MICROSTRUCTURES AND MECHANICAL PROPERTIES OF BANDED TEXTURES OF FRICTION STIR WELDED 7075-T6 ALUMINUM ALLOY

  • LUAN Guo-Hong ,
  • KANG Ju ,
  • FU Rui-Dong
Expand
  • 1) Beijing Aeronautical Manufacturing Technology Research Institute, China Friction Stir Welding Center, Beijing 100024
    2) Yanshan University, College of Materials Science and Engineering, Qinhuangdao 066004

Received date: 2010-08-10

  Revised date: 2010-10-07

  Online published: 2011-02-11

Supported by

Supported by National Key Technology Research and Development Program (No.2006BAF04B09) and Aviation Science Key Foundation (No.2009ZE25007)

Abstract

Friction stir welding (FSW) is a ideal method for joining light metal materials, especially for AA2000 and AA7000 series aluminum alloys. In the welding field, many aspects of FSW have been studied quite extensively and comprehensively. However, the origin of the banded texture is still a subject of current research. One of the phenomena that strike researchers today is the occurrence of banded texture on the top surface in FSW joints. Furthermore, many waves also emerged in shoulder affected zone (SAZ) after a joint being polished and etched. The correlation between the banded textures and the waves is not clear. In this paper, 1.6 mm thick 7075-T6 aluminum alloy sheets were friction stir welded, microstructures and hardness profile of banded textures on the top surface of the joint were investigated. The results of metallographic observation showed that alternately light and dark waves presented in SAZ, the light waves coincided with valleys of the banded textures, whereas the dark waves coincided with peaks. SEM and TEM analyses revealed that compared with the valleys, the peaks were characterized by more secondary phase particles and small grains, resulting in higher hardness at the peaks.

Cite this article

LUAN Guo-Hong , KANG Ju , FU Rui-Dong . MICROSTRUCTURES AND MECHANICAL PROPERTIES OF BANDED TEXTURES OF FRICTION STIR WELDED 7075-T6 ALUMINUM ALLOY[J]. Acta Metall Sin, 2011 , 47(2) : 224 -230 . DOI: 10.3724/SP.J.1037.2010.00399

References

[1] Matrukanitz R P. ASM Handbook–Welding, Brazing and Soldering. Ohio, Geauga: ASM Int, 1990: 528

[2] Thomas W M, Nicholas E D, Needham J C, Murch M G, Templesmith P, Dawes C J. Int Pat, PCT/GB92/02203, 1991

[3] Mishra R S, Ma Z Y. Mater Sci Eng, 2005; R50: 1

[4] Cavaliere P, Cerri E, Squillace A. J Mater Sci, 2005; 40: 3669

[5] Lumsden J B, Mahoney M W, Pollock G. Corrosion, 1999; 55: 1127

[6] Kang J, Fu R D, Luan G H, Dong C L, He M. Corros Sci, 2010; 52: 620

[7] Chai P, Luan GH, Guo D L, Li J. Trans China Weld Inst, 2005; 26: 79

(柴 鹏, 栾国红, 郭德伦, 李 菊. 焊接学报, 2005; 26: 79)

[8] Li Y, Murr L E, Mclure J C. Scr Mater, 1999; 40: 1041

[9] Lu S X, Yan J C, Li W G, Yang S Q. Acta Metall Sin (Engl Lett), 2005; 18: 552

[10] Rhodnev C G, Mahonev M V, Bingel W H. Scr Mater, 1997; 37: 69

[11] Krishnan K N. Mater Sci Eng, 2002; A327: 246

[12] Liu H J, Chen Y C, Feng J C. Scr Mater, 2006; 55: 231

[13] Attallah M M, Salem H G. Mater Sci Eng, 2005; A391: 51

[14] Dawes C J. Sheet Metal Ind–Weld Join, 1995; 72: 22

[15] Cui G R, Ma Z Y, Li S X. Scr Mater, 2008; 58: 1082

[16] Wang D Y, Feng J C. Trans China Weld Inst, 2003; 24: 42

(王大勇, 冯吉才. 焊接学报, 2003; 24: 42)

[17] Chen Z W, Cui S. Scr Mater, 2008; 58: 417

[18] Yan J H, Sutton M A, Reynolds A P. Sci Technol Weld Joining, 2007; 12: 72

[19] Jin H, Saimoto S, Ball M, Threadgill P L. Mater Sci Technol, 2001; 17: 1605

[20] Schneider J A, Nunes A C. Metall Mater Trans, 2004; 35B: 777

[21] Yang B S, Yan J H, Michael S A, Reynolds P A. Mater Sci Eng, 2004; A364: 55

[22] Zhu R Z. Metal Corrosion Science. Beijing: China Metallurgical Industry Press, 1989: 97–131

(朱日彰. 金属腐蚀学. 北京: 冶金工业出版社, 1989: 97-131)

[23] Cao G, Kou S. Weld J, 2005; 1: 1
Outlines

/