论文

CONVECTION EFFECTS AND BANDING STRUCTURE FORMATION MECHANISM DURING DIRECTIONAL SOLIDIFICATION OF PERITECTIC ALLOYS
I. Experimental Result

  • LUO Liang-Shun ,
  • ZHANG Yu-Min ,
  • SU Pan-Qiang ,
  • YU Xin ,
  • GUO Jing-Jie ,
  • FU Heng-Zhi
Expand
  • 1. School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001
    2. National Key Laboratory of Science and Technology on Advanced Composites in Special Environment, Harbin Institute
    of Technology, Harbin 150001

Received date: 2010-09-19

  Revised date: 2010-11-25

  Online published: 2011-03-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50901025 and 50771041) and National Science Foundation for Post–doctoral Scientists of China (No.20090450840)

Abstract

Systematic directional solidification experiments were conducted to investigate the convection effects on the banding structure evolution and macrosegregation in nonfaceted–non–faceted model Fe–Ni alloy using conventional resistance heating and induction heating Bridgman directional solidification methods in this paper. It was found that convection can induce severe axial and radial macrosegregation in the directionally solidified samples, and make the microstructures complex and mae the steady state difficult to achieve. Axiamacrosegregation was reflectein finite samples olidified from the beginning to the enof soidification with the transiion from primary phase to peritectic phase. The primary–peritectic transition depended on the alloy composition and convection strengh. Radial macrosegregation reflected in the solute concentration poor in the center and rich in edge, and a primary–peritectic transition also exist in the lateral directional from the sample to the edge.

Cite this article

LUO Liang-Shun , ZHANG Yu-Min , SU Pan-Qiang , YU Xin , GUO Jing-Jie , FU Heng-Zhi . CONVECTION EFFECTS AND BANDING STRUCTURE FORMATION MECHANISM DURING DIRECTIONAL SOLIDIFICATION OF PERITECTIC ALLOYS
I. Experimental Result[J]. Acta Metall Sin, 2011
, 47(3) : 275 -283 . DOI: 10.3724/SP.J.1037.2010.00485

References

[1] Kerr H W, Kurz W. Int Mater Rev, 1996; 41: 129

[2] Johnson D R, Inui H, Yamaguchi M. Acta Mater, 1996;44: 2523

[3] Lapin J, Klimova A, Velisek R, Kursa M. Scr Mater, 1997; 37: 85

[4] Zhong H, Li S M, Lu H Y, Liu L, Zou G R, Fu H Z. J Cryst Growth, 2008; 310: 3366

[5] Li S M, Ma B L, L¨u H Y, Liu L, Fu H Z. Acta Metall Sin, 2005; 41: 411

(李双明, 马伯乐, 吕海燕, 刘林, 傅恒志. 金属学报, 2005; 41: 411)

[6] Nagashio K, Takamura Y, Kuribayashi K. Scr Mater, 1999; 41: 1161

[7] Liu Y C. PhD Thesis, Northwestern Polytechnical University, Xi’an, 2000

(刘永长. 西北工业大学博士学位论文, 西安, 2000)

[8] Wang M. PhD Thesis, Northwestern Polytechnical University, Xi’an, 2002

(王猛. 西北工业大学博士学位论文, 西安, 2002)

[9] Fu H Z, Su Y Q, Guo J J, Xu D M. Acta Metall Sin, 2002; 38: 9

(傅恒志, 苏彦庆, 郭景杰, 徐达鸣. 金属学报, 2002; 38: 9)

[10] Dobler S, Lo T S, Plapp M, Karma A, Kurz W. Acta Mater, 2004; 52: 2795

[11] Su Y Q, Luo L S, Li X Z, Guo J J, Yang H M, Fu H Z. Appl Phys Lett, 2006; 89: 031918

[12] Trivedi R. Metall Trans, 1995; 26A: 1583

[13] Liu S, Trivedi R. Metall Trans, 2006; 37A: 3293

[14] Trivedi R, Shin J H. Mater Sci Eng, 2005; A413: 288

[15] Li X Z, Guo J J, Su Y Q, Wu S P, Fu H Z. Acta Metall Sin, 2005; 41: 593

(李新中, 郭景杰, 苏彦庆, 吴士平, 傅恒志. 金属学报, 2005; 41: 593)

[16] Guo J J, Li X Z, Su Y Q, Wu S P, Fu H Z. Acta Metall Sin, 2005; 41: 599

(郭景杰, 李新中, 苏彦庆, 吴士平, 傅恒志. 金属学报, 2005; 41: 599)

[17] Li S M, Liu L, Li X L, Fu H Z. Acta Metall Sin, 2004; 40: 20

(李双明, 刘林, 李晓历, 傅恒志.金属学报, 2004; 40: 20)

[18] Luo L S. PhD Thesis, Harbin Institute of Technology, 2008

(骆良顺. 哈尔滨工业大学博士学位论文, 2008)

[19] Karma A, Rappel W J, Fuh B C, Trivedi R. Metall Trans, 1998; 29A: 1457

[20] Luo L S, Su Y Q, Guo J J, Li X Z, Yang H M, Fu H Z. Appl Phys Lett, 2008; 92: 061903

[21] Xu X. Master Dissertation, Northwestern Polytechnical University, Xi’an, 2005

(许雄. 西北工业大学硕士学位论文, 西安, 2005)
Outlines

/

〈 〉