论文

PREPARATION OF SEMISOLID 5052 ALUMINUM ALLOY SLURRY BY INDIRECT ULTRASONIC VIBRATION

  • LV Shu-Lin ,
  • WU Shu-Sen ,
  • DAI Wei ,
  • AN Ping ,
  • MAO Wei-Wu
Expand
  • State Key Lab of Materials Processing and Die & Mould Technology, Huazhong University of Science and Technology, Wuhan 430074

Received date: 2010-10-15

  Revised date: 2011-01-04

  Online published: 2011-05-11

Supported by

Supported by National Natural Science Foundation of China (No.50775086) and High Technology Research and Development Program of China (No.2007AA03Z557)

Abstract

A new indirect ultrasonic vibration (IUV) apparatus was employed to prepare semisolid 5052 aluminum slurry. The effects of IUV temperature and time on the morphology of the semisolid slurry were studied. The results indicate that semisolid slurry with fine and globular primary grains can be obtained by applying IUV from the liquidus temperature (643℃) of this alloy or a higher temperature for about 50 s. When IUV is applied through the bottom of the metal cup at 643℃, a lot of nuclei form near the bottom of metal cup and these nuclei grow into globular grains. In this stage, the average diameter of primary grains decreases as IUV time increased up to 30 s and then it increases with further increasing of IUV time from 30 s to 60 s, and the average shape coefficient of primary grains increases as IUV time increased. When the IUV is applied at 640℃, dendrites can be broke up and a mixture structure consisted of rosette and globular grains with a average diameter of 105 μm is obtained.

Cite this article

LV Shu-Lin , WU Shu-Sen , DAI Wei , AN Ping , MAO Wei-Wu . PREPARATION OF SEMISOLID 5052 ALUMINUM ALLOY SLURRY BY INDIRECT ULTRASONIC VIBRATION[J]. Acta Metall Sin, 2011 , 47(5) : 634 -640 . DOI: 10.3724/SP.J.1037.2010.00552

References

[1] Wu S S, Zhao J W, Zhang L P, An P, Mao Y W. Solid State Phenom, 2008; 141–143: 451

[2] Zhao JW,Wu S S, Wan L, Chen Q H, An P. Acta Metall Sin, 2009; 45: 314

(赵君文, 吴树森, 万里, 陈启华, 安 萍. 金属学报, 2009; 45: 314)

[3] Zhao JW,Wu S S, An P, Mao YW. Solid State Phenom, 2008; 141–143: 767

[4] Abramov V, Abramov O, Bulgakov V, Sommer F. Mater Lett, 1998; 37: 27

[5] Eskin G I, Eskin D G. Ultrason Sonochem, 2003; 10: 297

[6] Jian X, Xu H, Meek T T, Han Q. Mater Lett, 2005; 59: 190

[7] Gao D M, Li Z J, Han Q Y, Zhai Q J. Mater Sci Eng, 2009; A502: 2

[8] Liu Q M, Zhang Y, Song Y L, Qi F P, Zhai Q J. Mater Des, 2007; 28: 1949

[9] Kaibyshev R, Musin F, Lesuer D R, Nieh T G. Mater Sci Eng, 2003; A342: 169

[10] Piao L, Motegi T. J Jpn Inst Light Met, 2005; 55(2): 86

[11] Lu S L, Wu S S, Zhu Z M, An P, Mao Y W. Trans Nonferrous Met Soc China, 2010; 20: 758

[12] Lu S L, Wu S S, Dai W, Zhu Z M, Mao, Y W, Wan L. Spec Cast Nonferrous Alloys, 2010; 30: 326

(吕书林, 吴树森, 戴维, 朱泽明, 毛有武, 万 里. 特种铸造及有色合金, 2010; 30: 326)

[13] Liu C, Pan Y, Aoyama S. In: Bhasin A K, Moore J J, Young K P, Midson S, eds., Proc 5th Int Conf on Semi–solid Processing of Alloys and Composites, Colorado: Golden, 1998: 431

[14] Kapustina O A. The Physical Principles of Ultrasonic Manufactureing. Moscow: Nauka, 1970: 45

[15] Ohno A. Solidification: The Separation Theory and Its Practical Applications. Berlin: Springer, 1987: 1

[16] Qian M, Ramirez A, Das A. J Cryst Growth, 2009; 311: 3708

[17] Wu S S, Xie L Z, Zhao J W, Nakae H. Scr Mater, 2008; 58: 556

[18] Qian M, Ramirez A, Das A, Stjohn D H. J Cryst Growth, 2010; 312: 2267

[19] Taghavi F, Saghafian H, Kharrazi Y H K. Mater Des, 2009; 30: 115

[20] Campbell J. Int Mater Rev, 1981; 2: 71
Outlines

/

〈 〉