论文

HYDROGEN ABSORPTION BEHAVIOR OF 1500 MPa--GRADE HIGH STRENGTH STEEL 42CrMoVNb

  • LI Yang ,
  • ZHANG Yong-Jian ,
  • HUI Wei-Jun ,
  • YU Mao-Qiu ,
  • DONG Han
Expand
  • National Engineering Research Center of Advanced Steel Technology, Central Iron and Steel Research Institute, Beijing 100081

Received date: 2010-10-11

  Revised date: 2010-11-15

  Online published: 2011-04-11

Supported by

Supported by National High Technology Research and Development Program of China (No.2009AA033401) and National Key Technology R&D Program of China (No.2007BAE51B03)

Abstract

Hydrogen absorption behaviors of a newly developed 1500 MPa-grade high strength steel 42CrMoVNb at different austenitizing temperatures and tempering temperatures were studied using cathodic charging and hydrogen thermal desorption analysis, which were also compared with commercial structural steel 42CrMo. The results show that the hydrogen escape peak temperatures (θp) in hydrogen evolution curves of hydrogen charged 42CrMoVNb specimens are between 200 ℃ to 300 ℃ both at as-quenched condition and as-tempered condition. The absorbed hydrogen content of 42CrMoVNb specimen increases slowly with increasing tempering temperature up to 500 ℃. When the tempering temperature exceeded 500 ℃, the absorbed hydrogen content increases sharply and reaches its peak, 6.6×10-6, for the specimen tempered at 600 ℃, which is 5 times as much as that of the as-quenched specimen. Thereafter the absorbed hydrogen content declines sharply as the tempering temperature was gone up sequentially. When the specimen was tempered at 400 ℃, the absorbed hydrogen content decreases slightly with austenitizing temperature increasing, and in the microstructure no fine dispersed (V, X)C carbide precipitated, while when the specimen was tempered at 600 ℃, the absorbed hydrogen content increases sharply with austenitizing temperature increasing, and more fine dispersed (V, X)C precipitated. These results indicate that fine dispersed (V, X)C precipitate could  be regarded as a strong hydrogen trap, and the trap activation energy, Ea, is equal to about\linebreak 28.7 kJ/mol, which was obtained by change heating rate.

Cite this article

LI Yang , ZHANG Yong-Jian , HUI Wei-Jun , YU Mao-Qiu , DONG Han . HYDROGEN ABSORPTION BEHAVIOR OF 1500 MPa--GRADE HIGH STRENGTH STEEL 42CrMoVNb[J]. Acta Metall Sin, 2011 , 47(4) : 423 -428 . DOI: 10.3724/SP.J.1037.2010.00537

References

[1] Chu W Y. Hydrogen Damage and Delayed fracture. Beijing: Metallurgy Industry Press, 1988: 86 p

(褚武扬. 氢损伤与滞后断裂. 北京: 冶金工业出版社, 1988: 86)

[2] Shinsaku M. Delayed Fracture. Tokyo: Nikkan Kogyo Shimbun, 1989: 192

(松山晋作. 迟れ破坏. 东京: 日刊工业新闻社, 1989: 192)

[3] Hui W J, Dong H, Weng Y Q. Iron Steel, 2001; 36(3): 69

(惠卫军, 董 瀚, 翁宇庆. 钢铁, 2001; 36(3): 69)

[4] Hasegawa T, Nakahara T, Yamada Y, Nakamura M. Wire J Int, 1992; (8): 49

[5] Kushida T, Matsumoto H, Kuratomi N, Tsumura T, Nakasato F, Kudo T. Tetsu Hagane, 1996; 82: 297

(栉田隆弘, 松本 \ 齐, 仓富直行, 津村辉隆, 中里福和, 工\parbox[t]{0.26cm}{\vspace*{-6.2pt}\hspace*{-1.2pt}

\includegraphics[width=0.23cm]{teng.eps}}\hspace*{0.2pt}赳夫. 铁と钢, 1996; 82: 297)

[6] Takehiro T, Toru H, Kaneaki T. Tetsu Hagane, 2002; 88: 771

(土田武広, 原彻, 津崎蒹彰. 铁と钢, 2002; 88: 771)

[7] Hui W J, Dong H, Weng Y Q. J Iron Steel Res Int, 2003; 10(4): 63

[8] Hui W J, Dong H, Weng Y Q, Shi J. J Iron Steel Res Int, 2005; 12: 43

[9] Hui W J, Dong H, Weng Y Q, Chen S L, Wang M Q. J Iron Steel Res Int, 2002; 9: 40

[10] Qi J Y, Li Y J, Zhou H J. Trans Mater Heat Treat, 1984; (1): 4

(齐靖远, 黎永均, 周惠久. 材料热处理学报, 1984; (1): 4)

[11] Hui W J, Dong H, Weng Y Q, Shi J, Zhang X Z. Acta Metall Sin, 2004; 40: 1274

(惠卫军, 董瀚, 翁宇庆, 时捷, 章晓中. 金属学报, 2004; 40: 1274)

[12] Li G F, Wu R G, Lei T C. Metall Trans, 1992; 23A: 2879

[13] Hui W J, Weng Y Q, Dong H. High Strength Steels for Fasteners. Beijing: Metallurgical Industry Press, 2009: 124

(惠卫军, 翁宇庆, 董瀚. 高强度紧固件用钢. 北京: 冶金工业出版社, 2009: 124)

[14] Llewellyn D T. Ironmak Steelmak, 1996; 23: 397

[15] Yao D Q, Hu Z Q, Shi C X. Mater Mech Eng, 1989; (1): 1

(姚大千, 胡壮麒, 师昌绪. 机械工程材料, 1989; (1): 1)

[16] Choo W Y, Lee J Y. Metall Trans, 1982; 13A: 135

[17] Choo W Y, Lee J Y. J Mater Sci, 1982; 17: 1930
Outlines

/

〈 〉