论文

ELECTROPLATING MECHANISM OF NANOSTRUCTURED BLACK Ni FILMS

  • SONG Li-Xiao ,
  • ZHANG Zhao ,
  • ZHANG Jian-Qing ,
  • CAO Chu-Na
Expand
  • Department of Chemistry, Zhejiang University, Hangzhou 310027

Received date: 2010-06-08

  Revised date: 2010-08-13

  Online published: 2011-01-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50771092 and 21073162)

Abstract

Nanocrystalline black nickel film has been obtained from a modified Watt bath by using DC (direct current) electroplating method, and characterized by using SEM and XRD. Meanwhile, the initial electroplating behavior of the nanocrystalline black Ni film was investigated using cyclic voltammetry (CV) and electrochemical impedance spectroscopy (EIS). The results showed that the black Ni film is substantially smooth and bright, and consists of particles with the mean size 51.4 nm. The deposition of black Ni film followed the mechanism of three-dimensional (3D) nucleation and subsequent grain growth. With the increase of the negative potential bias, the main deposition process of black Ni film onto brass changed from the under-potential deposition (UPD) through heterogeneous finally to homogeneous nucleation/growth, which consequently resulted in the initial increase and subsequently decrease of charge-transfer-resistance (Rt). At the high negative bias, the occurrence of the low and the ultra-low frequency inductive loops on EIS plots, can be attributed to the adsorptions of hydrogen atoms and the nickel hydroxyl compound onto cathode surface, which retarded the nucleation/growth process of nickel.

Cite this article

SONG Li-Xiao , ZHANG Zhao , ZHANG Jian-Qing , CAO Chu-Na . ELECTROPLATING MECHANISM OF NANOSTRUCTURED BLACK Ni FILMS[J]. Acta Metall Sin, 2011 , 47(1) : 123 -128 . DOI: 10.3724/SP.J.1037.2010.00268

References

[1] Wieczerniak W, Tremmel R A. Plat Surf Finishing, 1982; 69(6): 90

[2] Costa G, Della V P, Ribeiro M J, Oliveira A P N, Monros G, Labrincha J A. Dyes Pigm, 2008; 71: 137

[3] Zhang W K, Xia X H, Huang H, Gan Y P, Wu J B, Tu J P. J Power Sources, 2008; 184: 646

[4] Cui G F, Li N, Li D Y, Zheng J, Wu Q L. Surf Coat Technol, 2006; 200: 6808

[5] Shashikala A R, Sharma A K, Bhandri D R. Sol Energy Mater Sol Cells, 2007; 91: 629

[6] Saxena V, Rani R U, Sharma A K. Surf Coat Technol, 2006; 201: 855

[7] Won Y S, Park S S, Lee J, Kim J Y, Lee S J. Appl Surf Sci, 2010; 257: 56

[8] Vaishya J S, Tripathi T C. Energy Conver Manage, 1986; 26: 291

[9] Zhang Z K, Cui Z L, Chen K Z. Chin Sci Bull, 1997; 42: 1535

[10] Nieman G W, Weertman J R, Siegel R W. Mater Res Symp Proc, 1994; 206: 493

[11] Wackelgard E. Sol Energy Mater Sol Cells, 1998; 56: 35

[12] Lira–Cantu M, Sabio A M, Brustenga A, G´omez–Romero P. Sol Energy Mater Sol Cells, 2005; 87: 685

[13] Margarita M H, Manuel P P, Nikola B, Ignacio G. J Electroanal Chem, 1998; 443: 81

[14] Margarita M H, Manuel P P, Nikola B, Ignacio G. Surf Sci, 1998; 399: 80

[15] Rani R U, Sharma A K, Minu C. J Appl Electrochem, 2010; 40: 333

[16] Li Y N, Liang Z Z, Liang J Q. Acta Phys Sin, 2010; 59: 4530

[17] Epelboin I, Joussellin M, Wiart R. J Electroanal Chem, 1981; 119: 61

[18] Epelboin I, Joussellin M. J Electroanal Chem, 1979; 101: 281

[19] Ma C B, Cao F H, Zhang Z, Zhang J Q. Appl Surf Sci, 2006; 253: 2251

[20] Nowak P, Socha R P, Kaisheva M, Fransaer J, Celis J P, Stoinov Z. J Appl Electrochem, 2000; 30: 429
Outlines

/

〈 〉