论文

MATHEMATICAL MODEL AND THEORETICAL RESEARCH OF UNIT ROLLING PRESSURE DISTRIBUTION IN RECTANGULAR GROOVE DURING RHEO–ROLLING OF SEMISOLID ALLOY

  • HUANG Hong-Qian ,
  • CAO Fu-Rong ,
  • GUAN Ren-Guo ,
  • DIAO Tie-Yong ,
  • GENG Zhen-Huan
Expand
  • College of Materials and Metallurgy, Northeastern University, Shenyang 110819

Received date: 2010-11-04

  Revised date: 2010-12-13

  Online published: 2011-03-11

Supported by

Supported by National Natural Science Foundation of China (Nos.51034002 and 50974038) and Key China University Basic Scientific Research Expenses (No.090502003)

Abstract

Semisolid metal forming (SSF) is recognized as a new forming technology, which has been paid more and more attention by the researchers all over the world. The semisolid rolling process (rheo–rolling) combines the fabrication of semisolid slurry with continuously rolling as an important neoteric means to achieve near–shape forming. Compared with the traditional rolling process, this technology has the features of short machining process, low energy consumption, low cost equipment and high yield. However, one of the difficulties of using this technology to produce strip is that the solid and liquid phases prone to separation with each other during rheo–rolling deformation, especially when the semisolid slurry has a low solid fraction. The phenomenon causes macrosegregation and reduces the quality of the strip, as a result, limiting its industrial application. Using rectangular groove roller may solve this problem. In this paper, the mathematical model of unit rolling pressure distribution in rectangular groove during rheo–rolling was established. AZ91D magnesium alloy was taken as an example, and the effects of rolling strip thickness, width and roller radius on unit pressure were calculated and studied. he calculation results reveal that the smaller the thickness of rheo–rolled strip is, the narrower the width is, the bigger the peak unit rolling pressure is and the larger the average unit rolling pressure is. However, when the strip thickness decreases, the peak unit rolling pressure moves towards the exit while when width decreases, the peak unit rolling pressure moves towards the entrance. The larger the roller radius is, the bigger the peak unit rolling pressure is, the larger the average unit olling pressure is, and the peak value deviates towards the exit.

Cite this article

HUANG Hong-Qian , CAO Fu-Rong , GUAN Ren-Guo , DIAO Tie-Yong , GENG Zhen-Huan . MATHEMATICAL MODEL AND THEORETICAL RESEARCH OF UNIT ROLLING PRESSURE DISTRIBUTION IN RECTANGULAR GROOVE DURING RHEO–ROLLING OF SEMISOLID ALLOY[J]. Acta Metall Sin, 2011 , 47(3) : 291 -297 . DOI: 10.3724/SP.J.1037.2010.00590

References

[1] Luo S J, TianWT, Xie S S, MaoWM. Chin J Nonferrous Met, 2000; 10: 765

(罗守靖, 田文彤, 谢水生, 毛卫民. 中国有色金属学报, 2000; 10: 765)

[2] Song R B, Kang Y , Zhao A M. J Mater Process Technol, 2008; 198: 291

[3] Haga T. J Mater Process Technol, 2002; 130: 558

[4] Haga T, Kenta T, Masaaki I. J Mater Process Technol, 2004; 153: 42

[5] Haga T, Suzuki S. J Mater Process Technol, 2004; 157–158: 695

[6] Guan R G. Theory and Technology of Metallic Semisolid Forming. Beijing: Metallurgical Industrial Press, 2005: 14

(管仁国. 金属半固态成形理论与技术. 北京: 冶金工业出版社, 2005: 14)

[7] Ji Z S, Yan H H, Zheng X P, Sugiyama S O, Yanagimoto J. J Mater Process Technol, 2008; 202: 412

[8] Kang C G, Yoon J H. J Mater Process Technol, 1997; 66: 76

[9] Xie S S, Yang H Q, Huang G J, Li L. J Plast Eng, 2007; 14: 80

(谢水生, 杨浩强, 黄国杰, 李雷. 塑性工程学报, 2007; 14: 80)

[10] Kang C G, Kim Y D. J Mater Process Technol, 1997; 67: 71

[11] Zhu Z H, Xiao W F, LI X Q, Hu S C. Chin J Mech Eng, 2002; 38(7): 153

(朱志华, 肖文峰, 李晓谦, 胡仕成. 机械工程学报, 2002; 38(7): 153)

[12] Zhao D W. Mechanics of Materials Forming. Shenyang: Northeastern University Press, 2002: 115

(赵德文. 材料成形力学. 沈阳: 东北大学出版社, 2002: 115)

[13] Wei L . Principle of Metal Forming. Beijing: Metallurgical Industrial Press, 2008: 55

(魏立群. 金属压力加工原理. 冶金工业出版社, 2008: 55)

[14] Yan H, Xia J C, Wang G C, Hu G A, Li H J. Mater Rev, 2002; 16(11): 8

(闫洪, 夏巨谌, 王高潮, 胡国安, 李海江. 材料导报, 2002; 16(11): 8)

[15] Pan H P, Ding Z Y, Dong Y S, Xie S X. Acta Metall Sin, 2003; 39: 369

(潘洪平,丁志勇, 董原生, 谢水生. 金属学报, 2003; 39: 369)

[16] Xing Z H. Master Dessertation, Northeastern University, Shenyang, 2007

(邢振环. 东北大学硕士论文, 沈阳, 2007)

[17] Seheil E. Z Metallkd, 1942; 34: 70
Outlines

/

〈 〉