论文

AN APPROACH TO ESTIMATE ROOM TEMPERATURE CREEP OF STRUCTURAL STEELS

  • ZHE De-Fu ,
  • DIAO Jie ,
  • ZHANG -Jun-Shan
Expand
  • 1) School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024
    2) Department of System Safety, Nagaoka University of Technology, Nagaoka 940-2188, Japan

Received date: 2010-07-12

  Revised date: 2010-09-09

  Online published: 2011-02-11

Supported by

Supported by National Nature Science Foundation of China (No.50271013)

Abstract

Room temperature creep (RTC) behaviors of the as-rolled (AR) and normalized (Nor) X70 pipeline steel as well as the AISI304 stainless steel were investigated. At different stress levels, their RTCs mainly showed the feature of logarithmic creep with continuously falling rate. By comparing RTC with tensile tests, it was found that the loading process of RTC test was the same as the tensile test, and the strain rate at the start of RTC was equal to that at the end of loading process. Based on these results and by combining the constitutive equations of RTC with the Ramberg-Osgood equation, which is generally used to describe the stress-strain relationship in tensile tests, an approach to estimate RTC strain was presented as a function of the applied stress. On applying it to the X70 pipeline steel and AISI304 stainless steel, it was indicated that the estimated results of RTC were well consistent with the experimental data and that all the errors were within a factor of 2.

Cite this article

ZHE De-Fu , DIAO Jie , ZHANG -Jun-Shan . AN APPROACH TO ESTIMATE ROOM TEMPERATURE CREEP OF STRUCTURAL STEELS[J]. Acta Metall Sin, 2011 , 47(2) : 179 -184 . DOI: 10.3724/SP.J.1037.2010.00336

References

[1] Andrade E N Da C. Proc Roy Soc, 1910; A84: 1

[2] Cottrell A H. Philos Mag Lett, 1996; 73(1): 35

[3] Hult J. Creep in Structures. New York: Springer Verlag, 1970: 1

[4] Evans H E. Mechanisms of Creep Fracture. London: Elsevier Applied Science, 1984: 1

[5] Zhang J S. Strength of Materials. Harbin: Harbin Institute of Technology Press, 2004: 129

(张俊善. 材料强度学. 哈尔滨: 哈尔滨工业大学出版社, 2004: 129)

[6] Zhang J S. High Temperature Deformation and Fracture of Materials. Beijing: Science Press, 2007: 1

(张俊善. 材料的高温变形与断裂. 北京: 科学出版社, 2007: 1)

[7] Schoeck G. Mechanical Behaviour of Materials at Elevated Temperature. New York: McGraw–Hill, 1961: 1

[8] Feng D. Metal Physics–Mechanical Properties of Metals. Beijing: Science Press, 1999: 548

(冯端. 金属物理学-第三卷金属力学性质. 北京: 科学出版社, 1999: 548)

[9] Oehlert A, Atrens A. Acta Metall Mater, 1994; 42: 1493

[10] Zhao Z B, Northwood D O, Liu C, Liu Y X. J Mater Process Technol, 1999; 89–90: 569

[11] Neeraj T, Hou D H, Daehn G S, Mills M J. Acta Mater, 2000; 48: 1225

[12] Yamada T, Kawabata K, Sato E, Kuribayashi K, Jimbo I. Mater Sci Eng, 2004; A387–389: 719

[13] Alden T H. Metall Trans, 1987; 18A : 51

[14] Wang S H, Zhang Y G, Chen W X. J Mater Sci, 2001; 36: 1931

[15] Nie D F, Zhao J. Key Eng Mater, 2007; 353–358: 138

[16] Nie D F, Zhao J, Mo T, Chen W X. Mater Lett, 2008; 62: 51

[17] Zhao J, Mo T, Nie D F. Mater Sci Eng, 2008; A483–484: 572

[18] Nie D F, Zhao J. Acta Metall Sin, 2009; 45: 840

(聂德福, 赵杰. 金属学报, 2009; 45: 840)

[19] Chen W, Kania R, Worthingham R, Boven G V. Acta Mater, 2009; 57: 6200

[20] Kocks U F, Mecking H. Prog Mater Sci, 2003; 48: 171

[21] Ramberg W, Osgood W R. Technical Note (902), NACA, 1943
Outlines

/