MAGNETOCALORIC EFFECT IN MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03) COMPOUNDS

  • YU Dong-Mei ,
  • SONG Lin ,
  • YU Yao-Hui ,
  • ZHANG Wei ,
  • BI Li-He
Expand
  • Inner Mongolia Key Laboratory for Physics and Chemistry of Functional Materials, Inner Mongolia Normal University,
    Hohhot 010022

Received date: 2010-10-25

  Revised date: 2010-11-22

  Online published: 2011-03-11

Supported by

Supported by National Natural Science Foundation of China (No.50961010), National Natural Science Foundation of Inner Mongolia (No.20080404ZD09) and Graduate Student Foundation of Inner Mongolia Normal University (No.CXJJS10034)

Abstract

Structural and magnetocaloric properties of the MnFeP0.63Ge0.12Si0.25Bx (x=0,0.01, 0.02, 0.03, atomic fraction) compounds have been inestigated. XRD result shows that the MnFeP0.63Ge0.12Si0.25Bx  (x=0, 0.01, 0.02, 0.03) compounds mainly consist of the Fe2P–typhxagonal structure phase with space group P¯62m. It is fond that the lattice paraeter a increases and the lattice parameter c slighly decreases with increasing x, and the unit celvolume does not change. The agnetic measurements show that the Curie temperature increases from 300 K to 347 K, and thermal hysteresis are 20, 17, 11 and 6 K for x= 0 to 0.03. The aximm values of the magnetic entropy chage are 11.1, 11.26 and 11.8 J/(kg·K), respectively, or 0—1.5 T fields.

Cite this article

YU Dong-Mei , SONG Lin , YU Yao-Hui , ZHANG Wei , BI Li-He . MAGNETOCALORIC EFFECT IN MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03) COMPOUNDS[J]. Acta Metall Sin, 2011 , 47(3) : 344 -348 . DOI: 10.3724/SP.J.1037.2010.00566

References

[1] Tegus O, Br¨uck E, Buschow K H J, de Boer F R. Nature,2002; 415: 150

[2] Yan A, M¨uller K H, Schultz L, Gutfleisch O. J Appl Phys, 2006; 99: 08K903

[3] DagulaW, Tegus O, Li XW, Song L, Br¨uck E, Cam Thanh D T, de Boer F R, Buschow K H J. J Appl Phys, 2006; 99: 08Q105

[4] Br¨uck E, Tegus O, Zhang L, Li XW, de Boer F R, Buschow K H J. J Alloys Compds, 2004; 383: 32

[5] Br¨uck E, Tegus O, Li X W, de Boer F R, Buschow K H J. Physica, 2003; 327: 431

[6] Tegus O, Fuquan B, Dagula W, Zhang L, Br¨uck E, Si P Z, de Boer F R, Buschow K H J. J Alloys Compds, 2005; 396: 6

[7] Cam Thanh D T, Br¨uck E, Tegus O, Klaasse J C P, Gortenmulder T J, Buschow K H J. J Appl Phys, 2006; 99: 08Q107

[8] Br¨uck E, Ilynb M, Tishin A M, Tegus O. J Magn Magn Mater, 2005; 290–291: 8

[9] Tegus O, Br¨uck E, Dagula W, Li X W, Zhang L, Buschow K H J, de Boer F R. J Appl Phys, 2003; 93: 7655

[10] Tegus O, Br¨uck E, Li X W, Zhang L, DagulaW, de Boer F R, Buschow K H J. J Magn Magn Mater, 2004; 272–276: 2389

[11] Zhang L, Moze O, Prokes K, Tegus O, Br¨uck E. J Magn Magn Mater, 2005; 290–291: 679

[12] Ou Z Q, Wang G F, Song L, Tegus O, Br¨uck E, Buschow K J. J Phys: Condens Matter, 2006; 18: 11577

[13] Yan A, M¨uller K H, Schultz L, Gutfleisch O. J Appl Phys, 2006; 99: 08K903

[14] Wang G F. Master Desertation, Inner Mongolia Normal University, hohhot, 2007

(王高峰. 内蒙古师范大学硕士学位论文, 呼和浩特, 2007)

[15] Zhang L. PhD Thesis, University of Amsterdam, 2005

[16] Hang J H, Song L, Jin P Y, Wang G F, Liu J R, Yan H W, Zhang J X. J Funct Mater, 2006; 37: 1888

(黄焦宏, 松林, 金培育, 王高峰, 刘金荣, 闫宏伟, 张久兴. 功能材料, 2006; 37: 1888)

[17] Li F A, Song L, Bao L H, Ha S C L, Tegus O, Hang J H. Acta Metall Sin, 2008; 44: 371

(李福安, 松林, 包黎红, 哈斯朝鲁, 特古斯, 黄焦宏. 金属学报, 2008; 44: 371)

[18] Li F A, Song L, Wang G F, Xie G Q, Zheng L, Hang J H, Tegus O. J Funct Mater, 2010; 41: 515

(李福安, 松林, 王高峰, 谢国秋, 郑立, 黄焦宏, 特古斯. 功能材料, 2010; 41: 515)

[19] Li F A, Song L, Zheng L, Hang J H, Tegus O. Met Funct Mater, 2010; 17: 22

(李福安, 松林, 郑立, 黄焦宏, 特古斯. 金属功能材料, 2010; 17: 22)

[20] Beckman O, Lundgren L, Buschow K H J. Handbook of Magnetic Materials. Amsterdam: Elsevier Science Publication, 1991: 186

[21] Gschneidner Jr K A, Pecharsky V K. Annu Rev Mater Sci, 2000; 30: 387
Outlines

/

〈 〉