论文

A SIMPLE VECTOR ANALYSIS METHOD FOR MARTENSITE CRYSTALLOGRAPHY

  • GU Xin-Fu ,
  • ZHANG Wen-Zheng
Expand
  • Laboratory of Advanced Materials, Department of Materials Science and Engineering, Tsinghua University, Beijing 100084

Received date: 2010-10-26

  Revised date: 2010-11-23

  Online published: 2011-02-11

Supported by

Supported by National Natural Science Foundation of China (No.50971076)

Abstract

The displacements of vectors in a habit plane (HP) are assumed to lie along a particular Burgers vector, so that the misfit in the interface can be fully accommodated by a set of dislocations with that Burgers vector. This assumption is consistent with many models and experimental observations. Based on this assumption, a simple method based on vector analysis has been developed. By applying this method to fcc/bcc system, the classical solutions from the phenomenal theory of martensite crystallography can be reproduced. In addition, a simple form of equation for general HP orientations satisfying the above assumption has also been derived. The present method provides a simple but general tool for analysis of irrational HP generated from either martensitic or diffusional transformations.

Cite this article

GU Xin-Fu , ZHANG Wen-Zheng . A SIMPLE VECTOR ANALYSIS METHOD FOR MARTENSITE CRYSTALLOGRAPHY[J]. Acta Metall Sin, 2011 , 47(2) : 241 -245 . DOI: 10.3724/SP.J.1037.2010.00571

References

[1] Bowles J S, MacKenzie J K. Acta Metall, 1954; 2: 129

[2] Mackenzie J K, Bowles J S. Acta Metall, 1954; 2: 138

[3] Bowles J S, MacKenzie J K. Acta Metall, 1954; 2: 224

[4] Wechsler M, Lieberman D, Read T. Trans AIME, 1953; 179: 1503

[5] Wayman C M. Introduction to the Crystallography of Martensitic Transformations. New York: MacMillan, 1964: 111

[6] Tsu T Y. Martensitic Transformation and Martensites. Beijing: Science Press, 1981: 376

(徐祖耀. 马氏体相变与马氏体. 北京: 科学出版社, 1981: 376)

[7] Nishiyama Z. Martensitic Transformation. New York: Academic Press, 1978: 337

[8] Suzuki H. Sci Rep Res Inst Tohoku Univ, 1954; 6A: 30

[9] Kajiwara S. Trans Jpn Inst Met, 1976; 17: 435

[10] Kato H. Scr Mater, 1998; 38: 1125

[11] Frank F C. Acta Metall, 1953; 1: 15

[12] Bilby B A, Frank F C. Acta Metall, 1960; 8: 239

[13] Pond R C, Celotto S, Hirth J P. Acta Mater, 2003; 51: 5385

[14] Pond R C, Ma X, Chai Y W, Hirth J P. In: Nabarro F R N, Hirth J P, eds., Dislocations in Solids, Amsterdam: Elsevier, 2007: 225

[15] Gu X F, Zhang W Z. Philos Mag, 2010; 90: 3281

[16] Zhang W Z, Purdy G R. Philos Mag, 1993; 68: 291

[17] Zhang W Z, Purdy G R. Acta Metall Mater, 1993; 41: 543

[18] Ye F, Zhang W Z, Qiu D. Acta Mater, 2004; 52: 2449

[19] Qiu D, Zhang W Z. Acta Mater, 2007; 55: 6754

[20] Bhadeshia H K D H. Worked Examples in the Geometry of Crystals. London: Institute of Materials, 2001: 68

[21] Zhang W Z. Philos Mag, 1998; 78: 913

[22] Gu X F, Zhang W Z. Philos Mag, 2010; 90: 450
Outlines

/

〈 〉