论文

EXPERIMENTAL RESEARCH ON MAGNETIC PULSE JOINING OF 3A21 ALUMINUM ALLOY-20 STEEL TUBES

  • XU Zhi-Dan ,
  • LI Chun-Feng ,
  • DIAO Zhi-Hua
Expand
  • 1) School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001
    2) State Key Laboratory of Advanced Welding Production Technology, Harbin Institute of Technology, Harbin 150001

Received date: 2010-09-25

  Revised date: 2010-11-15

  Online published: 2011-02-11

Supported by

Supported by Funds of State Key Lab of Advanced Welding Production Technology, Harbin Institute of Technology (AWPT-M05) and China Postdoctoral Science Foundation (Nos.20080440127 and 200902382)

Abstract

Magnetic pulse joining (MPJ) is a solid state joining technology, by which mechanical or metallurgical joint is obtained. It can be used to assemble and join dissimilar metals. In this work, by means of MPJ setup with low inductance coil, the effects of discharge voltage, radial gap between tubes and lap length on the tensile and peel testing strength of 3A21 aluminum alloy-20 steel tubes joint were investigated experimentally. The microstructural observation and the energy spectrum analysis (by linear scan) of basic elements distribution within the MPJ joint interface were performed by SEM. The results showed that an increasing discharge voltage contributed to the change of MPJ joint from mechanical joint to metallurgical one. The metallurgical joint with the small wave joining interface was obtained under a voltage of 5.5 kV, a radial gap of 1.5 mm, and a lap length of 3/4 coil length, where the mutual diffusion of Al and Fe elements occurred. The severe plastic deformation with sharp strain gradient, and the distinct grain refinement occurred in the matrix metals near the joining interface.

Cite this article

XU Zhi-Dan , LI Chun-Feng , DIAO Zhi-Hua . EXPERIMENTAL RESEARCH ON MAGNETIC PULSE JOINING OF 3A21 ALUMINUM ALLOY-20 STEEL TUBES[J]. Acta Metall Sin, 2011 , 47(2) : 197 -202 . DOI: 10.3724/SP.J.1037.2010.00501

References

[1] Yu H P, Xu D G, Li C F. Forg Stamp Technol, 2009; 34(2): 1

(于海平, 徐殿国, 李春峰. 锻压技术, 2009; 34(2): 1)

[2] Benedyk J C. Light Met Age, 2001; 59: 48

[3] Sun M R. Weld Technol, 1999; 6: 13

(孙明如. 焊接技术, 1999; 6: 13)

[4] Kochan A. Assemb Auto, 2000; 20: 129

[5] Anthony L, Velocci J. Aviat Week Space Technol, 1993; 139: 59

[6] Uhlmann E, Hahn R, Jurgasch D. Steel Res Int, 2005; 76: 245

[7] Marya M, Priem D, Marya S. Mater Sci Forum, 2003; 426–432: 4001

[8] Kimchi M, Shao H, Cheng W, Krishnaswamy P. Weld World, 2004; 48: 19

[9] Shribman V, Stern A, Livs Y, Gafri O. Weld J, 2002; 4: 33

[10] Marya M, Marya S. Sci Technol Weld Join, 2004; 9: 541

[11] Stern A, Aizenshtein M. Sci Technol Weld Join, 2002; 7: 339

[12] Aizawa T, Kashani M, Okagawa K. Weld World, 2005; 49: 212

[13] Ben–Artzy A, Stern A, Frage N, Shribman V, Sadot O. Int J Impact Eng, 2010; 37: 307

[14] Watanabe M, Kumai S, Hagimoto G, Zhang Q S, Nakayama K. Mater Trans, 2009; 50: 279

[15] Kore S D, Date P P, Kulkarni S V. Int J Impact Eng, 2007; 34: 1327

[16] Ben–Artzy A, Stern A, Frage N. Sci Technol Weld Join, 2008; 13: 402

[17] Wang Y H. Research and Practice of Explosive Welding of Metal Plates. Beijing: National Defense Industry Press, 2007: 31

(王耀华. 金属板材爆炸焊接研究与实践. 北京: 国防工业出版社, 2007: 31)
Outlines

/

〈 〉