炀曾. 材料热处理学报, 2008; 29(2): 71)

[8] Melnick L M. Translated by Liu C S. Determination of Gaseous Elements in Metals. Beijing: Metallurgy Industry Press, 1987: 19

(Melnick L M, 刘崇嗣译. 金属中气体元素的测定. 北京: 冶金工业出版社, 1987: 199)

[9] Bilic A, Gale J D. Solid State Ionics, 2008; 179: 871

[10] Mercier V M M, Sluis P V D. Solid State Ionics, 2001; 145: 17

[11] Pollet M, Daturi M, Marinel S. J Eur Ceram Soc, 2004; 24: 1805

[12] Yajima T, Kazeoka H, Yogo T, Iwahara H. Solid State Ionics, 1991; 47: 271

[13] Iwahara H, Shimura T, Matsumoto H. Electrochemistry, 2000; 68: 154

[14] Katahira K, Matsumoto H, Iwahara H, Koide K, Iwamoto T. Sens Actuators, 2001; 73B: 130

[15] Hang Z T. Industrial Catalysis. Beijing: Chemical Industry Press, 2006: 50

(黄仲涛. 工业催化. 北京: 化学工业出版社, 2006: 50)
Outlines

/