MAGNETIC STRUCTURE OF RAPIDLY QUENCHED FeCo-BASED RIBBON ANNEALED UNDER TENSILE STRESS IN FLOWING ATMOSPHERE

  • FANG Yuan-Zhang ,
  • XU Qi-Meng ,
  • YE Hui-Qun ,
  • FAN Xiao-Zhen ,
  • QIU Jian-Feng
Expand
  • 1) School of Materials Science and Engineering, Xi'an University of Architecture and Technology, Xi'an 710055
    2) College of Mathematics, Physics and Information Engineering, Zhejiang Normal University, Jinhua 321004

Received date: 2010-11-08

  Revised date: 2011-01-19

  Online published: 2011-04-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50871104 and 11079029), Natural Science Foundation of Zhejiang Province (No.Y4080324) and Natural Science Foundation of Shaanxi Province (No.Sj08e101)

Abstract

The FeCo-based ribbons (Fe36Co36Nb4Si4.8B19.2) with dirrerent magnetic structures were prepared by single roller quenched method and then annealed with direct current under tensile stress in flowing atmosphere. The longitudinally driven giant magneto-impedance (LDGMI) effect in the stress-Joule-heated FeCo-based ribbon was measured with HP4294A impedance analyzer. The dependences between the characteristic parameters of the LDGMI profiles, ratio of giant magneto-impedance and half-height width of the applied magnetic field at the bottom, and driving current frequency were analyzed. The difference of the LDGMI profiles of the annealed FeCo-based ribbons with various remained thicknesses obtained by etching with 16.7% HCl solution was compared. The mechanism and the character of the stress-induced magnetic structure in FeCo-based ribbons were exposured by means of the principle of the skin effect and the theory of the dependence of giant magneto-impedance on the magnetic anisotropy in the magnetic materials.

Cite this article

FANG Yuan-Zhang , XU Qi-Meng , YE Hui-Qun , FAN Xiao-Zhen , QIU Jian-Feng . MAGNETIC STRUCTURE OF RAPIDLY QUENCHED FeCo-BASED RIBBON ANNEALED UNDER TENSILE STRESS IN FLOWING ATMOSPHERE[J]. Acta Metall Sin, 2011 , 47(4) : 475 -481 . DOI: 10.3724/SP.J.1037.2010.00597

References

[1] Duwez P, Lin S C H. J Appl Phys, 1967; 38: 4096

[2] Masumoto T, Kimura H M, Inoue A, Waseda Y. Mater Sci Eng, 1976; 24: 141

[3] Kikuchi M, Fujimori H, Obi T, Masumoto T. Jpn J Appl Phys, 1975; 14: 1077

[4] Yoshizawa Y, Oguma S, Yamauchi K. J Appl Phys, 1988; 64: 6044

[5] Wu H Z, Liu Y H, Zhang L, Xiao S Q, Dai Y Y. Acta Metall Sin, 2000; 36: 997

(吴厚政, 刘宜华, 张 林, 萧淑琴, 代由勇. 金属学报, 2000; 36: 997)

[6] Jiang H G, Tong H Y, Ding B Z, Hu Z Q, Song Q H, Dong L, Zhou Q. Acta Metall Sin, 1993; 29: B515

(姜洪刚, 佟华宇, 丁炳哲, 胡壮麒, 宋启洪, 董林, 周强. 金属学报, 1993; 29: B515)

[7] Chen W P, Xiao S Q, Wang W J, Liu Y H. Acta Metall Sin, 2004; 40: 1295

(陈卫平, 萧淑琴, 王文静, 刘宜华. 金属学报, 2004; 40: 1295)

[8] Inoue A. Acta Mater, 2000; 48: 279

[9] Xu M, Sun Y, Quan M X, Wang Y D, Zuo L. Acta Metall Sin, 2007; 43: 699

(徐民, 孙 羽, 全明秀, 王沿东, 左良. 金属学报, 2007; 43: 699)

[10] Shen B L, Inoue A, Chang C T. Appl Phys Lett, 2004; 85: 4911

[11] Wang Z C, Gong F F, Yang X L, Zeng L, Chen G, Yang J X, Qian S M, Yang D P. J Appl Phys, 2000; 87: 4819

[12] Herzer G. J Magn Magn Mater, 1992; 112: 258

[13] Yoshizawa Y, Oguma S, Yamauchi K. J Appl Phys, 1988; 64: 6044

[14] Yoshizawa Y, Yamauchi K. IEEE Trans Magn, 1989; 25: 3324

[15] Kraus L, Zaveta K, Heczko O, Duhaj P, Vlasak G, Schnaider T. J Magn Magn Mater, 1992; 112: 275

[16] Herzer G. IEEE Trans Magn, 1994; 30: 4800

[17] Fang Y Z, Zheng J J, Wu F M, Xu Q M, Ye H Q, Zhang J Q, Zheng J L, Li T Y. Appl Phys Lett, 2010; 96: 092508–1 [18] Yang J X, Yang X L, Chen G. Chin Sci Bull, 1998; 43: 1051

(杨介信, 杨燮龙, 陈国. 科学通报, 1998; 43: 1051)

[19] Phan M H, Peng H X. Prog Mater Sci, 2008; 53: 323
Outlines

/

〈 〉