论文

MICROSTRUCTURE EVOLUTION OF LAVES PHASE Cr2Nb/Cr ALLOYS PREPARED BY ARC MELTING

  • LI Ke-Wei ,
  • LI Shuang-Meng ,
  • FU Heng-Zhi
Expand
  • State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi’an 710072

Received date: 2010-12-27

  Revised date: 2011-03-22

  Online published: 2011-06-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50971101 and 51074127), Specialized Research Fund for the Doctoral Program of Higher Education (No.20096102110011) and Basic Research Foundation of NWPU (No.JC201029)

Abstract

The Cr–12%Nb (atomic fraction) and Cr–20%Nb alloys prepared by vacuum non–consumable arc melting were investigated to understand the  icrostructure evolution of the Laves phase Cr2Nb/Cr alloys. The solidified microstructures including the phase formation and competitive growth were studied using OM, XRD as well as SEM with an EDS. The results showed that different microstructure morphologies were observed in the Cr–12%Nb and Cr–20%Nb alloys. For the Cr–12%Nb alloy, divorced eutectics were grown at the bottom part of the ingot. Primary Cr dendrites and coupled eutectic (Cr2Nb+Cr) appeared in the middle and upper part of the ingot. For the Cr–20%Nb alloy, cellular eutectics of which the lamellar spacing was about 0.3 μm were found at the bottom of the ingot. With the decrease in cooling rate in the middle and upper part of the ingot, plate primary Cr2Nb dendrites and petal–like Cr2Nb dendrites were developedBesides, using the TMK model for rapid utctc solidification and the BCT dendrtc growth model, the inteface growth temperatures between the coupled eutectic (Cr2Nb+Cr) and priary Cr2Nb phase wee computed and compared with the experimental results. Based on the maximum interface growth temperature criteria, the earance of multiple solidified microstructures of the Cr–20%Nb alloy could be explaind  successfully.

Cite this article

LI Ke-Wei , LI Shuang-Meng , FU Heng-Zhi . MICROSTRUCTURE EVOLUTION OF LAVES PHASE Cr2Nb/Cr ALLOYS PREPARED BY ARC MELTING[J]. Acta Metall Sin, 2011 , 47(6) : 663 -670 . DOI: 10.3724/SP.J.1037.2010.00700

References

[1] Kazantzis A V, Aindow M, I P Jones, Triantafyllidis G K, Hosson J Th M De. Acta Mater, 2007; 55: 1873

[2] Von Keitz A, Sauthoff G. Intermetallics, 2002; 10: 497

[3] Liu C T, Zhu J H, Brady M P, McKamey C G, Pike L M. Intermetallics, 2000; 8: 1119

[4] Machon L, Sauthoff G. Intermetallics, 1996; 4: 469

[5] Liu C T, Tortorelli P F, Horton J A, Carmichael C A. Mater Sci Eng, 1996; A214: 23

[6] Xiao X, Lu S Q, Ma Y Q, Hu P, Huang M G, Nie X W.Rare Met Mater Eng, 2008; 37: 119

(肖 璇, 鲁世强, 马燕青, 胡 平, 黄明刚, 聂小武. 稀有金属材料与工程, 2008; 37: 119)

[7] Bewlay B P, Lipsitt H A, Jackson M R. Mater Sci Eng, 1995; A192–193: 534

[8] Bewlay B P, Sutliff J A, Jackson M R. Acta Metall Mater, 1994; 42: 2869

[9] He Y D, Qu X H, Huang B Y. Rare Mater, 2003; 3: 303

(何玉定, 曲选辉, 黄伯云. 稀有金属, 2003; 3; 303)

[10] Thoma D J, Perepezko J H. Mater Sci Eng, 1992; A156: 97

[11] Thoma D J, Perepezko J H. Mater Sci Eng, 1992; A156: 97

[12] Kumar K S, Hazzledine P M. Intermetallics, 2004; 12: 763

[13] Kazantzis A V, Aindow M, Jones I P, Triantafyllidis G K, De Hosson J Th M. Acta Mater, 2007; 55: 1873

[14] Tiller W A. The Science of Crystallization: Macroscopic Phenomena and Defect Generation. Cambridge: Cambridge University Press, 1992: 254

[15] Kurz W, Fisher D J. Fundamentals of Solidification. 4nd Ed. Switzerland: Trans Tech Publications Ltd., 2005: 108

[16] Fu H Z, Guo J J, Liu L, Li J S. Directional Solidification and Processing of Advanced Materials, Beijing: Science Press, 2008: 308

(傅恒志, 郭景杰, 刘 林, 李金山. 先进材料定向凝固, 北京: 科学出版社, 2008: 308)

[17] Trivedi R, Magnin P, Kurz W. Acta Metall, 1987; 35: 971

[18] Boettinger W J, Coriell S R, Trivedi R. Rapid Solidification Processing: Principles and Technology IV. Bataon Rouge LA: Clatitor’s Publishing Division, 1988: 13

[19] Li M, Kuribayashi K. Metall Mater Trans, 2003; 34A: 2999

[20] Liu R, Volkmann T, Herach M. Acta Mater, 2001; 49439

[21] Umeda T, Okane T, Kurz W. Acta Mater, 1996; 44: 4209

[22] Hu H Q. Theory of Metal Solidification, 2nd Ed. Beijing: China Machine Press, 2007: 168

(胡汉起. 金属凝固原理. 北京: 机械工业出版社, 2007: 168)

[23] Ohno A. translated by Xing J D, Solidification of Metals: Theory, Practice and Application. Beijing: China Machine Press, 1990: 117

(Ohno A, 刑建东 译. 金属的凝固---理论、实践及应用. 北京: 机械工业出版社, 1990: 117)

[24] Stefanescu D M. Science and Engineering of Casting Solidification, 2nd Ed. Berlin: Springer, 2009: 195
Outlines

/

〈 〉