论文

STUDY OF Mn AND P SOLUTE DISTRIBUTIONS AND THEIR EFFECT ON THE TENSILE BEHAVIOR IN ULTRA LOW CARBON BAKE HARDENING STEELS

  • YU Hua ,
  • SHI Wen ,
  • HE Yan-Lin ,
  • LI Lin
Expand
  • College of Materials Science and Engineering, Shanghai University, Shanghai 200072

Received date: 2010-12-23

  Revised date: 2011-01-21

  Online published: 2011-03-11

Supported by

Supported by National Nature Science Foundation of China (Nos.50934011 and 50971137) and National Basic Research Program of China (No.2010CB630802)

Abstract

With the increasing requirement of vehicle weight reduction and energy conservation from automobile industry, the investigation and development of high strength steel sheet has been stressed extensively. Bake hardening steel, as a new kind of automotive steel, exhibits low strength and good formability  before drawing, after which increases obviously in the yield strength during baking process, and is then widely used in the outer plate of modern cars. Mn and P are often added to sheet steel to increase the strength, and their distributions have significant effect on drawability, bake hardening property and surface quality of bake hardening steels. In this paper, the distributions of Mn and P and their effect on tensile behavior in bake hardening steels were studied. For investigation, two kinds of bake hardening steels (BH–Mn and BH–P steels) were heated to 800  ℃, held for 2 min and cooled by water quenching. Three dimensional atom probe (3DAP) technique, internal friction experiments and tensile tests were carried out to analysis the effect of Mn and P distribution patterns on the interstitial atom distribution and Cottrell atmosphere in the matrix, so as to obtain the influence of solute istributions on tensile behavior. The results indicate that P segregates mainly in bake hardening steel, and part of P segregates together with C, which strongly pin the dislocations and is the main reason that induces the yield point elongation during tensile process. In BH–Mn steel, Mn hardly segregates in the matrix and C segregates very little, so the strength of BH–Mn steel is lower than that of BH–P steel, whereas the plasticity is better than BH–P steel. The segregation of P together with C and its pinning of dislocations will influence Snoek–Ke–Koster internal friction, and mkes the disappearance of Snoek–Ke–Koster peak.

Cite this article

YU Hua , SHI Wen , HE Yan-Lin , LI Lin . STUDY OF Mn AND P SOLUTE DISTRIBUTIONS AND THEIR EFFECT ON THE TENSILE BEHAVIOR IN ULTRA LOW CARBON BAKE HARDENING STEELS[J]. Acta Metall Sin, 2011 , 47(3) : 263 -268 . DOI: 10.3724/SP.J.1037.2010.00693

References

[1] Jeong Y S, Matsubae–Yokoyama K, Kubo H, Pak J J, Nagasaka T. Resour, Cnserv Recyclig, 2009; 53: 479

[2] Zhang J X, Xiong X M. Acta Metall Sin, 2003; 39: 1127

(张进修, 熊小敏. 金属学报, 2003; 39: 1127)

[3] Waleed Al S, John G S, Kip F, David K M. Metall Mater Trans, 2006; 37A: 206

[4] Ruiz D, Rivera–Tovar J L, Segers D, Vandenberghe R E, Houbaert Y. Mater Sci Eng, 2006; A442: 462

[5] Ji J W, Zhao Z Q, He L D, Geng D Q. Acta Phys Sin, 1985; 34: 1620

(戢景文, 赵赠祺, 贺礼端, 耿殿奇. 物理学报, 1985; 34: 1620)

[6] Zhang Z, Lin Q, Yu Z. Mater Sci Eng, 2000; A291: 22

[7] Wu J, Song S H, Weng L Q, Xi T H, Yuan Z X. Mater Charact, 2008; 59: 261

[8] Wang K,Wang M, i H, Xu T. Mater Sci ng, 2008; A485: 347

[9] Smith J F, Southworth H N. Surf Technol, 1984; 21: 205

[10] Perhacova J, Grman D, Svoboda M, Patscheider J, Vyrostkova A, Janovc J. Mater Lett, 2001; 47: 44

[11] Pereloma E V, Timokhina I B, Miller M K, Hodgson P D. Acta Mater, 2007; 55: 2587

[12] Liu Q D, Chu Y L, Wang Z M, Liu W Q, Zhou B X. Acta Metall Sin, 2008; 44: 1281

(刘庆冬, 褚于良, 王泽民, 刘文庆, 周邦新. 金属学报, 2008; 44: 1281)

[13] Zheng L, Xu T D, Deng Q, Si H. Acta Metall Sin, 2007; 43: 893

(郑磊, 徐庭栋, 邓群, 司红. 金属学报, 2007; 43: 893)

[14] Miller M K. Science, 1999; 286: 2285

[15] Craven A J, MacKenzie M, Cerezo A, Godfrey T, Clifton P H. Mater Sci Technol, 2008; 24: 641

[16] M´athis K, Rauch E F. Mater Sci Eng, 2007; A462: 248

[17] Liu Q D, Liu W Q, Wang Z M, Zhou B X. Acta Metall Sin, 2008; 44: 786

(刘庆冬, 刘文庆, 王泽民, 周邦新. 金属学报, 2008; 44: 786)

[18] Wert C, Marx I. Acta Metall, 1953; 1: 113

[19] Weller M. Mater Sci Eng, 2006; A442: 21

[20] Juan J S. In: Schaller R, Fantozzi T, Gremaud G eds., Mechanical Spectroscopy Q−1 2001, Uetikon–Zuerich, Switzerland: Trans Tech Publications Ltd, 2001: 32

[21] Bagramov R, Mari D, Benoit W. Philos Mag, 2001; 81A: 2797

[22] Tkalcec I, Mari D. Defect Diffus Forum, 2002; 203–205: 253

[23] Song X L, Yuan Z X, Jia J, Wang D, Fan L X. Scr Mater, 2010; 63: 446

[24] Zhao J Z, De A K, De Cooman B C. Mater Lett, 2000; 44: 374

[25] Cottrell A H, Bilby B A. Proc Phys Soc, 1949; 62A: 49

[26] Cowan J R, Evans H E, Jones R B, Bowen P. Acta Mater, 1998; 46: 6565

[27] Song S H, Wu J, Weng L Q, Yuan Z X. Mater Sci Eng, 2008; A497: 524
Outlines

/

〈 〉